Effect of porosity defects on the long-term corrosion behaviour of Fe-based amorphous alloy coated mild steel

S.D. Zhang, J. Wu, W.B. Qi, J.Q. Wang

Corrosion Science· Volume 110
Publisher page

Abstract

Abstract The correlation between the porosity defects, inevitably existed in thermally sprayed Fe-based amorphous coating, and the long-term corrosion behaviour of the coated steels have been studied by salt spray tests, electrochemical measurements, XPS and ToF-SIMS techniques. It has been found that porosity defects reduce the long-term corrosion resistance, increase the passive current density and lower the stability of the passive film. The deteriorated corrosion resistance is ascribed to the reduced Cr:Fe atom ratio around the porosity defects that is demonstrated by ToF- SIMS. These results provide a guide for the design of corrosion-resistant amorphous alloy coatings for engineering applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · High-Temperature Coating Behaviors · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Corrosion resistance of amorphous iron alloys containing chromium10.2320/jinstmet1952.38.9_835 ↗
2. ESCA study of passive film on an extremely corrosion-resistant amorphous iron alloy10.1016/S0010-938X(76)80010-8 ↗
3. The corrosion behavior of amorphous Fe-Cr-Mo-P-C and Fe-Cr-W-P-C alloys in 6-M HCl solution10.1016/0010-938X(92)90147-U ↗
4. Corrosion behaviour of the Mg65Y10Cu15Ag10 bulk metallic glass10.1016/j.msea.2003.10.026 ↗
5. Corrosion and related mechanical properties of bulk metallic glasses10.1557/jmr.2007.0051 ↗
6. Influence of yttrium as a minority alloying element on the corrosion behavior in Fe-based bulk metallic glasses10.1016/j.electacta.2008.08.017 ↗
7. Identifying the role of nanoscale heterogeneities in pitting behaviour of Al-based metallic glass10.1016/j.corsci.2011.05.047 ↗
8. In situ EC-AFM study of the effect of nanocrystals on the passivation and pit initiation in an Al-based metallic glass10.1016/j.corsci.2014.02.005 ↗
9. Iron-based bulk metallic glasses10.1179/1743280412Y.0000000007 ↗
10. Recent development and application products of bulk glassy alloys10.1016/j.actamat.2010.11.027 ↗
11. Characterization of plasma sprayed Fe-17Cr-38Mo-4C amorphous coatings crystallizing at extremely high temperature10.1007/BF02645879 ↗
12. Corrosion resistance of Fe-16% Cr-30% Mo-(C, B P) amorphous coatings sprayed by HVOF and APS processes10.2320/matertrans.46.80 ↗
13. Corrosion resistances of iron-based amorphous metals with yttrium and tungsten additions in hot calcium chloride brine & natural seawater: Fe48Mo14Cr15Y2C15B6 and W-containing variants10.1149/1.2789251 ↗
14. Corrosion resistance of thermally sprayed high-boron iron-based amorphous-metal coatings10.1557/jmr.2007.0291 ↗
15. High performance amorphous steel coating prepared by HVOF thermal spraying10.1016/j.jallcom.2007.11.133 ↗
16. Microstructure and properties of Fe-based amorphous metallic coating produced by high velocity axial plasma spraying10.1016/j.jallcom.2009.04.086 ↗
17. Influence of the size of spraying powders on the microstructure and corrosion resistance of Fe-based amorphous coating10.1016/j.electacta.2011.05.020 ↗
18. Iron-based amorphous metals: high-performance corrosion-resistant material development10.1007/s11661-008-9779-8 ↗
19. The effects of microstructural features on the performance gap in corrosion resistance between bulk and HVOF sprayed Inconel 62510.1016/j.surfcoat.2009.12.028 ↗
20. Formation and corrosion behavior of Fe-based amorphous metallic coatings by HVOF thermal spraying10.1016/j.surfcoat.2009.08.025 ↗
21. Structure and corrosion behavior of 316L stainless steel coatings formed by HVAF spraying with and without sealing10.1016/j.surfcoat.2008.09.011 ↗
22. Effect of porosity sealing treatments on the corrosion resistance of high-velocity oxy-fuel (HVOF)-sprayed Fe-based amorphous metallic coatings10.1016/j.surfcoat.2011.08.045 ↗
