Abstract
Abstract Different charging conditions aimed at introducing significant hydrogen concentrations without microstructural damages in a 316L austenitic stainless steel were investigated. The equivalent hydrogen pressure developed at the surface of the samples during cathodic charging was estimated from hydrogen concentration measurements. A clear hydrogen absorption, controlled by diffusion, was evidenced during the immersion of 316L steel samples in 30% MgCl 2 at the open circuit potential at 117 °C. Deuterium profiling by SIMS was performed to check the validity of the few literature data on hydrogen diffusivity in the near room temperature range in this material. On the other hand, the macroscopic effects of hydrogen on the tensile characteristics of the steel were investigated and compared at 20 °C and at −196 °C with samples cathodically pre-charged, charged during tensile straining or pre-charged at high temperature–high pressure in gas phase. Hydrogen is shown to affect both the short range and the long range forces exerted on the strain-induced mobile dislocations. The hydrogen-induced softening effect observed at 20 °C and the systematic decrease of the ductility support a mechanism involving the enhanced transport of hydrogen atoms by mobile dislocations. This mechanism is confirmed by the absence of softening and of ductility loss at −196 °C and by the strain-enhanced tritium desorption from samples cathodically pre-charged with tritium, measured by β counting during tensile deformation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Chêne · Bull. Cercle Et. Met. · 1980 · 16-1/16-12 · 1419
2. Caskey · Scripta Metall. · 1981 · 15 · 118310.1016/0036-9748(81)90294-5 ↗
3. Some solutions to hydrogen embrittlement problems in Fe Ni Cr austenitic structures
4. Hydrogen damage in stainless steel
5. Rozenak · Acta Metall. · 1990 · 38 · 203110.1016/0956-7151(90)90070-W ↗
6. Ferreira · Acta Mater. · 1998 · 46 · 174910.1016/S1359-6454(97)00349-2 ↗
7. Ulmer · Acta Metall. · 1991 · 39 · 123710.1016/0956-7151(91)90211-I ↗
8. Abraham · Metall. Mater. Trans. · 1995 · 26A · 284910.1007/BF02669643 ↗
9. Abraham · Metall. Mater. Trans. · 1995 · 26A · 285910.1007/BF02669644 ↗
10. Shivanyuk · Mater. Sci. Eng. A · 2001 · 300 · 28410.1016/S0921-5093(00)01442-8 ↗
11. Effect of hydrogen on plastic deformation of stable 18Cr–16Ni–10Mn austenitic stainless steel single crystals
12. Gavriljuk · Acta Mater. · 2003 · 51 · 129310.1016/S1359-6454(02)00524-4 ↗
13. Katz · Eng. Fract. Mech. · 2001 · 68 · 64610.1016/S0013-7944(00)00119-3 ↗
14. G. Girardin, Thèse Ecole Nationale Supérieure des Mines de Saint-Etienne, France no. 334TD, 2004.
15. M. Ménard, J.-M Olive, A.-M Brass, I. Aubert, Effects of hydrogen on surface slip band morphology of a type 316L stainless steel, in: Proceedings of the second NACE International Conference on Environmental-Induced cracking of metals (EICM-2), Banff, Alberta, Canada, 19–23 September 2004.
16. Hardie · Corr. Sci. · 2004 · 46 · 308910.1016/j.corsci.2004.03.017 ↗
17. Zackroczymski · Corr. Sci. · 2005 · 47 · 140310.1016/j.corsci.2004.07.036 ↗
18. Sofronis · J. Mech. Phys. Solids · 2001 · 43 · 4910.1016/0022-5096(94)00056-B ↗
19. Château · Acta Mater. · 2002 · 50 · 150710.1016/S1359-6454(02)00008-3 ↗
20. Mechanisms of hydrogen related fracture of metals
21. Magnin · Acta Mater. · 1996 · 44 · 145710.1016/1359-6454(95)00301-0 ↗
22. La corrosion sous contrainte des aciers inoxydables
23. Interactions of hydrogen with moving dislocations in Ni base alloys. Consequences on the intergranular rupture
24. P. Tison, Influence de l’hydrogène sur le comportement des métaux, in: CEA Service de documentation, Saclay, France (Ed.), CEA-R-5240 (1), ISSN 0429-3460, 1984, pp.1–303.
25. Louthan · Corros. Sci. · 1975 · 15 · 56510.1016/0010-938X(75)90022-0 ↗
26. Quick · Metal Trans. · 1979 · 10A · 6710.1007/BF02686408 ↗
27. Forcey · J. Nucl. Mater. · 1988 · 160 · 11710.1016/0022-3115(88)90038-4 ↗
28. J. Chêne, A.-M. Brass, in press.
29. Bockris · Electrochim. Acta · 1971 · 16 · 216910.1016/0013-4686(71)85027-2 ↗
30. Brass · Metall. Trans. · 2004 · 35A · 144910.1007/s11661-004-0253-y ↗
31. Griffiths · Corros. Sci. · 1995 · 37 · 187910.1016/0010-938X(95)00077-W ↗
32. Miyazaki · Acta Metall. · 1979 · 27 · 85510.1016/0001-6160(79)90120-2 ↗
33. Feaugas · Metall. Mater. Trans. · 2003 · 34A · 232910.1007/s11661-003-0296-5 ↗
34. Brass · Mater. Sci. Eng. A · 2002 · 323 · 9710.1016/S0921-5093(01)01349-1 ↗
35. Donovan · Metall. Trans. A · 1976 · 7 · 167710.1007/BF02817885 ↗
36. Hydrogen transport by deformation and hydrogen embrittlement in selected stainless steels
37. Calder · J. Nucl. Mater. · 1973 · 46 · 4610.1016/0022-3115(73)90121-9 ↗
38. Role of grain boundaries and cold work on hydrogen permeation in nickel
39. Li · Corros. Sci. · 2003 · 45 · 135510.1016/S0010-938X(02)00225-1 ↗
40. Feaugas · Acta Mater. · 1999 · 47 · 361710.1016/S1359-6454(99)00222-0 ↗