journal article·2008-02

Inhibition effect of nonionic surfactant on the corrosion of cold rolled steel in hydrochloric acid

Xianghong Li, Shuduan Deng, Guannan Mu, Hui Fu, Fazhong Yang

Corrosion Science· Volume 50· Issue 2
Publisher page

Abstract

Abstract The inhibition effect of Tween-20 as a nonionic surfactant on the corrosion of cold rolled steel (CRS) in 1.0–8.0 M HCl has been studied at different temperatures (20–50 °C) by weight loss and potentiodynamic polarization methods. Atomic force microscope (AFM) provided the CRS surface conditions. The results show that Tween-20 is a good inhibitor in 1.0 M HCl, and the inhibition efficiency (IE) increases with the inhibitor concentration, while decreases with increasing the hydrochloric acid concentration and temperature. Effect of immersion time was also studied and discussed. The adsorption of inhibitor on the CRS surface obeys the Langmuir adsorption isotherm equation. Both thermodynamic and kinetic parameters have been obtained by adsorption theory and kinetic equations. The inhibition effect is satisfactorily explained by the parameters. Polarization curves show that Tween-20 is a mixed-type inhibitor in hydrochloric acid. The results obtained from weight loss and polarization are in good agreement, and Tween-20 inhibition action could also be evidenced by surface AFM images.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Hudson · Met. Finish. · 1980 · 78 · 21
2. Singh · Corros. Sci. · 1994 · 37 · 100510.1016/0010-938X(95)00010-H ↗
3. Sykes · Brit. Corros. J. · 1990 · 25 · 17510.1179/000705990798269577 ↗
4. ElAzhar · Corros. Sci. · 2001 · 43 · 222910.1016/S0010-938X(01)00034-8 ↗
5. Singh · Corrosion · 1993 · 49 · 59410.5006/1.3316090 ↗
6. Banerjee · Corrosion · 1992 · 48 · 1010.5006/1.3315912 ↗
7. Arab · Corrosion · 1993 · 49 · 12210.5006/1.3299206 ↗
8. Raspi · Nickel Corros. · 1993 · 49 · 82110.5006/1.3316005 ↗
9. Chen · Daily Chem. Ind. · 1986 · 2 · 56
10. Shi · Daily Chem. Ind. · 1987 · 1 · 9
11. Bentiss · Corros. Sci. · 2000 · 42 · 12710.1016/S0010-938X(99)00049-9 ↗
12. Christopher · Corros. Sci. · 1994 · 36 · 15
13. Hajjaji · Corrosion · 1993 · 49 · 32610.5006/1.3316057 ↗
14. Elachouri · Corros. Sci. · 1995 · 37 · 38110.1016/0010-938X(94)00134-R ↗
15. Luo · Corrosion · 1998 · 54 · 61910.5006/1.3287638 ↗
16. Migahed · Mater. Chem. Phys. · 2004 · 85 · 27310.1016/j.matchemphys.2003.12.027 ↗
17. Osman · Mater. Chem. Phys. · 1997 · 50 · 27110.1016/S0254-0584(97)01941-X ↗
18. Zucchi · Corros. Sci. · 1992 · 33 · 113510.1016/0010-938X(92)90167-2 ↗
19. Elachouri · Corros. Sci. · 1994 · 37 · 38110.1016/0010-938X(94)00134-R ↗
20. Wei · J. Colloid Interf. Sci. · 2003 · 259 · 9710.1016/S0021-9797(03)00025-0 ↗
21. Maayta · Brit. Corros. J. · 2001 · 36 · 13310.1179/000705901101501569 ↗
22. Villamil · J. Electroanal. Chem. · 1999 · 472 · 11210.1016/S0022-0728(99)00267-3 ↗
23. Fuchs-Godec · Colloids Surf. A · 2004 · 244 · 7310.1016/j.colsurfa.2004.05.015 ↗
24. Ma · Corros. Sci. · 2003 · 45 · 86710.1016/S0010-938X(02)00175-0 ↗
25. Zhao · Corros. Sci. · 1999 · 41 · 193710.1016/S0010-938X(99)00029-3 ↗
26. Abd El Rehim · Mater. Chem. Phys. · 2001 · 70 · 6410.1016/S0254-0584(00)00468-5 ↗
27. Abd El Rehim · Mater. Chem. Phys. · 2002 · 78 · 33710.1016/S0254-0584(01)00602-2 ↗
28. Maayta · Corros. Sci. · 2004 · 46 · 112910.1016/j.corsci.2003.09.009 ↗
