journal article·2008-08

Stress corrosion cracking behavior of X70 pipe steel in an acidic soil environment

Z.Y. Liu, X.G. Li, C.W. Du, G.L. Zhai, Y.F. Cheng

Corrosion Science· Volume 50· Issue 8
Publisher page

Abstract

Stress corrosion cracking (SCC) behavior of X70 pipe steel was investigated in an extracted acidic soil solution by slow strain rate test (SSRT), potentiodynamic polarization curve measurements and surface analysis technique. The SCC process and mechanism of X70 steel in the acidic soil solution is mixed-controlled by both anodic dissolution and the hydrogen involvement. With the different applied potentials, the dominance of SCC process changes. At a relatively less negative potential, the steel SCC is based primarily on the anodic dissolution mechanism. When the applied potential is shifted negatively, hydrogen is involved in the cracking process, resulting in a transgranular cracking mode. With the further negative shift of applied potential, the SCC of the steel follows completely a hydrogen-based mechanism, with a river-bed shaped brittle feature of the fracture surface. Heat treatment alters the microstructure of the steel, resulting in a change of SCC susceptibility. In particular, the quenched steel with a bainite microstructure has a high susceptibility to SCC in the acidic soil, while the as-received steel with a ferrite matrix have a low SCC susceptibility.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. R.N. Parkins, Corrosion’2000, NACE, Houston, 2000, Paper no. 363.
2. M. Baker Jr., Stress Corrosion Cracking Studies, Integrity Management Program DTRS56-02-D-70036, Department of Transportation, Office and Pipeline Safety, 2004.
3. National Energy Board, Report of Public Inquiry Concerning Stress Corrosion Cracking on Canadian Oil and Gas Pipelines, MH-2-95, November 1996.
4. Kentish · Brit. Corrosion Journal · 1985 · 20 · 13910.1179/000705985798272786 ↗
5. Sutcliffe · Corrosion · 1972 · 28 · 31310.5006/0010-9312-28.8.313 ↗
6. Li · Electrochimica Acta · 2008 · 53 · 283110.1016/j.electacta.2007.10.077 ↗
7. J.A. Beavers, C.E. Jaskece, Corrosion/98, NACE Inter, Houston, TX, 1998, Paper no. 304.
8. Parkins · Corrosion · 1999 · 55 · 31210.5006/1.3283993 ↗
9. Niu · Applied Surface Science · 2007 · 253 · 862610.1016/j.apsusc.2007.04.066 ↗
10. Bouaeshi · Corrosion · 2007 · 23 · 64810.5006/1.3278415 ↗
11. van Boven · Acta Materialia · 2007 · 55 · 2910.1016/j.actamat.2006.08.037 ↗
12. Cheng · Electrochemistry Communication · 2007 · 9 · 55810.1016/j.elecom.2006.10.035 ↗
13. Fang · Journal of Material Science · 2003 · 38 · 12710.1023/A:1021126202539 ↗
14. Gu · Corrosion · 1999 · 55 · 9610.5006/1.3283971 ↗
15. Qiao · Corrosion · 1998 · 54 · 11510.5006/1.3284834 ↗
16. T. Kushidu, K. Nose, H. Asabi, M. Kimura, Y. Yamane, S. Endo, H. Kawano, Corrosion/2001, NACE, Houston, TX, 2001, Paper no.213.
17. Ahmed · Corrosion · 1997 · 53 · 58110.5006/1.3290290 ↗
18. Brongers · Corrosion · 2000 · 56 · 105010.5006/1.3294382 ↗
19. T.R. Jack, B. Erno, K. Krist, Corrosion/2000, NACE, Houston, TX, 2000, Paper no. 362.
20. J.A. Beavers, C.L. Durr, B.S. Delanty, D.M. Owen, R.L. Sutherby, Corrosion/2001, NACE, Houston, TX, 2001, Paper no. 217.
21. Gonzalez-Rodriguez · Corrosion · 2002 · 58 · 58410.5006/1.3277649 ↗
22. Park · Corrosion · 2002 · 58 · 32910.5006/1.3287682 ↗
23. Chen · Corrosion · 2002 · 58 · 26710.5006/1.3279878 ↗
24. Li · Electrochimica Acta · 2007 · 52 · 811110.1016/j.electacta.2007.07.015 ↗
25. Cheng · Journal of Materials Science · 2007 · 42 · 270110.1007/s10853-006-1375-y ↗
26. Chinese National Standard for Stress Corrosion Cracking Tests, GB T15970, 2007.
27. Zhao · Journal of University of Science and Technology Beijing · 2007 · 14 · 41010.1016/S1005-8850(07)60081-4 ↗
28. Hirth · Metallurgical Transactions A · 1980 · 11A · 86110.1007/BF02654700 ↗
29. Parkins · Corrosion Science · 1980 · 20 · 14710.1016/0010-938X(80)90128-6 ↗