Growth characteristics and corrosion resistance of micro-arc oxidation coating on pure magnesium for biomedical applications
Source abstract
Abstract
Protective micro-arc oxidation (MAO) coating was prepared on pure magnesium in aqueous solution without toxic components under a constant current density. The whole anodizing process can be divided into four stages based on the differences in voltage, sparking behaviour and oxygen evolution. SEM micrographs show that a thick and dense coating can be obtained after anodizing for adequate time. The corrosion resistance of the samples with anodic coatings was evaluated by drop experiments and potentiodynamic polarization tests. The results confirm that the thick and dense coating can efficiently protect the magnesium substrate from corrosion in aggressive environments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
2. Control of biodegradation of biocompatible magnesium alloys10.1016/j.corsci.2007.01.001 ↗
3. Electrodeposition of hydroxyapatite coating on AZ91D magnesium alloy for biomaterial application10.1016/j.matlet.2008.02.048 ↗
4. Magnesium: nutrition and metabolism10.1016/S0098-2997(02)00089-4 ↗
5. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
6. Influence of heat treatment on degradation behavior of bio-degradable die-cast AZ63 magnesium alloy in simulated body fluid10.1016/j.msea.2006.12.020 ↗
7. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
8. Biocorrosion of magnesium alloys: a new principle in cardiovascular implant technology?10.1136/heart.89.6.651 ↗
9. Protective coatings on magnesium and its alloys – a critical review10.1016/S0925-8388(01)01899-0 ↗
10. Corrosion resistance property of the ceramic coating obtained through microarc oxidation on the AZ31 magnesium alloy surfaces10.1016/j.surfcoat.2006.07.079 ↗
11. Corrosion properties of AZ31 magnesium alloy and protective effects of chemical conversion layers and anodized coatings10.1016/S1003-6326(07)60123-X ↗
12. Electrochemical behavior of anodized Mg alloy AZ91D in chloride containing aqueous solution10.1016/j.corsci.2005.01.010 ↗
13. Recent progress in corrosion and protection of magnesium alloys–an overview of cast’s research work10.1002/adem.200500013 ↗
14. Electrochemical corrosion behavior of composite coatings of sealed MAO film on magnesium alloy AZ91D10.1016/j.electacta.2005.08.026 ↗
15. Formation mechanism of pulse current anodized film on AZ91D Mg alloy10.1016/S1003-6326(08)60004-7 ↗
16. Electrochemical corrosion behavior of composite MAO/sol–gel coatings on magnesium alloy AZ91D using combined micro-arc oxidation and sol–gel technique10.1016/j.jallcom.2008.06.135 ↗
17. Anodic films formed on magnesium in organic silicate-containing electrolytes10.1016/j.corsci.2009.02.001 ↗
18. HB5061-77, Standard quality test method for chemical oxidation film of magnesium alloys.
19. How useful is SBF in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
20. Formation of micro-arc oxidation coatings on AZ91HP magnesium alloys10.1016/j.corsci.2009.08.009 ↗
21. The effect of zirconium grain refinement on the corrosion behaviour of magnesium-rare earth alloy MEZ10.1016/S1471-5317(02)00008-1 ↗
22. The effects of heat treatment and zirconium on the corrosion behaviour of Mg–3Nd–0.2Zn–0.4Zr (wt.%) alloy10.1016/j.corsci.2006.12.011 ↗
23. Influence of anodising current on the corrosion resistance of anodised AZ91D magnesium alloy10.1016/j.corsci.2005.08.004 ↗
24. The corrosion performance of anodized magnesium alloys10.1016/j.corsci.2006.02.008 ↗
25. Effects of Na2SiO3 on anodization of Mg–Al–Zn alloy in 3M KOH solution10.1016/j.corsci.2004.02.001 ↗
26. Experimental evaluation of some electrolytic breakdown hypotheses10.1016/0013-4686(71)85169-1 ↗
27. Analysis of phase distribution for ceramic coatings formed by microarc oxidation on aluminum alloy10.1111/j.1151-2916.1998.tb02493.x ↗
28. Growth regularity of ceramic coatings formed by microarc oxidation on Al–Cu–Mg alloy10.1016/S0040-6090(00)01026-9 ↗
29. The anodic dissolution of magnesium in chloride and sulphate solutions10.1016/S0010-938X(97)00090-5 ↗
30. The development of binary Mg–Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
31. The electrochemical corrosion of pure magnesium in 1N NaCl10.1016/S0010-938X(96)00172-2 ↗
32. Electrochemical reactivity surface composition corrosion mechanisms of the complex metallic alloy Al3Mg210.1016/j.corsci.2009.10.015 ↗
33. Corrosion characterization of Mg–8Li alloy in NaCl solution10.1016/j.corsci.2009.03.011 ↗
34. Growth characterization of anodic film on AZ91D magnesium alloy in an electrolyte of Na2SiO3 and KF10.1016/S1005-8850(06)60091-1 ↗
35. Effect of heat treatment on corrosion and electrochemical behavior of Mg–3Nd–0.2Zn–0.4Zr (wt.%) alloy10.1016/j.electacta.2006.09.069 ↗