29. Guo · Colloids Surf. A · 2002 · 209 · 3710.1016/S0927-7757(02)00032-8 ↗
30. Branzoi · Mater. Chem. Phys. · 2002 · 78 · 12210.1016/S0254-0584(02)00222-5 ↗
31. Elachouri · Corrosion · 1996 · 52 · 10310.5006/1.3292100 ↗
32. Algaber · Mater. Chem. Phys. · 2004 · 86 · 2610.1016/j.matchemphys.2004.01.040 ↗
33. Osman · Anti-Corros. Methods Mater. · 1997 · 44 · 31810.1108/00035599710177619 ↗
34. Tang · Corros. Sci. · 2003 · 45 · 225110.1016/S0010-938X(03)00046-5 ↗
35. Manjula · Anti-Corros. Methods Mater. · 2001 · 48 · 31910.1108/EUM0000000005883 ↗
36. Lebrini · Corros. Sci. · 2006 · 48 · 127910.1016/j.corsci.2005.05.001 ↗
37. Mu · Corrosion · 1996 · 52 · 85310.5006/1.3292077 ↗
38. Sekine · Corrosion · 1986 · 42 · 27210.5006/1.3584904 ↗
39. Riggs · 1973 · 7
40. Mu · Mater. Chem. Phys. · 2004 · 86 · 5910.1016/j.matchemphys.2004.01.041 ↗
41. Wang · Mater. Prot. · 2001 · 34 · 16
42. Moretti · Werkst. Korros. · 1994 · 45 · 64110.1002/maco.19940451203 ↗
43. Khamis · Corrosion · 1990 · 46 · 47610.5006/1.3585135 ↗
44. Moretti · Corros. Sci. · 2004 · 46 · 38710.1016/S0010-938X(03)00150-1 ↗
45. Martinez · Appl. Surf. Sci. · 2002 · 199 · 8310.1016/S0169-4332(02)00546-9 ↗
46. Do · 1998
47. Cano · Adsorption · 2004 · 10 · 21910.1023/B:ADSO.0000046358.35572.4c ↗
48. Li · Anti-Corros. Methods Mater. · 2003 · 50 · 41010.1108/00035590310501567 ↗
49. Gomma · Mater. Chem. Phys. · 1995 · 39 · 20910.1016/0254-0584(94)01436-K ↗
50. Donahue · J. Electrochem. Soc. · 1965 · 112 · 88610.1149/1.2423723 ↗
51. Kamis · Corrosion · 1991 · 47 · 67710.5006/1.3585307 ↗
52. Bensajjay · Anti-Corros. Methods Mater. · 2003 · 50 · 40210.1108/00035590310501558 ↗
53. Committee of Chinese Industrial Engineering · 2003
54. Ateya · Corros. Sci. · 1984 · 24 · 50910.1016/0010-938X(84)90033-7 ↗
55. Emranuzzaman · Corros. Eng. Sci. Technol. · 2004 · 39 · 32710.1179/174327804X13181 ↗
56. Mu · Acta Chim. Sinica · 2004 · 62 · 2386
57. Chen · Chem. J. Chin. Univ. · 1993 · 14 · 1432
58. Banerjee · Corrosion · 1989 · 45 · 78010.5006/1.3585034 ↗
59. Ferreira · Mater. Chem. Phys. · 2004 · 83 · 12910.1016/j.matchemphys.2003.09.020 ↗
60. Popova · Corros. Sci. · 2003 · 45 · 3310.1016/S0010-938X(02)00072-0 ↗
61. Al-Mayouf · Corrosion · 2001 · 57 · 61410.5006/1.3290388 ↗
62. Al-Mayouf · Desalination · 1998 · 116 · 2510.1016/S0011-9164(98)00054-X ↗
63. Granese · Corros. Sci. · 1992 · 33 · 143910.1016/0010-938X(92)90182-3 ↗
64. Mathur · Corrosion · 1982 · 38 · 17110.5006/1.3579270 ↗
65. Yin · Corros. Sci. · 1995 · 37 · 97510.1016/0010-938X(95)00008-8 ↗
66. Wang · Corros. Sci. · 2001 · 43 · 197
67. Li · Appl. Surf. Sci. · 2005 · 252 · 125410.1016/j.apsusc.2005.02.118 ↗
68. Mu · J. Colloid Interf. Sci. · 2005 · 289 · 18410.1016/j.jcis.2005.03.061 ↗
69. Mu · Corros. Sci. · 2006 · 48 · 44510.1016/j.corsci.2005.01.013 ↗
70. Elkadi · Corros. Sci. · 2000 · 42 · 70310.1016/S0010-938X(99)00101-8 ↗
71. Gewirth · Chem. Rev. · 1997 · 97 · 112910.1021/cr960067y ↗
72. Oppenherm · Science · 1991 · 254 · 688
73. Li · Colloids Surf. A · 1999 · 154 · 22710.1016/S0927-7757(98)00901-7 ↗
74. Teng · Science · 1998 · 282 · 72410.1126/science.282.5389.724 ↗
75. Huang · Corros. Sci. · 2003 · 45 · 262710.1016/S0010-938X(03)00083-0 ↗
76. J.E. Qu, X.P. Guo, in: The 13th China Inhibitor Conference, Kunming, 2004, p. 7 (in Chinese).