journal article·2002-02

Stability of protective oxide films in waste incineration environment—solubility measurement of oxides in molten chlorides

Tetsuo Ishitsuka, Koichi Nose

Corrosion Science· Volume 44· Issue 2
Publisher page

Abstract

Solubility measurements of several oxides in molten NaCl–KCl and NaCl–KCl–Na2SO4–K2SO4 were conducted in three different levels of basicity. The dissolution behavior of the oxides showed almost the same tendency as that shown by the dissolution behavior of the oxides in molten Na2SO4 in literature. In a waste incineration environment, a protective Cr2O3 film easily dissolves in molten chlorides as CrO42− because pO2− of the molten chlorides tends to have a small value due to the effect of water vapor contained in the combustion gas. From the result of the solubility measurement, the addition of molybdenum and/or silicon was expected to improve the corrosion resistance of alloys. Laboratory corrosion tests confirmed this expectation. However, the scale analysis suggested that the effect of molybdenum could not be explained completely by only the mechanism derived from the result of the solubility measurement.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear materials and radiation effects · Recycling and utilization of industrial and municipal waste in materials production · Molten salt chemistry and electrochemical processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Nishimoto · Hitachi Hyoron · 1970 · 52 · 326
2. Sakai · Boshoku Gijutsu · 1976 · 25 · 137
3. P.L. Daniel, J.L. Barna, J.D. Blue, Proceedings National Waste Processing Conference, 1986, p. 221
4. J.A. Harris, W.G. Lipscomb, G.D. Smith, Corrosion/87, NACE International, paper no. 402, 1987
5. H.H. Krause, Corrosion/91, NACE International, paper no. 242, 1991
6. W.G. Schuetzenduebel, I.E. Johnson, C.W. Clemons, H. Thielsch, Corrosion/91, NACE International, paper no. 244, 1991
7. Gupta · J. Electrochem. Soc. · 1980 · 127 · 219410.1149/1.2129374 ↗
8. Gupta · J. Electrochem. Soc. · 1980 · 127 · 265610.1149/1.2152132 ↗
9. Zhang · J. Electrochem. Soc. · 1985 · 132 · 73410.1149/1.2113943 ↗
10. Zhang · J. Electrochem. Soc. · 1985 · 132 · 249810.1149/1.2113608 ↗
11. Shi · J. Electrochem. Soc. · 1986 · 133 · 84910.1149/1.2108692 ↗
12. Rapp · Mater. Sci. Engng. · 1987 · 87 · 31910.1016/0025-5416(87)90394-6 ↗
13. Deanhardt · J. Electrochem. Soc. · 1981 · 128 · 257710.1149/1.2127295 ↗
14. Zhang · J. Electrochem. Soc. · 1986 · 133 · 65510.1149/1.2108648 ↗
15. Ota · Molten Salts · 1991 · 34 · 135
16. Takahashi · Molten Salts · 1994 · 37 · 215
17. Combes · C.R. Acad. Sci. · 1971 · 273 · 1740
18. Combes · Electrochim. Acta · 1975 · 20 · 19110.1016/0013-4686(75)85024-9 ↗
19. Kanzaki · J. Electronal. Chem. · 1975 · 58 · 33910.1016/S0022-0728(75)80091-X ↗
20. A. Momma, S. Haruyama, Nippon Kagaku Kaishi (1982) 1029 (in Japanese)10.1246/nikkashi.1982.1029 ↗
21. Urabe · Zairyo to Kankyo · 1993 · 42 · 39310.3323/jcorr1991.42.393 ↗
22. Y. Kawahara, K. Takahashi, Y. Nakagawa, T. Hosoda, T. Mizuko, Corrosion/2000, NACE International, paper no. 265, 200010.1299/jsmeenv.2000.10.309 ↗
23. A. Show, K. Tayama, K. Nagashima, M. Yoshiba, Proceedings International Symposium on High-Temperature Corrosion and Protection 2000, 2000, p. 443