journal article·2009-05

A first quantitative XPS study of the surface films formed, by exposure to water, on Mg and on the Mg–Al intermetallics: Al3Mg2 and Mg17Al12

Ming Liu, Sandrine Zanna, Helene Ardelean, Isabelle Frateur, Patrik Schmutz, Guangling Song, Andrej Atrens, Philippe Marcus

Corrosion Science· Volume 51· Issue 5
Publisher page

Abstract

An XPS investigation was carried out of the surface films, formed by exposure to ultrapure water, on mechanically ground Mg and the two Mg-Al intermetallic compounds: Al3Mg2 and Mg17Al12. The mechanically ground Mg surface had a film of MgO at the Mg metal surface covered by a Mg(OH)2 layer. formed by the reaction of the MgO with water vapour in the air. Upon immersion in ultrapure water, this film converted to a duplex film with an inner MgO layer next to the Mg metal and an external porous hydroxide layer. For both intermetallics, the XPS data is consistent with (i) preferential dissolution of Mg and (ii) a 10 nm thick film on the surface after immersion in ultrapure water; the film composition on Al3Mg2 was AlMg1.4O0.2(OH)(5.4) whilst on Mg17Al12 the composition was AlMg2.5(OH)(8). (C) 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
2. Understanding magnesium corrosion mechanism: a framework for improved alloy performance10.1002/adem.200310405 ↗
3. A critical review of the stress corrosion cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
4. Recent progress in corrosion and protection of magnesium alloys10.1002/adem.200500013 ↗
5. Recent insights into the mechanism of magnesium corrosion and research suggestions10.1002/adem.200600221 ↗
6. The effect of zirconium grain refinement on the corrosion behaviour of magnesium-rare earth alloy MEZ10.1016/S1471-5317(02)00008-1 ↗
7. Influence of dichromate ions on corrosion processes on pure magnesium10.1149/1.1554721 ↗
8. Corrosion resistance of aged die cast magnesium alloy AZ91D10.1016/j.msea.2003.08.060 ↗
9. Corrosion behaviour of magnesium in ethylene glycol10.1016/j.corsci.2003.10.008 ↗
10. The negative difference effect and unipositive Mg+10.1002/adem.200600275 ↗
11. Influence of homogenization annealing of AZ91 on mechanical properties and corrosion behavior10.1002/adem.200700234 ↗
12. Influence of microstructure on corrosion of as-cast ZE4110.1002/adem.200700246 ↗
13. Influence of the b-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
14. Influence of pH and chloride ion concentration on the corrosion of Mg alloy ZE4110.1016/j.corsci.2008.08.023 ↗
15. A study of the corrosion of AZ91 in 1N NaCl and the mechanism of magnesium corrosion10.1002/adem.200800005 ↗
16. The effect of crystallographic orientation on the active corrosion of pure magnesium10.1016/j.scriptamat.2007.10.027 ↗
17. A comparison of the corrosion behaviour in 5% NaCl solution of Mg alloys NZ30K and AZ91D10.1007/s10800-007-9426-x ↗
18. Electrochemical behavior of magnesium alloys AZ91D, AZCe2, and AZLa1 in chloride and sulfate solutions10.1007/s10800-007-9433-y ↗
19. The fractography of stress corrosion cracking (SCC) of Mg–Al alloys10.1007/s11661-008-9475-8 ↗
20. Characterisation of stress corrosion cracking (SCC) of Mg–Al alloys10.1016/j.msea.2007.11.064 ↗
21. The relation between microstructure and corrosion behavior of AZ80 Mg alloy following different extrusion temperatures10.1016/j.corsci.2008.03.003 ↗
22. Improvement of corrosion resistance of AZ91D magnesium alloy by holmium addition10.1016/j.corsci.2006.03.017 ↗
23. Influence of geometry on galvanic corrosion of AZ91D coupled to steel10.1016/j.corsci.2005.08.013 ↗
24. Simulation of galvanic corrosion of magnesium coupled to a steel fastener in NaCl solution10.1002/maco.200403855 ↗
25. Effect of magnesium hydride on the corrosion behavior of an AZ91 magnesium alloy in sodium chloride solution10.1016/j.corsci.2008.09.013 ↗
