Synergy of Cu and Sb to enhance the resistance of 3%Ni weathering steel to marine atmospheric corrosion
Source abstract
Abstract
Abstract Various contents of Cu and Sb elements were incorporated into 3%Ni steel to enhance its corrosion resistance in a simulated tropical marine atmosphere of high salinity. The electrochemical process and the corrosion product film (CPF) properties were analyzed to evaluate the role of Cu and Sb and their synergistic effect. The results showed that there was a synergy between 0.5 % Cu and 0.2 % Sb, which improved the corrosion resistance of 3%Ni steel. This synergy produced a 45-μm-thick inner layer enriched with Cu, Sb and Ni, optimizing the properties of CPF significantly in terms of compactness, phase composition, elemental distribution and electrochemical activity.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Weathering steels: from empirical development to scientific design. A review10.1016/j.corsci.2014.03.006 ↗
2. Atmospheric corrosion data of weathering steels. A review10.1016/j.corsci.2013.08.021 ↗
3. Atmospheric corrosion of weathering steels. Overview for engineers. Part I: basic concepts10.1016/j.conbuildmat.2019.03.334 ↗
4. Composition and protective ability of rust layer formed on weathering steel exposed to various environments10.1016/j.corsci.2005.10.004 ↗
5. Estimation of corrosion loss for Ni-added high corrosion resistant weathering steel based on field exposure test10.3323/jcorr.55.152 ↗
6. Creation of alloy design concept for anti air-born salinity weathering steel10.3323/jcorr1991.49.30 ↗
7. Long-time atmospheric corrosion tests on low-alloy steels
8. Nonlinear trending of corrosion of high nickel alloys in extended marine and atmospheric exposures10.1515/corrrev-2020-0079 ↗
9. Insight into the product film formed on Ni-advanced weathering steel in a tropical marine atmosphere10.1016/j.apsusc.2017.12.018 ↗
10. Characterization of corrosion products formed on Ni 2.4wt%–Cu 0.5wt%–Cr 0.5wt% weathering steel exposed in marine atmospheres10.1016/j.corsci.2014.07.011 ↗
11. Benefit of the corrosion product film formed on a new weathering steel containing 3% nickel under marine atmosphere in Maldives10.1016/j.corsci.2019.108416 ↗
12. Evaluation of applicability for Ni-advanced weathering steels and bridge high-performance steels to railway steel bridges10.2219/rtriqr.51.33 ↗
13. 3% Ni-Weathering steel plate for uncoated bridges at high air-bone salt environments
14. Atmospheric corrosion of Ni-advanced weathering steels in marine atmospheres of moderate salinity10.1016/j.corsci.2013.06.053 ↗
15. A study for corrosion behavior of a new-type weathering steel used in harsh marine environment10.1016/j.conbuildmat.2020.119760 ↗
16. Optimizing the nickel content in weathering steels to enhance their corrosion resistance in acidic atmospheres10.1016/j.corsci.2016.11.016 ↗
17. Boyd · 1974
18. Effect of Cu, Cr and Ni alloying elements on mechanical properties and atmospheric corrosion resistance of weathering steels in marine atmospheres of different aggressivities10.1002/maco.201709656 ↗
19. Control of Fe (O, OH)6 nano-network structures of rust for high atmospheric-corrosion resistance10.1016/j.corsci.2005.04.005 ↗
20. Five-year atmospheric corrosion of Cu, Cr and Ni weathering steels in a wide range of environments10.1016/j.corsci.2018.06.039 ↗
21. Effect of antimony on the corrosion behavior of low-alloy steel for flue gas desulfurization system10.1016/j.corsci.2007.11.027 ↗
22. Compositional design of low carbon sulphuric acid dewpoint corrosion resistant steel and corresponding anticorrosive mechanism10.1179/1743278212Y.0000000071 ↗
23. Electrochemical behavior of antimony and antimony oxide films in acid solutions10.5006/1.3278298 ↗
24. Effect of chloride ions on the corrosion behavior of low-alloy steel containing copper and antimony in sulfuric acid solution10.1007/s12540-015-4421-y ↗