23. Characterisation of three-dimensional porosity in an Fe-based amorphous coating and its correlation with corrosion behaviour10.1016/j.corsci.2015.01.022 ↗
24. Corrosion of high-velocity oxy-fuel (HVOF) sprayed iron-based amorphous metallic coatings for marine pump in sodium chloride solutions10.1002/maco.201106211 ↗
25. Comparison of the corrosion resistance of TiN and (Ti,Al)N coatings10.1016/0257-8972(92)90057-H ↗
26. Study of structure and corrosion resistance of Fe-based amorphous coatings prepared by HVAF and HVOF10.1016/j.corsci.2010.12.022 ↗
27. Slurry erosion–corrosion behaviour of high-velocity oxy-fuel (HVOF) sprayed Fe-based amorphous metallic coatings for marine pump in sand-containing NaCl solutions10.1016/j.corsci.2011.05.062 ↗
28. Rapid solidification and microstructure development during plasma spray deposition10.1007/BF02645275 ↗
29. Davis · 2004
30. Thermal transport properties of thermally sprayed coatings10.1179/imr.1992.37.1.271 ↗
31. Pawlowski · 2008
32. Origins of pitting corrosion10.1179/147842204225016859 ↗
33. A study on the self-sealing process of anodic films on aluminum by EIS10.1016/j.surfcoat.2005.10.031 ↗
34. Cerium conversion coatings for the corrosion protection of aluminium
35. Angle-resolved XPS analysis of molybdenum and tungsten in passive films on stainless steel PVD alloys10.1002/sia.1268 ↗
36. XPS determination of compositions of alloy surfaces and surface oxides on mechanically polished iron-chromium alloys10.1016/0010-938X(77)90067-1 ↗
37. Porosity evaluation of protective coatings onto steel, through electrochemical techniques10.1016/S0257-8972(99)00659-3 ↗
38. A study on the quantitative determination of through-coating porosity in PVD-grown coatings10.1016/j.apsusc.2004.03.213 ↗
39. Growth of passivating films on scratched 304L stainless steel in alkaline solution10.1016/0010-938X(83)90111-7 ↗
40. Passivity—the key to our metals-based civilization10.1351/pac199971060951 ↗
41. The coupled kinetics of film growth and dissolution of stainless steel repassivating in acid solutions10.1016/0010-938X(84)90070-2 ↗
42. Why stainless steel corrodes10.1038/415770a ↗
43. Passivity of chromium10.1149/1.2773790 ↗
44. The passivity of iron-chromium alloys10.1016/0010-938X(89)90060-7 ↗
45. On the role of Cr in the passivity of stainless steel10.1149/1.2108450 ↗
46. Theory of steady-state passive films10.1149/1.2086949 ↗
47. Iron-chromium alloys with special consideration of resistance to acids
48. Pitting initiation in Fe-based amorphous coatings10.1016/j.actamat.2012.04.005 ↗
49. Metallurgy (communication arising): stainless-steel corrosion and MnS inclusions10.1038/424389b ↗
50. The composition of the boundary region of MnS inclusions in stainless steel and its relevance in triggering pitting corrosion10.1016/j.corsci.2004.05.023 ↗
51. Identification of MnCr2O4 nano-octahedron in catalysing pitting corrosion of austenitic stainless steels10.1016/j.actamat.2010.05.043 ↗
52. Devitrification of Fe-based amorphous metal SAM 1651 and the effect of heat-treatment on corrosion behavior10.1149/1.3148325 ↗
53. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
54. The nucleation and growth of corrosion pits on stainless steel10.1016/0010-938X(93)90133-2 ↗
55. Repetitive nucleation of corrosion pits on stainless steel and the effects of surface roughness10.1149/1.1416503 ↗
56. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗
57. The cathodic reaction during repassivation of aluminium in open circuit10.1016/0010-938X(95)00023-D ↗
58. Metastable pitting corrosion of stainless steel and the transition to stability10.1098/rsta.1992.0114 ↗
59. Corrosion properties of Fe–Cr–Nb–B amorphous alloys and coatings10.1016/j.surfcoat.2014.06.022 ↗
60. Element-resolved corrosion analysis of stainless-type glass-forming steels10.1126/science.1230081 ↗