Corrosion of iron archaeological artefacts in soil: characterisation of the corrosion system
Source abstract
Abstract
This paper presents a study made on 40 iron archaeological artefacts buried in soil during several centuries. Samples were taken with the adhering soil and cross-sections were made. The used characterisation techniques are optical and electronic microscopies, EDS coupled to SEM, EPMA, micro-XRD under synchrotron radiation, micro-Raman spectrometry. A specific vocabulary is proposed to describe the corrosion layout. The most identified corrosion layout is made of several ten micrometers zones of magnetite and/or maghemite embedded in a goethite matrix. A corrosion mechanism is proposed in order to explain this profile. When the soil water contains more chlorine or carbonates, some specific corrosion product appear as akaganeite, oxychlorides and siderite.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Metallurgy and Cultural Artifacts
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Misawa · Corros. Sci. · 1974 · 14 · 13110.1016/S0010-938X(74)80051-X ↗
2. J.B. Memet, R. Sabot, C. Deslouis, C. Compère, Euromat’98, Lisboa, 1998, p. 233
3. B. Soerensen, D. Gregory, Metal 98 Conference on Metals Conservation, Draguignan-Figanières, France, 1998, p. 94
4. W. Gerwin, W. Sharff, R. Baumhauer, Metal 98 Conference on Metals Conservation, Draguignan-Figanières, France, 1998, p. 100
5. E. Angelini, E. Barberis, P. Bianco, F. Rosalbino, L. Ruatta, Metal 98 Conference on Metals Conservation, Draguignan-Figanières, France, 1998, p. 106
6. V. Fell, M. Ward, Metal 98 Conference on Metals Conservation, Draguignan-Figanières, France, 1998, p. 111
7. Matthiesen · Stud. Conserv. · 2003 · 48 · 18310.1179/sic.2003.48.3.183 ↗
8. R. Bertholon, C. Relier, Les métaux archéologiques, in: M.-C. Berduccou (Ed.), La conservation en archéologie, Méthodes et pratique de la conservation-restauration des vestiges archéologiques, Masson, Paris, Milan, Barcelone, Mexico, 1990, p. 163
9. R. Bertholon, La limite de la surface d’origine des objets métalliques archéologiques, Caractérisation, localisation et approche des mécanismes de conservation, Paris I, Paris, 2000
10. Pons · 2001
11. Pons · 2002
12. Neff · 2003
13. Dillmann · J. Phys. IV France · 2002 · 39310.1051/jp4:20020248 ↗
14. Stewart · Mater. Sci. Technol. · 2001 · 16 · 28310.1179/026708300101507848 ↗
15. Vega · 2003
16. Dillmann · J. Trace Microprobe Tech. · 1997 · 15 · 251
17. Dillmann · Corros. Sci. · 2002 · 44 · 223110.1016/S0010-938X(02)00028-8 ↗
18. D. Neff, S. Reguer, L. Bellot-Gurlet, P. Dillmann, R. Bertholon, J. Raman Spectrom. (Special Issue on the application of Raman spectroscopy in art and archaeology), 35, in press
19. J. Susini, R. Barrett, B. Kaulich, S. Oestreich, M. Salomé, Sixth International Conference on X-Ray Microscopy, New-York, 2000, p. 19
20. Bonnin-mosbah · Spectrochim. Acta B · 2002 · 57 · 71110.1016/S0584-8547(01)00407-4 ↗
21. D. Neff, P. Dillmann, G. Béranger, Eurocorr 2003, Budapest, 2003, CD ROM
22. S. Reguer, P. Dillmann, P. Lagarde, Eurocorr 2004, Nice, CD ROM
23. Buchwald · Mater. Charact. · 1998 · 40 · 7310.1016/S1044-5803(97)00105-8 ↗
24. Dieudonné-Glad · Historical Metall. · 2001 · 35 · 67
25. P. Dillmann, P. Fluzin, Early ironworking in Europe, Archaeology and Experiment, International Conference, CSA-UISPP 19–25 September 1997, Plas Tan Bwlch, 1997, p. 88
26. Dillmann · Bull. Mater. Sci. · 2001 · 24 · 31710.1007/BF02704929 ↗
27. S. Reguer, D. Neff, E. Vega, P. Dillmann, Spectrochim. Acta Part B, submitted for publication
28. Cornell · 2003