Abstract
Abstract This study investigated the grain size effect on the resistance to hydrogen embrittlement (HE) of API 2W Grade 60 steels using in situ slow-strain-rate testing. Hydrogen was electrochemically charged into specimens and the hydrogen content evolved from diffusible hydrogen-trap sites was measured by thermal desorption spectrometry (TDS). The fine-grained (14 μm) steel showed superior HE resistance despite exhibiting higher total hydrogen content than the coarse-grained (35 μm) steel. Decreasing grain size resulted in a larger grain boundary area, thereby better reducing the normalized amount of diffusible hydrogen trapped per unit length of grain boundary.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Evaluation of hydrogen trapping in high strength steels by thermal desorption spectroscopy10.1016/j.msea.2012.04.078 ↗
2. Hydrogen control in steel weld metal by means of fluoride additions in welding flux
3. Effects of nitrogen content and weld cooling time on the simulated heat-affected zone toughness in a Ti-containing steel10.1007/s10853-006-0498-5 ↗
4. Electrochemically induced annealing of stainless-steel surfaces10.1038/35038040 ↗
5. Detecting electrochemical transients generated by erosion–corrosion10.1016/S0013-4686(01)00646-6 ↗
6. Reduction of delayed fracture susceptibility of tempered martensitic steel through increased Si content and surface softening10.2355/isijinternational.53.714 ↗
7. Influence of hydrogen on the mechanical properties of some medium-strength Ni-Cr-Mo steels10.1016/j.msea.2014.08.056 ↗
8. Hydrogen embrittlement and rock bolt stress corrosion cracking10.1016/j.engfailanal.2008.01.004 ↗
9. SCC of commercial steels exposed to high hydrogen fugacity10.1016/j.engfailanal.2007.10.004 ↗
10. Effect of grain size on mechanical electrochemical and hydrogen embrittlement behaviour of a micro-alloy steel10.1016/j.msea.2012.09.011 ↗
11. Effect of grain size on the hydrogen embrittlement sensitivity of a precipitation strengthened Fe-Ni based alloy10.1016/j.msea.2013.11.062 ↗
12. Effect of grain size on the hydrogen-assisted cracking in duplex stainless steels10.1016/S0921-5093(99)00174-4 ↗
13. Effects of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels10.1016/j.ijhydene.2011.10.099 ↗
14. The effect of grain size and aging on hydrogen embrittlement of a maraging steel10.1016/j.corsci.2008.06.044 ↗
15. Dependence of hydrogen-induced lattice defects and hydrogen embrittlement of cold-drawn pearlitic steels on hydrogen trap state temperature, strain rate and hydrogen content10.1016/j.actamat.2014.07.008 ↗
16. Effects of loading factors on environmental fatigue behavior of low-alloy pressure vessel steels in simulated BWR water10.1016/j.nucengdes.2006.09.043 ↗
17. Hydrogen embrittlement of weld metal of austenitic stainless steels10.1016/S0010-938X(02)00011-2 ↗
18. 2D modelling of the effect of grain size on hydrogen diffusion in X70 steel10.1016/j.commatsci.2012.01.003 ↗
19. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
20. Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel10.1016/j.actamat.2012.04.010 ↗
21. Effects of cryogenic and tempered treatment on the hydrogen embrittlement susceptibility of TRIP-780 steels10.1016/j.ijhydene.2013.05.113 ↗
22. Hydrogen embrittlement of ultra high strength 300 grade maraging steel10.1016/j.corsci.2015.06.022 ↗
23. Hydrogen-assisted quasi-cleavage fracture in a single crystalline type 316 austenitic stainless steel10.1016/j.corsci.2013.06.018 ↗
24. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
25. The advantage of grain refinement in the hydrogen embrittlement of Fe-18Mn-0. 6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
26. Effect of cathodic hydrogen-charging current density on mechanical properties of prestrained high strength steels10.1016/j.msea.2015.06.003 ↗
27. Effect of hydrogen on the properties and fracture characteristics of TRIP 800 steels10.1016/j.corsci.2011.04.015 ↗
28. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
29. Effects of grain size on hydrogen environment embrittlement of high strength low alloy steel in 45MPa gaseous hydrogen10.2320/matertrans.M2009241 ↗
30. Strain mapping near a triple junction in strained Ni-based alloy using EBSD and biaxial nanogauges10.1016/j.actamat.2011.01.051 ↗
31. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe-Mn-Al-C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
32. Effects of tungsten on the hydrogen embrittlement behaviour of microalloyed steels10.1016/j.corsci.2014.01.042 ↗
33. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
34. Effect of nano-carbide formation on hydrogen-delayed fracture for quenching and tempering steels during high-frequency induction heat treatment10.1016/j.msea.2012.02.008 ↗
35. Microstructural effects on hydrogen delayed fracture of 600MPa and 800MPa grade deposited weld metal10.3365/KJMM.2012.50.1.052 ↗
36. Combined thermal desorption spectroscopy differential scanning calorimetry, scanning electron microscopy and X-ray diffraction study of hydrogen trapping in cold deformed TRIP steel10.1016/j.actamat.2012.01.026 ↗
37. Numerical modeling of thermal desorption mass spectroscopy (TDS) for the study of hydrogen diffusion and trapping interactions in metals10.1016/j.ijhydene.2015.01.001 ↗
38. Thermal desorption spectroscopy study of the interaction between hydrogen and different microstructural constituents in lab cast Fe–C alloys10.1016/j.corsci.2012.08.017 ↗
39. The effect of carbon on hydrogen embrittlement in stable Cr-Ni-Mn-N austenitic stainless steels10.1016/j.corsci.2017.05.004 ↗
40. The influence of calcareous deposits on hydrogen uptake and embrittlement of API 5CT P110 steel10.1016/j.corsci.2017.02.007 ↗
41. Theory of do for atomic diffusion in metals10.1063/1.1699967 ↗