journal article·2008-05

Corrosion of ultra-fine grained copper fabricated by equal-channel angular pressing

Hiroyuki Miyamoto, Kohei Harada, Takuro Mimaki, Alexei Vinogradov, Satoshi Hashimoto

Corrosion Science· Volume 50· Issue 5
Publisher page

Abstract

Corrosion of ultra-fine grain (UFG) copper fabricated by equal-channel angular pressing (ECAP) has been investigated in comparison with that in recrystallized coarse grain (CG) copper. Corrosion current was estimated by a Tafel extrapolation method to examine the kinetics of corrosion in a modified Livingstone etchant, which is sensitive to dislocations and grain boundaries. UFG copper exhibited a lower corrosion current in comparison with that in its recrystallized coarse grain (CG) counterpart despite the fact that the dislocation density and total fraction of grain boundaries are much greater in UFG copper than in CG copper. Corrosion damage on the surface of UFG copper is macroscopically rather uniform whereas obvious attack at grain boundaries and selective corrosion of some grain interiors were observed in CG copper.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Bulk nanostructured materials from severe plastic deformation10.1016/S0079-6425(99)00007-9 ↗
2. Nanostructured metals retaining ductility10.1038/nmat1141 ↗
3. On the corrosion behaviour of ultra-fine grain copper10.1016/S1359-6462(99)00170-0 ↗
4. Corrosion resistance of ultra fine-grained Ti10.1016/j.scriptamat.2004.04.011 ↗
5. Pitting corrosion resistance of ultrafine-grained aluminum processed by severe plastic deformation10.2320/jinstmet.69.892 ↗
6. Pitting corrosion resistance of anodized aluminum alloy processed by severe plastic deformation10.2320/jinstmet.70.534 ↗
7. Stress corrosion cracking susceptibility of ultra-fine grain copper produced by equal-channel angular pressing10.1016/S0921-5093(01)01332-6 ↗
8. Corrosion, stress corrosion cracking and fatigue of ultra-fine grain copper fabricated by severe plastic deformation10.1016/S0151-9107(02)80008-3 ↗
9. Mechanical, thermal and stress-corrosion properties of ultra-fine grain copper
10. The corrosion behavior of nanocrystalline nickel10.1016/0956-716X(91)90171-V ↗
11. The corrosion behavior of nanocrystalline electrodeposits
12. Effect of pH on the corrosion behavior of nanocrystalline cobalt10.4028/www.scientific.net/JMNM.15-16.643 ↗
13. Intergranular corrosion of copper and α-Cu–Al alloy bicrystals10.1080/01418619108213908 ↗
14. Behavior of intergranular corrosion of <011> tilt grain boundaries of pure copper bicrystals10.1016/S0010-938X(01)00158-5 ↗
15. Etch pits at dislocations in copper10.1063/1.1735748 ↗
16. Corrosion of grain boundaries: Initiation process and testing
17. A kinetical model for the electrochemical grooving of grain boundaries10.1016/0013-4686(80)87127-1 ↗
18. On the contribution of triple junctions to the structure and properties of nanocrystalline materials10.1016/0956-716X(90)90354-J ↗
19. On the persistence of four-fold triple line nodes in nanostructured materials10.1016/0956-716X(93)90572-A ↗
20. Enhancing the operating life and performance of lead–acid batteries via grain-boundary engineering10.1557/S0883769400053422 ↗
21. The effect of boundary structure (energy) on interfacial corrosion10.1016/0001-6160(82)90157-2 ↗