SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel
Source abstract
Abstract
Scanning Kelvin probe force microscopy (SKPFM) of annealed and cold-rolled grade 2205 duplex stainless steel has been correlated with microstructure analysis using electron back-scattered diffraction (EBSD). In annealed microstructure Volta potential differences indicated micro-galvanic coupling between ferrite and austenite reasoning selective dissolution of ferrite. The introduction of cold work reduced the difference between both phases, but the development of local extremes in Volta potential was observed. Microstructure analysis revealed the presence of larger misorientation concentrations at these sites, which can explain the changes in observed corrosion behaviour, from selective dissolution in the annealed condition to localised corrosion attack after cold-rolling.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Misorientation development in grains of tensile strained and crept 2.25%Cr–1%Mo steel10.1016/S1359-6462(01)01197-6 ↗
2. Load sharing between austenite and ferrite in a duplex stainless steel during cyclic loading10.1007/s11661-000-0166-3 ↗
3. Nilsson · 2007
4. Pitting corrosion of metals: a review of the critical factors10.1149/1.1838615 ↗
5. Corrosion behaviour of cold-deformed austenitic alloys
6. Low-temperature stress corrosion cracking of austenitic and duplex stainless steels under chloride deposits10.5006/1242 ↗
7. Significance and mechanism of the crack initiation process during very high cycle fatigue of duplex stainless steel10.1016/j.proeng.2014.06.238 ↗
8. The effect of cooling rate on the mechanical and corrosion properties of SAF 2205 (UNS 31,803) duplex stainless steel welds10.1016/S1359-6462(00)00613-8 ↗
9. Evolution of intragranular misorientation during plastic deformation10.2320/jinstmet1952.64.1_50 ↗
10. Influences of tensile strain and strain rate on the electron work function of metals and alloys10.1016/j.scriptamat.2005.10.064 ↗
11. Electron work function at grain boundary and the corrosion behavior of nanocrystalline metallic materials10.1557/PROC-0887-Q05-03 ↗
12. Moore, W. J., Physikalische Chemie. 4. Auflage ed., Walter de Gruyter, 1986.
13. Application of Volta potential mapping to determine metal surface defects10.1016/j.electacta.2007.05.077 ↗
14. Kelvin probe force microscopy10.1063/1.105227 ↗
15. High-resolution Kelvin probe microscopy in corrosion science: Scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
16. Bagotsky · 2006
17. Bockris · 2002 · vol. 2A · 1
18. Characterization of corrosion interfaces by the scanning Kelvin probe force microscopy technique10.1149/1.1359199 ↗
19. Sadewasser · 2012
20. Effect of surface geometrical configurations induced by microcracks on the electron work function10.1016/j.actamat.2005.04.042 ↗
21. Variations of work function and corrosion behaviors of deformed copper surfaces10.1016/j.apsusc.2004.07.017 ↗
22. Influence of surface morphology on corrosion and electronic behavior10.1016/j.actamat.2005.09.017 ↗
23. Calibration of the scanning Kelvin probe force microscope under controlled environmental conditions10.1016/j.electacta.2012.01.054 ↗
24. Application of a Kelvin microprobe to the corrosion of metals in humid atmospheres10.1149/1.2085578 ↗
25. Leygraf · 2000
26. Hicks · 2008
27. Automatic lateral calibration of tunneling microscope scanners10.1063/1.1149091 ↗
28. IASTM International · 2003
29. Strain induced martensitic transformation of Fe–20Cr–5Mn–0.2Ni duplex stainless steel during cold rolling: effects of nitrogen addition10.1016/j.msea.2011.04.038 ↗
30. Depletion effects at phase boundaries in in 2205 duplex stainless steel characterized with SKPFM and TEM/EDS10.1016/j.corsci.2009.05.012 ↗
31. Characterization of ferrite-austenite boundary region of duplex stainless steels by SAES10.1149/1.1796447 ↗
32. Effect of microstructure on atmospheric-induced corrosion of heat-treated grade 2205 and 2507 duplex stainless steels
33. Effect of 475(C embrittlement on the corrosion behaviour of grade 2205 duplex stainless steel investigated using local probing techniques
34. Kelvin probe force microscopy and atmospheric corrosion of cold-rolled grade 2205 duplex stainless steel
35. Probing propensity of grade 2205 duplex stainless steel towards atmospheric chloride-induced stress corrosion cracking10.1179/1743278214Y.0000000205 ↗
36. Pitting corrosion resistance of cast duplex stainless steels in 3.5% NaCl solution10.1016/j.matchar.2008.03.015 ↗
37. In situ study of selective dissolution of duplex stainless steel 2205 by electrochemical scanning tunnelling microscopy10.1016/S0010-938X(00)00180-3 ↗
38. Potential dependence of preferential dissolution behavior of a duplex stainless steel in simulated solution inside crevice10.3323/jcorr.60.363 ↗
39. Dissolution behavior of α and γ phases of a duplex stainless steel in a simulated crevice solution10.1149/1.3407544 ↗
40. Stress corrosion cracking resistance of duplex stainless steels
41. Cottis · 2010 · vol. 1
42. Effect of nitrogen content on the environmentally-assisted cracking susceptibility of duplex stainless steels10.1007/s11661-003-0211-0 ↗
43. Corrosion behaviour of ferrite and austenite phases on super duplex stainless steel in a modified green-death solution10.1016/j.corsci.2014.08.014 ↗
44. The physical meaning of electrode potentials at metal surfaces and polymer/metal interfaces: consequences for delamination10.1149/1.2926589 ↗
45. Electrochemical corrosion behaviour of a novel submicron-grained austenitic stainless steel in an acidic NaCl solution10.1016/j.msea.2006.05.138 ↗
46. Corrosion mechanisms for iron and low alloy steels exposed to the atmosphere10.1149/1.2086948 ↗
47. ASM Handbook, Volume 13A: Corrosion: Fundamentals, Testing, and Protection. vol. 13
48. Marcus · 2006
49. Hydrogen-enhanced cracking of 2205 duplex stainless steel10.1111/j.1460-2695.2007.01191.x ↗
50. Effect of annealing temperature on the mechanical and corrosion behavior of a newly developed novel lean duplex stainless steel10.3390/ma7096604 ↗