Abstract
Abstract The effect of dispersed nanosized spherical NbC precipitates (∼10 nm) on the hydrogen embrittlement (HE) of martensitic steel was investigated by slow strain rate tests, hydrogen permeation tests, atom probe tomography and microstructural examination. HE susceptibility decreases as the amount of NbC increases. NbC plays dual roles in HE. Primarily, NbC alleviates hydrogen accumulation in other areas via hydrogen traps which are induced by NbC directly and increased by the additional grain boundaries resulting from NbC, inhibiting the hydrogen-enhanced decohesion. Moreover, NbC impedes the hydrogen-enhanced localized plasticity by pinning hydrogen-dislocation atmospheres and reducing Σ3 boundary fraction. Secondarily, NbC weakens the beneficial {111}//ND texture, reduces the crack-propagation resistance, and plays a harmful role.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (84)
Show source-provided references
1. Effect of heat treatment on hydrogen-assisted fracture behavior of PH13-8Mo steel10.1016/j.corsci.2017.09.018 ↗
2. Evaluation of susceptibility of high strength steels to delayed fracture by using cyclic corrosion test and slow strain rate test10.1016/j.corsci.2010.02.005 ↗
3. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
4. Further study of the hydrogen embrittlement of martensitic advanced high-strength steel in simulated auto service conditions10.1016/j.corsci.2018.02.037 ↗
5. Hydrogen transport and embrittlement in 300 M and AerMet100 ultra high strength steels10.1016/j.corsci.2010.01.001 ↗
6. Hydrogen embrittlement assessment of ultra-high strength steel 30CrMnSiNi210.1016/j.corsci.2013.08.013 ↗
7. Hydrogen embrittlement of metals: a primer for the failure analyst, J. Fail
8. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
9. Hydrogen absorption and embrittlement of ultra-high strength aluminized press hardening steel10.1016/j.msea.2018.08.003 ↗
10. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
11. Hydrogen influence on some advanced high-strength steels10.1016/j.corsci.2017.06.012 ↗
12. Hydrogen embrittlement, internal stress and defects in steel
13. The role of hydrogen and other interstitials in the mechanical behavior of metals
14. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
15. Hydrogen related failure of steels – a new aspect10.1179/026708304225019687 ↗
16. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
17. The effect of hydrogen on dislocation dynamics10.1016/S0013-7944(01)00011-X ↗
18. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process10.1016/0001-6160(88)90113-7 ↗
19. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
20. Microstructural and crystallographic study of hydrogen-assisted cracking in high strength PSB1080 steel10.1016/j.ijhydene.2018.07.158 ↗
21. Hydrogen damage of steels: a case study and hydrogen embrittlement model10.1016/j.engfailanal.2015.05.017 ↗
22. Hydrogen trapping on non metallic inclusions in cr-mo low alloy steels10.1016/S0010-938X(98)00008-0 ↗
23. Influence of macro segregation on hydrogen environment embrittlement of SUS 316L stainless steel10.1016/j.ijhydene.2009.02.015 ↗
24. Effect of grain boundary engineering on hydrogen embrittlement in Fe-Mn-C TWIP steel at various strain rates10.1016/j.corsci.2018.07.028 ↗
25. Developing bearing steels combining hydrogen resistance and improved hardness10.1016/j.matdes.2012.07.030 ↗
26. Hydrogen environment embrittlement of an ODS RAF steel–Role of irreversible hydrogen trap sites10.1016/j.ijhydene.2010.06.071 ↗
27. Effects of tungsten on the hydrogen embrittlement behaviour of microalloyed steels10.1016/j.corsci.2014.01.042 ↗
28. The effect of carbon on hydrogen embrittlement in stable Cr-Ni-Mn-N austenitic stainless steels10.1016/j.corsci.2017.05.004 ↗
29. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
30. Effects of titanium content on hydrogen embrittlement susceptibility of hot-stamped boron steels10.1016/j.jallcom.2017.12.004 ↗
31. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
32. Effects of vanadium carbides on hydrogen embrittlement of tempered martensitic steel10.1007/s12540-016-5631-7 ↗
33. Influence of vanadium on the hydrogen embrittlement of aluminized ultra-high strength press hardening steel10.1016/j.msea.2018.08.027 ↗
34. Effect of Nb on hydrogen-induced delayed fracture in high strength hot stamping steels10.1016/j.msea.2014.12.051 ↗
35. Effect of niobium precipitation behavior on microstructure and hydrogen induced cracking of press hardening steel 22MnB510.1016/j.msea.2018.02.021 ↗
36. A focus on different factors affecting hydrogen induced cracking in oil and natural gas pipeline steel10.1016/j.engfailanal.2017.05.022 ↗
37. Effect of arisen dislocation density and texture components during cold rolling and annealing treatments on hydrogen induced cracking susceptibility in pipeline steel10.1557/jmr.2016.357 ↗