26. Effects of dust and salt particles on the formation and spreading of micro-droplets on AZ91 magnesium alloy10.1016/j.corsci.2008.01.027 ↗
27. In situ observation of crack initiation and propagation of the charged magnesium alloy under cyclic wet–dry conditions10.1016/j.corsci.2008.05.013 ↗
28. Ion beam analysis of corrosion films on a high magnesium alloy (Magnox Al 80)
29. Studies of inhibition of magnesium corrosion10.1149/1.2411579 ↗
30. Morphology and structure of oxide-films formed on magnesium by exposure to air water10.1149/1.2049981 ↗
31. A TEM investigation of naturally formed oxide films on pure magnesium10.1016/S0010-938X(97)00037-1 ↗
32. An AES and XPS study of the initial oxidation of polycrystalline magnesium with water vapour at room température10.1016/0039-6028(93)90396-2 ↗
33. The initial interaction of water vapour with Mg–Al alloy surfaces at room température10.1016/0039-6028(94)90003-5 ↗
34. Formation and breakdown of surface films on magnesium and its alloys in aqueous solutions10.1016/j.corsci.2006.05.033 ↗
35. AC impedance spectroscopy study of the corrosion behavior of an AZ91 magnesium alloy in 0.1M sodium sulfate solution10.1016/j.electacta.2006.10.007 ↗
36. In situ observation of formation and spreading of micro-droplets on magnesium and its alloy under cyclic wet–dry conditions10.1016/j.corsci.2006.09.003 ↗
37. States and transport of hydrogen in the corrosion process of an AZ91 magnesium alloy in aqueous solution10.1016/j.corsci.2008.01.028 ↗
38. An XPS investigation of the oxidation/corrosion of melt-spun Mg10.1016/S0169-4332(99)00593-0 ↗
39. Quantitative X-ray photoelectron spectroscopy characterization of magnesium oxidized in air10.1149/1.1393369 ↗
40. Initial surface film on magnesium metal: a characterization by X-ray photoelectron spectroscopy (XPS) and photocurrent spectroscopy (PCS)10.1016/j.electacta.2007.03.019 ↗
41. Calculations of electron inelastic mean free paths. II. Data for 27 elements over the 50–2000eV range10.1002/sia.740171304 ↗
42. Hartree-Slater subshell photoionization cross-sections at 1254 and 1487 eV10.1016/0368-2048(76)80015-1 ↗
43. Differential charging in XPS. Part I: demonstration of lateral charging in a bulk insulator using imaging XPS10.1002/(SICI)1096-9918(199606)24:6<422::AID-SIA142>3.0.CO;2-G ↗
44. Differential charging in XPS. Part II: sample mounting and X-ray flux effects on heterogeneous samples10.1002/(SICI)1096-9918(199607)24:7<459::AID-SIA139>3.0.CO;2-5 ↗
45. Differential charging in XPS. Part III: a comparison of charging in thin polymer overlayers on conducting and non-conducting substrates10.1002/(SICI)1096-9918(199710)25:11<904::AID-SIA316>3.0.CO;2-D ↗
46. Oxidation of magnesium10.1002/sia.1346 ↗
47. XPS study of the major minerals in bauxite: Gibbsite, bayerite and (pseudo-) boehmite10.1016/j.jcis.2005.09.054 ↗
48. The secondary passive film for type 304 stainless steel in 0.5M H2SO410.1149/1.1838078 ↗
49. The chemistry of copper patination10.1016/S0010-938X(98)00093-6 ↗
50. Atmospheric corrosion and the colour, structure and composition of natural patinas on copper10.1016/j.corsci.2005.09.011 ↗
51. Electrochemical corrosion of pure magnesium in 1N NaCl10.1016/S0010-938X(96)00172-2 ↗
52. Measurement of oxide film growth on Mg and Al surfaces over extended periods using XPS10.1016/S0039-6028(97)00054-X ↗
53. The oxidation kinetics of Mg and Al surfaces studied by AES and XPS10.1016/S0039-6028(97)00351-8 ↗
54. Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride10.1016/S0010-938X(98)00078-X ↗
55. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
56. Morphology and structure of oxide films formed on MgAl alloys by exposure to air and water10.1149/1.1837048 ↗