Corrosion of copper in seawater and its aerosols in a tropical island
Source abstract
Abstract
Abstract A complete characterization of copper corrosion behavior has been carried out under permanent immersion, water line, splash zone and at the atmosphere (near and far from the sea) at the tropical Cuban archipelago. No significant differences have been determined for corrosion of copper under complete immersion for test sites representative of Cuban archipelago. The maximum corrosion rate was observed on the line of water, related to the partial removing of the corrosion products layer due to water movement (waves) and a higher availability of oxygen. Patina composition was characterized using XRD, IR, EDS and SEM techniques. Paratacamite (Cu2(OH)3Cl) was the main component of the patina formed under complete immersion, on the line of water and in the splash zone. In poorly polluted atmospheric marine environments also atacamite (another structural modification of Cu2(OH)3Cl) was found. When environmental SO2 reaches a competitive level with the chloride aerosol the patina formed is a complex mixture of basic cupric chlorides (paratacamite and atacamite) and basic cupric sulfates, antlerite (Cu3(SO4)(OH)4) and brochantite (Cu4(SO4)(OH)6). Brochantite and basic cupric chlorides are detected at inland rural sites. The patina morphology reveals details about the local environment in which it is formed and shed light on its more or less protective role for the metal. The relatively large corrosion rate under complete immersion and on the line of water is related to the formation of a patina with poor adherence to the metal surface and to a porous layer of cuprite formed by relatively large octahedral crystals.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Gas Sensing Nanomaterials and Sensors · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Vernon · J. Inst. Metals · 1930 · 44 · 389
2. Leidheiser · 1971 · 230
3. Mattsson · 1982 · 365
4. Graedel · Corros. Sci · 1987 · 27 · 72110.1016/0010-938X(87)90053-9 ↗
5. Fitzgerald · Corros. Sci · 1998 · 40 · 202910.1016/S0010-938X(98)00093-6 ↗
6. Kalashnikova · Corros. Rev · 1995 · 13 · 26110.1515/CORRREV.1995.13.2-4.261 ↗
7. ISO 8407:1991 (E), Corrosion of Metals and Alloys, Removal of Corrosion Products from Corrosion Tests Specimens, 1991
8. Fernández · Solid State Ionics · 1996 · 93 · 13910.1016/S0167-2738(96)00443-2 ↗
9. Lluis-Riera · Serie Oceanogr. (ACC) · 1972 · 14 · 3
10. Shanon · Acta Crystall · 1976 · 32A · 75110.1107/S0567739476001551 ↗
11. Graedel · J. Electrochem. Soc · 1990 · 137 · 238510.1149/1.2086948 ↗
12. Tomashov · 1966 · 672
13. La Que · 1975 · 332
14. Mattsson · ChemTech · 1985 · 234
15. Feliu · Corros. Sci · 1993 · 34 · 40310.1016/0010-938X(93)90112-T ↗
16. M. Morcillo, J. Simancas, S. Feliu, in: Atmospheric Corrosion, ASTM STP, vol. 1239, Philadelphia, 1995, p. 19510.1520/STP14920S ↗
17. Schumacher · 1983 · 512
18. Hummer · Mater. Protect · 1968 · 7 · 41
19. Mendoza · Corros. Sci · 2000 · 42 · 112310.1016/S0010-938X(99)00135-3 ↗
20. National Atlas of Cuba, Havana, Cuban Institute of Geodesy and Cartography, 1978
21. F. Corvo, Ph.D. Thesis, CNIC, Havana, Cuba, 1980
22. Corvo · Corrosion (NACE) · 1984 · 40 · 17010.5006/1.3581934 ↗
23. Mendoza · Corros. Sci · 1999 · 41 · 7510.1016/S0010-938X(98)00081-X ↗
24. Corvo · Corrosion · 1995 · 37 · 188910.1016/0010-938X(95)00058-R ↗
25. Steiger · 1995 · 115
26. Kruger · J. Electrochem. Soc · 1959 · 106 · 84710.1149/1.2427161 ↗
27. Graedel · Corros. Sci · 1987 · 27 · 74110.1016/0010-938X(87)90054-0 ↗
28. Nemecz · 1981
29. Opila · Corros. Sci · 1987 · 27 · 68510.1016/0010-938X(87)90050-3 ↗
30. Nassau · Corros. Sci · 1987 · 27 · 66910.1016/0010-938X(87)90049-7 ↗
31. Matteini · Stud. Conservat · 1984 · 22 · 18
32. Veleva · Electrochim. Acta · 1996 · 41 · 164110.1016/0013-4686(95)00417-3 ↗