38. Hydrogen-induced cracking assessment in pipeline steels through permeation and crystallographic texture measurements10.1007/s11665-016-2021-8 ↗
39. Hydrogen trapping phenomena in martensitic steels, Gaseous HE of materials in energy technologies
40. Quantitative Analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
41. Nano-precipitates design with hydrogen trapping character in high strength steels
42. Correlation between vanadium carbide size and hydrogen trapping in ferritic steel10.1016/j.scriptamat.2018.04.013 ↗
43. Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel10.1016/j.actamat.2018.05.003 ↗
44. The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography10.1016/j.scriptamat.2010.03.012 ↗
45. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel10.1126/science.aal2418 ↗
46. The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel10.1016/j.actamat.2017.08.011 ↗
47. Direct observation of hydrogen-trapping sites in newly developed high-strength mooring chain steel by atom probe tomography10.1016/j.pnsc.2013.06.005 ↗
48. Carbides and possible hydrogen irreversible trapping sites in ultrahigh strength round steel10.1016/j.micron.2017.09.005 ↗
49. Hydrogen diffusion and trapping in V-microalloyed mooring chain steels10.1016/j.matlet.2017.11.029 ↗
50. Thermal desorption spectroscopy evaluation of the hydrogen trapping capacity of NbC and NbN precipitates10.1007/s11661-013-2181-1 ↗
51. Modelling hydrogen migration and trapping in steels10.1016/j.matdes.2016.05.051 ↗
52. The effect of dislocation contrast on x-ray line broadening: a new approach to line profile analysis10.1063/1.117951 ↗
53. The mechanism of hydrogen evolution on iron in acid solutions by determination of permeation rates10.1149/1.2426195 ↗
54. Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking10.1016/j.ijhydene.2009.09.090 ↗
55. Critical hydrogen concentration for hydrogen-induced blistering on AISI 430 stainless steel10.1016/S0254-0584(03)00084-1 ↗
56. Dissolution and precipitation behaviour in steels microalloyed with niobium during thermomechanical processing10.1016/j.actamat.2015.06.057 ↗
57. Precipitation hardening in metals10.1179/026708399773002782 ↗
58. Influence of hydrogen on mechanical properties and fracture of tempered 13 wt% Cr martensitic stainless steel10.1016/j.msea.2017.05.086 ↗
59. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
60. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and quasi-cleavage fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
61. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
62. Hydrogen embrittlement of low carbon structural steel10.1016/j.mspro.2014.06.190 ↗
63. A review of strain analysis using Electron backscatter Diffraction10.1017/S1431927611000055 ↗
64. Crystallographic feature of hydrogen-related fracture in 2Mn-0.1C ferritic steel10.1016/j.ijhydene.2018.05.011 ↗
65. 3D structural and atomic-scale analysis of lath martensite: effect of the transformation sequence10.1016/j.actamat.2015.05.023 ↗
66. Microstructures and hardness of as-quenched martensites (0.1–0.5%C)10.1016/j.actamat.2011.05.061 ↗
67. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
68. Hydrogen trapping in an API 5L X6010.1016/j.corsci.2011.09.008 ↗
69. Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel10.1016/j.corsci.2018.04.041 ↗
70. Hydrogen trapping in high strength martensitic steel after austenitized at different temperatures10.1016/j.ijhydene.2013.08.121 ↗
71. Effect of quenching temperature on sulfide stress cracking behavior of martensitic steel10.1016/j.msea.2018.03.063 ↗
72. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
73. Texture and grain boundary study in high strength Fe–18Ni–Co steel related to hydrogen embrittlement10.1016/j.matdes.2015.11.093 ↗
74. Role of lattice strain and texture in hydrogen embrittlement of 18Ni (300) maraging steel10.1016/j.ijhydene.2017.03.209 ↗
75. Effect of precipitate dispersion on recrystallization texture of niobium-added extra-low carbon cold-rolled steel sheet10.2355/isijinternational1966.26.737 ↗
76. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
77. On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels10.1016/j.corsci.2011.08.031 ↗
78. Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking10.1016/j.msea.2014.10.009 ↗
79. Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
80. A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies10.1016/j.corsci.2008.10.006 ↗
81. Role of microtexture in the interaction and coalescence of hydrogen-induced cracks10.1016/j.corsci.2009.02.010 ↗
82. New insight into high-temperature creep deformation and fracture of T92 steel involving precipitates, dislocations and nanovoid10.1016/j.matchar.2017.01.025 ↗
83. The effect of nanosized (Ti,Mo)C precipitates on hydrogen embrittlement of tempered lath martensitic steel10.1016/j.actamat.2014.04.051 ↗
84. Effect of vanadium content on hydrogen diffusion behaviors and hydrogen induced ductility loss of X80 pipeline steel10.1016/j.msea.2018.09.048 ↗