A room temperature cured sol–gel anticorrosion pre-treatment for Al 2024-T3 alloys
Source abstract
Abstract
The inherent reactivity of the Al-Cu alloys is such that their use for structural, marine, and aerospace components and structures would not be possible without prior application of a corrosion protection system. Historically these corrosion protection systems have been based upon the use of chemicals containing Cr(VI) compounds. Organic-inorganic hybrid silane coatings are of increasing interest in industry due to their potential application for the replacement of current toxic hexavalent chromate based treatments. In the present study, a hybrid epoxy-silica-alumina coating with or without doped cerium nitrate has been prepared using a sol-gel method. The hybrid coatings were applied by a dip-technique to an Al-Cu alloy, Al 2024-T3, and subsequently cured at room temperature. The anticorrosion properties of the coatings within 3.5% NaCl were studied using electrochemical impedance spectroscopy (EIS), and conventional DC polarisation. An exfoliation test method involving immersion in a solution of 4 M NaCl, 0.5 M KNO3 and 0.1 M HNO3 was also used. The cerium nitrate doped sol-gel coating exhibited excellent anticorrosion properties providing an adherent protection film on the Al 2024-T3 substrate. The resistance to corrosion of the sol-gel coating was also evaluated by analysing the morphology of the coating before and after corrosion testing using scanning electron microscopy. © 2007 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Twite · Prog. Org. Coat. · 1998 · 33 · 9110.1016/S0300-9440(98)00015-0 ↗
2. Fracassi · Surf. Coat. Technol. · 2003 · 174 · 10710.1016/S0257-8972(03)00422-5 ↗
3. Vacandio · Surf. Coat. Technol. · 2001 · 137 · 28410.1016/S0257-8972(00)01110-5 ↗
4. Zheludkevich · J. Mater. Chem. · 2005 · 15 · 509910.1039/b419153f ↗
5. Blawert · Surf. Coat. Technol. · 2005 · 200 · 6810.1016/j.surfcoat.2005.02.035 ↗
6. Pepe · J. Non-Cryst. Solids · 2004 · 348 · 16210.1016/j.jnoncrysol.2004.08.141 ↗
7. Khramov · Prog. Org. Coat. · 2003 · 47 · 20710.1016/S0300-9440(03)00140-1 ↗
8. Metroke · Prog. Org. Coat. · 2004 · 50 · 23110.1016/j.porgcoat.2004.03.001 ↗
9. Khramov · Thin Solid Films · 2004 · 447–448 · 54910.1016/j.tsf.2003.07.016 ↗
10. Zheludkevich · Electrochim. Acta · 2005 · 51 · 20810.1016/j.electacta.2005.04.021 ↗
11. Lamaka · Electrochem. Commun. · 2006 · 8 · 42110.1016/j.elecom.2005.12.019 ↗
12. Shchukin · Adv. Mater. · 2006 · 18 · 167210.1002/adma.200502053 ↗
13. Kasten · Surf. Coat. Technol. · 2001 · 140 · 1110.1016/S0257-8972(01)01004-0 ↗
14. Aramaki · Corros. Sci. · 2005 · 47 · 128510.1016/j.corsci.2004.05.022 ↗
15. Wang · Mater. Chem. Phys. · 2003 · 77 · 80210.1016/S0254-0584(02)00142-6 ↗
16. Voevodin · Surf. Coat. Technol. · 2001 · 140 · 2410.1016/S0257-8972(01)00999-9 ↗
17. Barranco · Corros. Sci. · 2004 · 46 · 220310.1016/j.corsci.2003.09.032 ↗
18. Fedrizzi · Electrochim. Acta · 2006 · 51 · 186410.1016/j.electacta.2005.02.146 ↗
19. Mansfeld · J. Electrochem. Soc. · 1988 · 135 · 82810.1149/1.2095786 ↗
20. H.M. Wang, R. Akid. Corros. Sci., submitted for publication.
21. Hinton · J. Alloys Compd. · 1992 · 180 · 1510.1016/0925-8388(92)90359-H ↗
22. Arenas · Electrochim. Acta · 2003 · 48 · 369310.1016/S0013-4686(03)00507-3 ↗
23. Aldykiewicz · J. Electrochem. Soc. · 1996 · 143 · 14710.1149/1.1836400 ↗
24. Montemor · Prog. Org. Coat. · 2002 · 44/1 · 79
25. Trabelsi · Prog. Org. Coat. · 2005 · 54 · 27610.1016/j.porgcoat.2005.07.006 ↗
26. Exfoliation corrosion susceptibility in 2xxx and 7xxx series aluminium alloys (EXCO test), American Society for Testing and Materials, Annual Book of ASTM Standards, 1985.