journal article·2008-04Open access

Corrosion characterization of tin–lead and lead free solders in 3.5wt.% NaCl solution

Dezhi Li, Paul P. Conway, Changqing Liu

Corrosion Science· Volume 50· Issue 4

Abstract

Abstract The corrosion resistance of Sn–Pb and several candidate lead free solders were investigated in 3.5 wt.% NaCl solution through potentiodynamic polarisation. Results showed that in NaCl solution lead free solders had better corrosion resistance than Sn–Pb solder and the corrosion resistance of lead free solders was similar, but the corrosion resistance of Sn–Ag solder was better than that of Sn–Ag–Cu and Sn–Cu solders. The corrosion products for Sn–Pb solder had a two-layered structure with Sn-rich phases at the outer layer and looser Pb-rich phases at the inner layer. The loose Pb-rich layer was detrimental to the corrosion property. The corrosion product on the surface of all these solders was tin oxide chloride hydroxide.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Directive of the European Commission for the Reduction of Hazardous Substances, Directive 2000/0159 (COD) C5-0487/2002, LEX 391, PE-CONS 3662/2/02 Rev 2, ENV581, CODEC 1273, 2003.
2. B.P. Richards, C.L. Levoguer, C.P. Hunt, K. Nimmo, S. Peters, P. Cusack, An analysis of the current status of lead-free soldering, available at: http://www.npl.co.uk/ei/documents/pbfreereport.pdf.
3. IPC, Lead Free Solder Selection, available at: http://leadfree.ipc.org/RoHS_3-2-1.asp.
4. Metallurgy of low-temperature Pb-free solders for electronic assembly10.1179/imr.1995.40.2.65 ↗
5. The electrochemical corrosion behaviour of Pb-free Al–Zn–Sn solders in NaCl solution10.1016/S0254-0584(98)00171-0 ↗
6. Corrosion resistance of ZrN films on AISI 304 stainless steel substrate10.1016/S0257-8972(02)00882-4 ↗
7. Inhibition of copper corrosion by isatin in aerated 0.5M H2SO410.1016/S0010-938X(02)00134-8 ↗
8. Pit formation and growth of alloy 600 in Cl- ion-containing thiosulphate solution at temperatures 298–573K using fractal geometry10.1016/S0010-938X(02)00212-3 ↗
9. The influences of sealing methods on corrosion behavior of anodized aluminum alloys in NaCl solutions10.1016/S0257-8972(02)00779-X ↗
10. The potentiodynamic polarisation behavior of Pb-free XIn-9(5Al–Zn)–YSn solders10.1016/S0254-0584(97)02062-2 ↗
11. Electrochemical behavior of a new solder material (Sn–In–Ag)10.1016/S0167-577X(03)00326-4 ↗
12. The effect of alloying element gallium on the polarisation characteristics of Pb-free Sn–Zn–Ag–Al–XGa solders in NaCl solution10.1016/j.corsci.2005.02.003 ↗
13. Electrochemical migration of Sn–Pb and lead free solder alloys under distilled water10.1007/s10854-006-6764-0 ↗
14. Electrochemical corrosion study of Pb-free solders10.1557/jmr.2006.0035 ↗
15. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
16. Potential-pH diagrams for the Sn/H2O–Cl system10.1016/0013-4686(84)87028-0 ↗
17. D.Q. Yu, C.M.L. Wu, L. Wang, The electrochemical corrosion behavior of Sn9Zn and Sn–8Zn–3Bi lead-free solder alloys in NaCl solution, in: 16th International Corrosion Conference, Beijing, China, 2005, 19–24.
18. Anodic passivation of tin in slightly alkaline solutions10.1016/0013-4686(80)80016-8 ↗
19. Investigation on lead corrosion products in sea water and in neutral saline solutions10.1002/maco.19820330707 ↗