Corrosion of high purity Mg, AZ91, ZE41 and Mg2Zn0.2Mn in Hank’s solution at room temperature
Source abstract
Abstract
This work compared the corrosion of typical Mg alloys (AZ91, ZE41 and Mg2Zn0.2Mn) and high purity (HP) Mg in Hank's solution at room temperature and in 3% NaCl saturated with Mg(OH)(2). Corrosion was characterised by the evolved hydrogen and the surfaces after immersion. Corrosion in Hank's solution was weakly influenced by microstructure in contrast to corrosion in the 3% NaCl solution. This is attributed to the formation of a more protective surface film in Hank's solution, causing extra resistance between the alpha-Mg matrix and the second phase. The alloys with substantial Zn contents had a shorter incubation period in Hank's solution. (C) 2010 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
2. Understanding magnesium corrosion - A framework for improved alloy performance10.1002/adem.200310405 ↗
3. Electrochemical corrosion of pure magnesium in 1N NaCl10.1016/S0010-938X(96)00172-2 ↗
4. The anodic dissolution of magnesium in chloride and sulphate solutions10.1016/S0010-938X(97)00090-5 ↗
5. Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride10.1016/S0010-938X(98)00078-X ↗
6. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
7. An exploratory study of the corrosion of Mg alloys during interrupted salt spray testing10.1016/j.corsci.2009.03.014 ↗
8. Calculated phase diagrams and the corrosion of die-cast Mg–Al alloys10.1016/j.corsci.2008.12.015 ↗
9. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
10. The influence of Yttrium (Y) on the corrosion of Mg–Y binary alloys10.1016/j.corsci.2010.07.019 ↗
11. Recent insights into the mechanism of magnesium corrosion and research suggestions10.1002/adem.200600221 ↗
12. An hydrogen evolution method for the estimation of the corrosion rate of magnesium alloys
13. The history of biodegradable magnesium implants: a review10.1016/j.actbio.2010.02.028 ↗
14. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
15. In vivo corrosion and corrosion protection of magnesium alloy LAE44210.1016/j.actbio.2009.10.012 ↗
16. Witte · Biomaterials · 2006 · 27 · 101310.1016/j.biomaterials.2005.07.037 ↗
17. On the in vitro and in vivo degradation performance and biological response of new biodegradable Mg-Y-Zn alloys10.1016/j.actbio.2009.10.008 ↗
18. On the biodegradation performance of an Mg-Y-RE alloy with various surface conditions in simulated body fluid10.1016/j.actbio.2008.07.034 ↗
19. Magnesium alloys as implant materials - Principles of property design for Mg-RE alloys10.1016/j.actbio.2009.09.010 ↗
20. A survey of bio-corrosion rates of magnesium alloys10.1016/j.corsci.2009.09.033 ↗
21. Critical discussion of the results from different corrosion studies of Mg and Mg alloys for biomaterial applications10.1016/j.actbio.2009.12.048 ↗
22. Control of biodegradation of biocompatible magnesium alloys10.1016/j.corsci.2007.01.001 ↗
23. Effect of heat treatment on corrosion behaviour of magnesium alloy AZ91D in simulated body fluid10.1016/j.corsci.2009.11.030 ↗
24. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
25. Effect of Y on the bio-corrosion behaviour of extruded Mg-Zn-Mn alloy in Hank’s solution10.1016/j.msec.2009.09.014 ↗
26. Electrochemical behaviour of magnesium alloys as biodegradable materials in Hank’s solution10.1016/j.electacta.2010.05.062 ↗
27. Research on an Mg–Zn alloy as a degradable biomaterial10.1016/j.actbio.2009.06.028 ↗
28. In vitro degradation, hemolysis and MC3T3–E1 cell adhesion of biodegradable Mg–Zn alloy10.1016/j.msec.2009.03.001 ↗
29. Preparation of SBF with different HCO3- content and its influence on the composition of biomimetic apatites10.1016/j.actbio.2005.11.001 ↗
30. 1999
31. Microstructure, mechanical and corrosion properties and biocompatibility of Mg-Zn-Mn alloys for biomedical application10.1016/j.msec.2008.08.024 ↗
32. Influence of pH and chloride ion concentration on the corrosion of Mg alloy ZE4110.1016/j.corsci.2008.08.023 ↗
33. Influence of microstructure on corrosion of as-cast ZE4110.1002/adem.200700246 ↗
34. A novel approach for the formation of Mg(OH)2/MgO nanowhiskers on magnesium: Rapid anodization in chloride containing solutions10.1016/j.elecom.2007.12.007 ↗
35. Magnesium salts and oxide: an XPS overview10.1016/S0169-4332(97)00180-3 ↗
36. Formation and breakdown of surface films on magnesium and its alloys in aqueous solutions10.1016/j.corsci.2006.05.033 ↗
37. Characterisation of TiN coatings and of the TiN/Si interface by X-ray photoelectron spectroscopy and Auger electron spectroscopy10.1016/0169-4332(93)90241-3 ↗