Mechanistic studies of corrosion product flaking on copper and copper-based alloys in marine environments
Source abstract
Abstract
The mechanism of corrosion product flaking on bare copper sheet and three copper-based alloys in chloride rich environments has been explored through field and laboratory exposures. The tendency for flaking is much more pronounced on Cu and Cu–4 wt%Sn than on Cu–15 wt%Zn and Cu–5 wt%Al–5 wt%Zn. This difference is explained by the initial formation of zinc and zinc–aluminum hydroxycarbonates on Cu15Zn and Cu5Al5Zn, which delays the formation of CuCl, a precursor of Cu2(OH)3Cl. As a result, the observed volume expansion during transformation of CuCl to Cu2(OH)3Cl, and concomitant corrosion product flaking, is less severe on Cu15Zn and Cu5Al5Zn than on Cu and Cu4Sn.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Materials Engineering and Processing · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. The evolution of outdoor copper patina10.1016/S0010-938X(01)00081-6 ↗
2. Morphological study of 16-year patinas formed on copper in a wide range of atmospheric exposures10.1016/j.corsci.2007.05.030 ↗
3. Some aspects of the atmospheric corrosion of copper in the presence of sodium chloride10.1149/1.1838422 ↗
4. Evolution of patinas on copper exposed in a suburban area10.1016/j.corsci.2006.05.044 ↗
5. Corrosion of copper in seawater and its aerosols in a tropical island10.1016/j.corsci.2004.05.015 ↗
6. Atmospheric corrosion of brass in outdoor applications: patina evolution, metal release and aesthetic appearance at urban exposure conditions10.1016/j.scitotenv.2011.09.083 ↗
7. Corrosion-induced copper runoff from naturally and pre-patinated copper in a marine environment10.1016/j.corsci.2006.04.004 ↗
8. Effect of carbon dioxide on sodium chloride-induced atmospheric corrosion of copper10.1149/1.2098327 ↗
9. The characterization of a corroded Egyptian bronze statue and a study of the degradation phenomena
10. Chlorides and basic chlorides
11. A review of copper chlorides and related salts in bronze corrosion and as painting pigments10.1179/sic.2000.45.1.39 ↗
12. Electrochemical and spectroscopic characterizations of patinas formed on an archaeological bronze coin10.1016/j.electacta.2005.01.050 ↗
13. The characterization of Sn-based corrosion products in ancient bronzes: a Raman approach10.1002/jrs.4037 ↗
14. Initial oxidation of brass induced by humidified air10.1016/j.apsusc.2011.09.080 ↗
15. Corrosion and runoff rates of Cu and three Cu-alloys in marine environments with increasing chloride deposition rate10.1016/j.scitotenv.2013.11.080 ↗
16. Reaction sequences in atmospheric corrosion of zinc
17. Atmospheric corrosion of Galfan coatings on steel in chloride-rich environments10.1016/j.corsci.2013.03.025 ↗
18. The initial release of zinc and aluminum from non-treated Galvalume and the formation of corrosion products in chloride containing media10.1016/j.apsusc.2011.12.112 ↗
19. Atmospheric corrosion of copper and copper-base alloys during twenty years’ exposure in a marine and an industrial environment
20. The use of synchrotron X-rays to observe copper corrosion in real time10.1021/ac300457e ↗
21. An in-situ X-ray absorption spectroelectrochemistry study of the response of artificial chloride corrosion layers on copper to remedial treatment10.1039/B814181A ↗
22. Effect of sodium chloride particles on the atmospheric corrosion of pure copper10.5006/1.3299244 ↗
23. Quantitative in situ analysis of initial atmospheric corrosion of copper induced by acetic acid10.1149/1.2715315 ↗
24. Simultaneous infrared reflection absorption spectroscopy and quartz crystal microbalance measurements for in situ studies of the metal/atmosphere interface10.1149/1.1837948 ↗
25. Surface characterization of artificial corrosion layers on copper alloy reference materials10.1016/S0169-4332(02)00005-3 ↗
26. Micro Raman spectroscopy used for the study of corrosion products on copper alloys: study of the chemical composition of artificial patinas used for restoration purposes10.1039/b419080g ↗
27. Formation processes of CuCl and regenerated Cu crystals on bronze surfaces in neutral and acidic media10.1016/j.apsusc.2005.08.041 ↗
28. Raman spectroscopy of selected copper minerals of significance in corrosion10.1016/S1386-1425(02)00315-3 ↗
29. Raman spectroscopy of the copper chloride minerals nantokite, eriochalcite and claringbullite – implications for copper corrosion10.1127/0028-3649/2003/2003-0433 ↗
30. Combined effects of gaseous pollutants and sodium chloride particles on the atmospheric corrosion of copper10.5006/1.3280618 ↗
31. Raman spectra of CuO nanocrystals10.1002/(SICI)1097-4555(199905)30:5<413::AID-JRS387>3.0.CO;2-N ↗
32. The contrastive studies of microwave and conventional roasting CuCl residue from zinc hydrometallurgy
33. Direct chlorination of carbon by copper chloride in a thermal process10.1021/es802996a ↗
34. Raman investigation of artificial patinas on recent bronze – part II: urban rain exposure10.1002/jrs.4124 ↗
35. Corrosion product formation on Zn55Al coated steel upon exposure in a marine atmosphere10.1016/j.corsci.2010.11.004 ↗
36. Synthesis and vibrational spectroscopic characterisation of synthetic hydrozincite and smithsonite10.1016/j.poly.2007.07.002 ↗
37. Thermo-Raman spectroscopy of selected layered double hydroxides of formula Cu6Al2(OH)16CO3 and Zn6Al2(OH)16CO310.1002/jrs.2148 ↗
38. Spatial distribution and formation of corrosion products in relation to zinc release for zinc sheet and coated pre-weathered zinc at an urban and a marine atmospheric condition10.1002/maco.201106361 ↗
39. The protective nature of passivation films on zinc: surface charge10.1016/j.corsci.2004.01.002 ↗
40. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel10.1016/j.corsci.2011.03.016 ↗
41. What really controls the atmospheric corrosion of zinc? Effect of marine aerosols on atmospheric corrosion of zinc10.1179/174328009X411145 ↗
42. Chemistry of corrosion products on Zn–Al–Mg alloy coated steel10.1016/j.corsci.2010.05.044 ↗