Abstract Cr enriched passive films were hardly formed on Type 304 stainless steel under humid atmosphere. Cr fraction in passive films under relative humidities (R.H.) in the range 30–70% was similar to the alloy composition. However, slightly Cr enriched passive films were formed under R.H. 90%. This is attributed to the thin continuous water layer into which Fe ions are selectively dissolved. When chloride is in the water layer, the Cr enrichment was enhanced by accelerated dissolution of Fe as chloride complex. At lower R.H., pitting corrosion occurred because of the more concentrated chloride in the water layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Importance of initial surface film in the degradation of stainless steels by atmospheric exposure10.1016/S0010-938X(03)00047-7 ↗
2. On the role of Cr in the passivity of stainless steel10.1149/1.2108450 ↗
3. The passivity of iron–chromium alloys10.1016/0010-938X(89)90060-7 ↗
4. An electrochemical study of the atmospheric corrosion of mild steel – I. Experimental method10.1016/0010-938X(94)90141-4 ↗
5. Formation and growth of micro-droplets during the initial stage of atmospheric corrosion10.1016/j.electacta.2004.01.032 ↗
6. On the atmospheric corrosion of metals which are covered with thin electrolyte layers – I. Verification of the experimental technique10.1016/0010-938X(90)90032-Z ↗
7. Tomashov · 1966
8. M.G. Fontana, Corrosion Engineering, third ed., McGraw-Hill, 1987.
9. Release rates of chromium and nickel from 304 and 316 stainless steel during urban atmospheric exposure – a combined field and laboratory study10.1016/S0010-938X(02)00054-9 ↗
10. Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions10.1016/j.corsci.2006.08.016 ↗
11. Pitting corrosion of bare stainless steel 304 under chloride solution droplets10.1149/1.3467850 ↗
12. On the atmospheric corrosion of metals which are covered with thin electrolyte layers – III. The measurement of polarisation curves on metal surfaces which are covered by thin electrolyte layers10.1016/0010-938X(90)90034-3 ↗
13. Electrochemical impedance spectroscopy of metals covered with a thin electrolyte layer10.1016/0013-4686(95)00438-6 ↗
14. Humidity fixed points of binary saturated aqueous solutions10.6028/jres.081A.011 ↗
15. Modification of passive film formed on an Fe–18Cr alloy in sulphuric acid solution by ultra-violet light irradiation10.2320/jinstmet1952.63.3_375 ↗
16. Improvement of pitting corrosion resistance of Type 304 stainless steel by modification of passive film with ultraviolet light irradiation10.1149/1.1838493 ↗
17. Surface composition of stainless steels during anodic dissolution and passivation studied by ESCA10.1149/1.2113683 ↗
18. XPS study of passive films formed on molybdenum-implanted austenitic stainless steels10.1002/sia.740190175 ↗
19. An XPS study of the passivity of a series of iron-chromium alloys in sulphuric acid10.1016/S0010-938X(78)80085-7 ↗
20. X-ray photoelectron spectroscopy and scanning tunneling microscopy study of passive films formed on (100) Fe–18Cr–13Ni single-crystal surfaces10.1149/1.1838366 ↗
21. Semiconductor properties and protective role of passive films of iron base alloys10.1016/j.corsci.2006.05.020 ↗
22. An X-ray photo-electron spectroscopic study of surface treatments of stainless steels10.1016/S0010-938X(79)80091-8 ↗
23. A mechanistic study of initial atmospheric corrosion kinetics using electrical resistance sensors10.1016/j.corsci.2005.04.011 ↗
24. Observation of micro-droplets on metal surface in early atmospheric corrosion10.1016/j.elecom.2005.06.016 ↗
25. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗
26. Modeling of atmospheric corrosion environments and its application to constant dew-point corrosion test10.3323/jcorr1991.47.519 ↗