Stress corrosion cracking of E690 steel as a welded joint in a simulated marine atmosphere containing sulphur dioxide
Source abstract
Abstract
Stress corrosion cracking (SCC) behavior and mechanism of E690 welded joint in simulated marine atmosphere containing SO2 were investigated using SSRT method and electrochemical measurements. Results showed that it had very high SCC susceptibility in this environment with a combined mechanism of anodic dissolution and hydrogen embrittlement (HE). The intercritical heat affected zone in the welded joint was the most vulnerable location to SCC because this zone has less strength, more negative potential, and higher corrosion current density. The M-A constituents had a detrimental effect on SCC behavior in the synergetic effect of stress concentration, micro-galvanic corrosion, and HE.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Failure analysis of a rock anchor made of stainless steel in marine environment10.1016/j.engfailanal.2011.09.011 ↗
2. Stress corrosion cracking of some steels in various environments10.1016/0013-7944(89)90203-8 ↗
3. SCC evaluation of type 304 and 316 austenitic stainless steels in acidic chloride solutions using the slow strain rate technique10.1016/j.corsci.2003.08.001 ↗
4. Risk assessment and evaluation of materials commonly used in desalination plants subjected to stress corrosion cracking in polluted marine environment10.1016/S0011-9164(02)01138-4 ↗
5. Stress corrosion cracking of A537 steel in simulated marine environments10.1016/j.corsci.2012.08.025 ↗
6. Study on stress corrosion crack of austenitic stainless steel in simulated ocean environment10.1016/j.proeng.2011.12.618 ↗
7. The initiation and propagation of chloride-induced transgranular stress-corrosion cracking (TGSCC) of 304L austenitic stainless steel under atmospheric conditions10.1016/j.corsci.2014.07.017 ↗
8. Hydrogen permeation and corrosion behavior of high strength steel MCM 430 in cyclic wet–dry SO2 environment10.1016/S0010-938X(03)00141-0 ↗
9. Hydrogen entry into steel during atmospheric corrosion process10.1016/j.corsci.2004.10.006 ↗
10. Atmospheric stress corrosion of 40CrNi2Si2MoVA steel
11. Mechanical properties and marine atmosphere corrosion behavior of E690 ocean platform steel
12. Strength effect in stress corrosion cracking of high-strength steel in aqueous solution10.5006/1.3290352 ↗
13. Some effects of yield strength on the stress corrosion cracking behaviour of low alloy steels in aqueous environments at ambient temperatures10.1016/j.engfailanal.2004.03.006 ↗
14. Corrosion of simulated weld HAZ of API X-80 pipeline steel10.1016/j.corsci.2012.06.014 ↗
15. Microstructure and stress corrosion cracking of the fusion boundary region in an alloy 182-A533B low alloy steel dissimilar weld joint10.1016/j.corsci.2010.08.002 ↗
16. Metallurgical investigations and corrosion behavior of failed weld joint in AISI 1518 low carbon steel pipeline10.1016/j.engfailanal.2015.03.015 ↗
17. Stress corrosion cracking in the heat-affected zone of A508 steel welds under high-temperature water10.1016/j.jnucmat.2010.10.052 ↗
18. GB/T 15970.7, Corrosion of metals and alloys—Stress corrosion testing—Part 7: Slow strain rate testing, Chinese National Standard, 2000.