25. Corrosion and SCC initiation behavior of low-alloy high-strength steels microalloyed with Nb and Sb in a simulated polluted marine atmosphere10.1016/j.jmrt.2020.09.033 ↗
26. Corrosion behaviour of experimental copper–antimony–molybdenum carbon steels in industrial and marine atmospheres and in a sulphuric acid aqueous solution10.1080/1478422X.2017.1305537 ↗
27. Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment10.1016/j.corsci.2018.04.007 ↗
28. Li · 2014
29. ASTM G1-03 · 2003
30. Microstructural characterisation and corrosion performance of old railway girder bridge steel and modern weathering structural steel10.1016/j.corsci.2016.10.004 ↗
31. RIR-measurement and use in quantitative XRD10.1017/S0885715600013257 ↗
32. Long-term atmospheric corrosion of mild steel10.1016/j.corsci.2010.10.007 ↗
33. State of chlorides in rusts formed on 3 mass% Ni-added weathering steel10.1149/1.3114949 ↗
34. Effect of Co and Ni on the corrosion behavior of low alloy steels in wet/dry environments10.1016/S0010-938X(00)00018-4 ↗
35. Improving the resistance of high-strength steel to SCC in a SO2-polluted marine atmosphere through Nb and Sb microalloying10.1016/j.corsci.2020.108693 ↗
36. Taxonomy for protective ability of rust layer using its composition formed on weathering steel bridge10.1016/j.corsci.2006.06.016 ↗
37. Characterization of rust layers on weathering steels air-exposed for a long period10.2320/matertrans.43.2818 ↗
38. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal–industrial atmosphere for 17 years10.1016/S0010-938X(03)00070-2 ↗
39. NIST XPS database. https://srdata.nist.gov/xps/selEnergyType.aspx.
40. Chastain · 1992 · 40 · 221
41. Nano structure and electrochemical behavior of the rust formed on Ni bearing steel after exposure tests in a tropical Indian environment10.2320/matertrans.M2014200 ↗
42. Atmospheric corrosion resistance of MnCuP weathering steel in simulated environments10.1016/j.corsci.2011.08.028 ↗
43. A study of the evolution of rust on Mo–Cu-bearing fire-resistant steel submitted to simulated atmospheric corrosion10.1016/j.corsci.2011.09.023 ↗
44. Chemical order in Ga or Sb modified germanium sulfide glasses around stoichiometry: high-resolution XPS and Raman studies10.1016/j.jnoncrysol.2018.07.040 ↗
45. Elastic stress impacting on the rust layer of S450EW weathering steel through magnetomechanical effect
46. The NBS tables of chemical thermodynamic properties
47. Electrochemical aspects of copper atmospheric corrosion in the presence of sodium chloride10.1016/j.electacta.2018.04.184 ↗
48. Some properties of copper and selected heavy metal sulfides. A limited literature review
49. Microstructure and elemental composition of electrochemically formed dendrites on lead-free micro-alloyed low Ag solder alloys used in electronics10.1016/j.corsci.2014.11.004 ↗
50. Electrochemical behavior of InSb thin films with different crystal structure in alkaline solution10.1016/j.electacta.2019.02.050 ↗
51. Young · 2019
52. Antimony in the metallurgical industry: a review of its chemistry and environmental stabilization options10.1016/j.hydromet.2016.06.014 ↗
53. Comparative studies on the codeposition of antimony and tin from acidic chloride and sulfate-chloride solutions
54. Theoretical simulation and experimental study of hydrolysis separation of SbCl3 in complexation–precipitation system10.1016/S1003-6326(16)64370-4 ↗
55. Stability constants of Sb5+ with Cl− and thermodynamics of Sb−S−Cl−H2O system involving complex behavior of Sb with Cl10.1016/S1003-6326(20)65469-3 ↗
56. Thermal decomposition of antimony oxyhalides: I. Oxychlorides10.1007/BF01904648 ↗
57. Corrosion behaviour of copper containing low alloy steels in sulphuric acid10.1016/j.corsci.2011.09.012 ↗
58. Roles of chloride ion in microvia filling by copper electrodeposition: I. studies using SEM and optical microscope10.1149/1.1849934 ↗
59. Behavior of antimony (III) during copper electrowinning in chloride solutions10.1007/BF02915041 ↗
60. Cathodic behaviour of antimony (III) species in chloride solutions10.1007/BF00578091 ↗