On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels
Source abstract
Abstract
Abstract Cathodic hydrogen charging was applied to low-carbon pipeline-steel samples produced using different thermomechanical paths. The samples developed similar microstructures but different crystallographic textures and grain–boundary distributions. This made it possible to investigate the resistance to hydrogen-induced cracking (HIC) of steels with strong {1 1 1}ND and {1 1 2}ND texture fibres, steels with a dominating {0 0 1}ND texture fibre, and steels with close-to-random textures; { h k l }ND representing grain orientations with { h k l } planes parallel to the steel rolling plane. The results show that strong {1 1 1}ND fibre textures produced by warm-rolling schedules significantly increase HIC-resistance of pipeline steels, whereas {0 0 1}ND and close-to-random textures make steels HIC-prone.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Hydrogen-induced cracking and sulphide stress cracking
2. Theories of hydrogen induced cracking of steels
3. Initiation of stress corrosion cracking and hydrogen-induced cracking in oil and gas line-pipe steels
4. Introduction to environmentally induced cracking
5. N. Loukachenko, P. Bourger, K.E. Orie, C. Chauvy, L. Couddreuse, P. Toussaint, Recent experience on sour service resistant steel behavior, in: Proc. of NACE International Annual Corrosion Conf. and Exp. (CORROSION’09), Atlanta GA, Paper 09352, March 22–26, 2009.
6. R.J. Pargeter, Susceptibility to SOHIC for linepipe and pressure vessel steels - Review of current knowledge, in: NACE International Annual Corrosion Conf. and Exp. (CORROSION’07), Nashville TN, Paper 07115, March 11–15, 2007.
7. Review of Published Literature on Wet H2S cracking of Steels Through 1989, 2003 Edition, NACE International Publication 8X294, Houston TX, 2003.
8. ANSI/API Specification 5L/ISO 3183, Specification for Line Pipe: Annex H, API Publishing Services, Washington DC, 2007.
9. Metallurgical considerations for commercial steels used for hydrogen service
10. Challenges in procurement of HIC resistant steels pipes10.1007/s11668-011-9475-7 ↗
11. Failure analysis of a crude oil pipeline10.1016/j.engfailanal.2006.12.001 ↗
12. Failures by SOHIC in sour hydrocarbon srvices10.1007/s11668-011-9467-7 ↗
13. EBSD study of hydrogen induced cracking in API-5L–X46 pipeline steel10.1016/j.scriptamat.2004.09.015 ↗
14. Role of crystallographic texture in hydrogen-induced cracking of low carbon steels for sour service piping10.1007/s11661-007-9130-9 ↗
15. F. Caleyo, V. Venegas, J. M. Hallen, J. E. Araujo, T. Baudin, On the influence of crystallographic texture on HIC, in: Proc. ASME 6th Int. Biennial Pipeline Conf. IPC2006, Calgary AB, Canada, Paper IPC2006-10530, September 25–29, 2006.
16. Transformation textures in steels10.1179/095066090790324046 ↗
17. Randle · 2003
18. Determination of the orientation distribution function from pole figures in arbitrarily defined cells10.1002/pssb.2221340205 ↗
19. D.J. Dingley, The development of automated diffraction in scanning and transmission electron microscopy, in: A.J. Schwartz, M. Kumar, B.L. Adams (Eds.), Electron Backscatter Diffraction in Materials Science, Kluger Academic; New York, 2003, pp. 1–16.10.1007/978-1-4757-3205-4_1 ↗
20. Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging10.1016/j.corsci.2011.05.060 ↗
21. NACE Standard Test Method TM0284-2003, Standard Test Method - Evaluation of Pipeline and Pressure Vessel Steels for Resistance to Hydrogen-Induced Cracking, NACE, Houston, 2003, pp. 1–16.
22. Relationship between hydrogen-induced cracking and type I sulfide stress cracking of high-strength linepipe steel10.1016/j.scriptamat.2009.10.028 ↗
23. Orientation correlations in primary recrystallized Fe-50%Ni10.1016/S0928-4931(00)00189-2 ↗
24. Gross · 2006
25. Role of microtexture in the interaction and coalescence of hydrogen-induced cracks10.1016/j.corsci.2009.02.010 ↗
26. Crack interaction, coalescence and mixed mode fracture mechanics10.1111/j.1460-2695.1996.tb00979.x ↗
27. Grain–boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
28. Measuring relative grain boundary energies and mobility in an aluminum foil from triple junction geometry10.1016/S1359-6462(01)00960-5 ↗
29. G. Domizzi, G. Anteri, J. Ovejero-García, Influence of sulphur content and inclusion distribution on the hydrogen induced blister cracking in pressure vessel and pipeline steels, Corros. Sci. 43 (2001) 325–339.10.1016/S0010-938X(00)00084-6 ↗
30. A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies10.1016/j.corsci.2008.10.006 ↗
31. A Markov Chain-Monte Carlo model for intergranular stress corrosion crack propagation in polycrystalline materials10.1016/j.msea.2009.01.072 ↗