19. Effect of inclusions on initiation of stress corrosion cracks in X70 pipeline steel in an acidic soil environment10.1016/j.corsci.2009.01.007 ↗
20. The role of TiN inclusions in stress corrosion crack initiation for Alloy 690TT in high-temperature and high-pressure water10.1016/j.corsci.2009.11.015 ↗
21. Validation of corrosion rates measured by the Tafel extrapolation method10.1016/j.corsci.2005.05.046 ↗
22. Numerical modeling of micro-galvanic corrosion10.1016/j.electacta.2010.09.044 ↗
23. Influence of peak temperature during simulation and real thermal cycles on microstructure and fracture properties of the reheated zones10.1016/j.matdes.2009.12.023 ↗
24. Effect of weld peak temperature on the microstructure, hardness, and transformation kinetics of simulated heat affected zone of hot rolled ultra-low carbon high strength Ti–Mo ferritic steel10.1016/j.matdes.2014.04.003 ↗
25. Effect of tandem submerged arc welding process and parameters of Gleeble simulator thermal cycles on properties of the intercritically reheated heat affected zone10.1016/j.matdes.2010.07.005 ↗
26. In situ corrosion characterization of simulated weld heat affected zone on API X80 pipeline steel10.1016/j.corsci.2014.04.053 ↗
27. Atomic mobilities, uphill diffusion and proeutectic ferrite growth in Fe–Mn–C alloys10.1016/j.calphad.2009.07.002 ↗
28. Effects of Mo, Cr and Nb on microstructure and mechanical properties of heat affected zone for Nb-bearing X80 pipeline steels10.1016/j.matdes.2013.07.037 ↗
29. Microstructure and toughness of the CGHAZ of an offshore platform steel10.1016/j.jmatprotec.2014.12.017 ↗
30. Correlation between microstructure, hardness and strength in HAZ of dissimilar welds of rotor steels10.1016/j.msea.2010.03.066 ↗
31. Microstructural evolution and mechanical properties of friction stir welded joint of Fe–Cr–Mn–Mo–N austenite stainless steel10.1016/j.matdes.2014.07.063 ↗
32. Variations of microstructure and properties of 690MPa grade low carbon bainitic steel after tempering10.1016/j.msea.2012.07.113 ↗
33. The effect of nonmetal inclusions and microstructure on local corrosion of carbon and low-alloyed steels10.1023/B:PROM.0000043062.19272.c5 ↗
34. On the influence of microstructure and carbide content of steels on the electrochemical dissolution process in aqueous NaCl-electrolytes10.1002/1521-4176(200210)53:10<740::AID-MACO740>3.0.CO;2-J ↗
35. The effect of microstructure and non-metallic inclusions on corrosion behavior of low carbon steel in chloride containing solutions10.1016/j.corsci.2013.11.038 ↗
36. Rusting evolution of Mn–Cu alloying steel in a simulated coastal environment
37. Impact of SO2 concentration on the corrosion rate of X70 steel and iron in water-saturated supercritical CO2 mixed with SO210.1016/j.supflu.2011.06.007 ↗
38. Role of climatic conditions on corrosion characteristics of structural steels10.1016/j.corsci.2007.06.026 ↗
39. Effect of sulphur dioxide on the corrosion of a low alloy steel in simulated coastal industrial atmosphere10.1016/j.corsci.2014.02.010 ↗
40. Initial stages of atmospheric corrosion of steel in the Arabian Gulf10.1016/0010-938X(91)90123-7 ↗
41. Evaluation of hydrogen entry into high strength steel under atmospheric corrosion10.1016/j.corsci.2009.11.046 ↗
42. Hydrogen entry into Fe and high strength steels under simulated atmospheric corrosion10.1016/j.electacta.2010.09.043 ↗
43. Effect of cathodic potentials on the SCC behavior of E690 steel in simulated seawater10.1016/j.msea.2015.05.109 ↗
44. Correlation of martensite–austenite constituent and cleavage crack initiation in welding heat affected zone of low carbon bainitic steel10.1016/j.matlet.2014.03.123 ↗
45. Investigation on tempering of granular bainite in an offshore platform steel10.1016/j.msea.2014.12.074 ↗
46. Influence of prior austenite grain size on martensite–austenite constituent and toughness in the heat affected zone of 700MPa high strength linepipe steel10.1016/j.msea.2014.07.100 ↗
47. Variations of work function and corrosion behaviors of deformed copper surfaces10.1016/j.apsusc.2004.07.017 ↗
48. High-resolution Kelvin probe microscopy in corrosion science: scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
49. SVET, SKP and EIS study of the corrosion behaviour of high strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
50. Corrosion of X100 pipeline steel under plastic strain in a neutral pH bicarbonate solution10.1016/j.corsci.2012.07.012 ↗
51. Effect of tensile strain on the rate of marine corrosion of steel plates10.1016/j.corsci.2009.06.010 ↗
52. Stainless steel pitting and early-stage stress corrosion cracking under ultra-low elastic load10.1016/j.corsci.2013.08.028 ↗
53. Effect of bainitic microstructure on the susceptibility of pipeline steels to hydrogen induced cracking10.1016/j.msea.2011.03.036 ↗
54. Hydrogen embrittlement of high strength steels: determination of the threshold stress intensity for small cracks nucleating at nonmetallic inclusions10.1016/j.engfracmech.2012.10.028 ↗
55. Mechanistic aspect of near-neutral pH stress corrosion cracking of pipelines under cathodic polarization10.1016/j.corsci.2011.10.002 ↗
56. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
57. Effects of tungsten on the hydrogen embrittlement behaviour of microalloyed steels10.1016/j.corsci.2014.01.042 ↗