journal article·2013-08

Pitting corrosion of rheocast A356 aluminium alloy in 3.5wt.% NaCl solution

R. Arrabal, B. Mingo, A. Pardo, M. Mohedano, E. Matykina, I. Rodríguez

Corrosion Science· Volume 73
Publisher page

Abstract

In this study, the microstructure and corrosion behaviour of rheocast and gravity-cast A356 aluminium alloys were examined and compared. Scanning Kelvin probe force microscopy (SKPFM) results proved that large potential differences between iron-containing intermetallics and the α-Al matrix were responsible for the initiation of the attack at the intermetallics/α-Al interfaces. For longer immersion times, corrosion attack proceeded through the eutectic areas. Semisolid processing refined the eutectic silicon and iron-intermetallics and reduced the potential difference between secondary phases and the matrix. This resulted in improved pitting corrosion resistance of the rheocast A356 aluminium alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Bauxite Residue and Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. Davis · 1993 · 706
2. Significant improvement of semi-solid microstructure and mechanical properties of A356 alloy by ARB process10.1016/j.msea.2010.11.086 ↗
3. Davis · 1993 · 579
4. Mondolfo · 1943
5. The effect of iron and manganese on the formation of intermetallic compounds in aluminum–silicon alloys10.1016/j.msea.2004.06.022 ↗
6. S. Jain, Corrosion and protection of heterogeneous cast Al–Si (356) and Al–Si–Cu–Fe (380) alloys by chromate and cerium inhibitors, The Ohio State University, Ohio, USA, 2006.
7. Electrochemical behavior of aluminum-base intermetallics containing iron10.1149/1.2086441 ↗
8. Role of intermetallic phases in localized corrosion of AA508310.1016/j.electacta.2006.12.072 ↗
9. Corrosion behavior of as-cast silicon carbide particulate-aluminum alloy metal–matrix composites10.5006/1.3293509 ↗
10. Semisolid metal processing10.1179/095066001225001076 ↗
11. Quantitative analysis of pitting corrosion behavior of thixoformed A356 alloy in chloride medium using electrochemical techniques10.1016/j.matdes.2008.10.003 ↗
12. Evaluation of pitting corrosion of thixoformed A356 alloy using a simulation model10.1016/S1003-6326(09)60361-7 ↗
13. Mechanical and corrosion properties of rheocast and low-pressure cast A356-T6 alloy10.1016/j.msea.2004.08.056 ↗
14. Pitting corrosion of A357 aluminium alloy obtained by semisolid processing10.1002/1521-4176(200109)52:9<691::AID-MACO691>3.0.CO;2-T ↗
15. Phenomenological observations on mechanical and corrosion properties of thixoformed 357 alloys: a comparison with permanent mold cast 357 alloys10.1007/s11661-002-0064-y ↗
16. Mushy/semi-solid metal forming technology – present and future10.1016/S0007-8506(07)61705-3 ↗
17. Influence of surface liquid segregation on corrosion behavior of semi-solid metal high pressure die cast aluminium alloys10.1016/S1003-6326(10)60591-2 ↗
18. The influence of liquid surface segregation on the pitting corrosion behavior of semi-solid metal high pressure die cast alloy F35710.2174/1876503300902010216 ↗
19. Influence of Fe-rich intermetallic inclusions on pit initiation on aluminum alloys in aerated NaCl10.1149/1.1391637 ↗
20. Influence of applied strain on the microstructural corrosion of AlMg2 as-cast aluminium alloy in sodium chloride solution10.1016/j.corsci.2012.08.047 ↗
21. Localised corrosion initiation and microstructural characterisation of an Al 2024 alloy with a higher Cu–Mg ratio10.1016/j.corsci.2011.10.035 ↗
22. Impact of ultrafine-grained microstructure on the corrosion of aluminium alloy AA202410.1016/j.corsci.2011.12.016 ↗
23. Corrosion of AA2024-T3 part II: co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
24. Relationship between microstructure, microhardness and corrosion sensitivity of an AA 2024-T3 friction stir welded joint10.1016/j.corsci.2011.05.049 ↗
25. Corrosion of AA2024-T3 part I: localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
26. Electrochemical characteristics of intermetallic phases in aluminum alloys10.1149/1.1869984 ↗
27. Electrochemical behavior and localized corrosion associated with Al7Cu2Fe particles in aluminum alloy 7075-T65110.1016/j.corsci.2006.02.007 ↗
28. Localized corrosion of a 2219 aluminium alloy exposed to a 3.5% NaCl solution10.1016/j.corsci.2010.04.035 ↗
29. Localized corrosion of 2024 T351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
30. Relation between microstructural aspects of AA2024 and its corrosion behaviour investigated using AFM scanning potential technique10.1016/S0010-938X(00)00002-0 ↗
31. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
32. Corrosion of AA2024-T3 part III: propagation10.1016/j.corsci.2010.09.035 ↗
33. ASTM G1-03. Standard practice for preparing, cleaning and evaluating corrosion test specimens, American Society for Testing and Materials, 2011.
34. Grain refining of conventional and semi-solid A356 Al–Si alloy10.1016/j.jmatprotec.2006.02.012 ↗
35. Effect of Sr and solidification conditions on characteristics of intermetallic in Al–Si 319 industrial alloys10.1016/j.matdes.2009.06.017 ↗
36. J.A. Taylor, The effect of iron in Al–Si casting alloys, in: 35th Australian Foundry Institute National Conference, Adelaide, South Australia, 2004, pp. 148–157.
37. Effects of electromagnetic stirring and superheat on the microstructural characteristics of Al–Si–Fe alloy10.1016/j.msea.2006.05.076 ↗
38. Crystallization behaviour of iron-containing intermetallic compounds in 319 aluminum alloy10.1007/BF02668540 ↗
39. Integrated AFM and SECM for in situ studies of localized corrosion of Al alloys10.1016/j.electacta.2006.12.073 ↗
40. The role of intermetallic particles in localized corrosion of an aluminum alloy studied by SKPFM and integrated AFM/SECM10.1149/1.2883737 ↗
41. Characterization of cast AlSi(Cu) alloys by scanning Kelvin probe force microscopy10.1016/j.electacta.2006.03.027 ↗
42. Corrosion behaviour of different tempers of AA7075 aluminium alloy10.1016/j.electacta.2004.01.046 ↗
43. Effect of solution heat treatment on galvanic coupling between intermetallics and matrix in AA7075-T610.1016/S0010-938X(03)00004-0 ↗
44. Local potential measurements with the SKPFM on aluminium alloys10.1016/j.electacta.2004.01.045 ↗
45. Relations between sample preparation and SKPFM Volta potential maps on an EN AW-6005 aluminium alloy10.1016/j.corsci.2004.07.029 ↗
46. Formation of a cerium-based conversion coating on AA2024: relationship with the microstructure10.1016/S0257-8972(03)00743-6 ↗
47. Characterization of AA2024-T3 by scanning Kelvin probe force microscopy10.1149/1.1838633 ↗
48. Enhanced performance of the AA2050-T8 aluminium alloy following excimer laser surface melting and anodising processes10.1016/j.tsf.2009.09.121 ↗
49. High power diode laser treatments for improving corrosion resistance of A380/SiCp aluminium composites10.1016/j.surfcoat.2008.03.025 ↗
50. Relationship between microstructure and corrosion performance of AA2050-T8 aluminium alloy after excimer laser surface melting10.1016/j.corsci.2010.03.003 ↗
51. Characterization of corrosion interfaces by the scanning Kelvin probe force microscopy technique10.1149/1.1359199 ↗
52. Mechanical properties of cast A356 alloy, solidified at cooling rates enhanced by phase transition of a cooling medium10.1016/j.msea.2006.10.025 ↗
53. Z. Szklarksa-Smialowska, Pitting corrosion of metals, Houston, TX, 1986.
54. EIS study on pitting corrosion of AA5083-H321 aluminium-magnesium alloy in stagnant 3.5% NaCl solution
55. Improvement of corrosion behavior of A3xx.x/SiCp composites in 3.5wt % NaCl solution by Ce surface coatings10.1149/1.2150151 ↗
56. Origins of pitting corrosion10.1179/147842204225016859 ↗
57. Pitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