Role of chlorides in hot corrosion of a cast Fe–Cr–Ni alloy. Part I: Experimental studies
Source abstract
Abstract
Abstract High alloy stainless steels are often used in corrosive, high temperature applications because they form a protective, adherent Cr 2 O 3 scale. When the environment in such applications includes condensed molten salts, especially alkali sulfates and alkali chlorides, these alloys are likely to undergo hot corrosion, even at moderate temperatures compared to their typical maximum application temperature. The chemical (or electrochemical) reactions and transport modes for hot corrosion in a system involving a multi-component alloy and a multi-component salt are complex, but some insight can be gained with the help of a multi-component thermochemical model to identify major reactions. The present work consists of two parts: (a) experimental measurements of hot corrosion rates and characterization of corrosion products on a commercial, cast super-duplex stainless steel (HH), which result from exposure to thin deposits of a mixture of alkali sulfates and alkali chlorides, and (b) an evaluation of possible corrosion reactions by a multi-component thermochemical model. In laboratory hot corrosion tests alloy coupons experienced rapid oxidation rates, penetration of the oxide scale, scale blistering, and scale spallation (on cooling). Compared to simple air oxidation, alkali sulfate deposits increased the corrosion rate by a factor of about 200, but mixtures of alkali sulfate and alkali chloride increased the rate by about 20,000 times. A principal goal of the study was to identify the role of alkali chlorides in accelerating hot corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Hot corrosion of stainless steel grate bars in taconite indurators
2. Evans · Oxid. Met · 1976 · 10 · 14910.1007/BF00612157 ↗
3. Rundell · Oxid. Met · 1991 · 36 · 25310.1007/BF00662965 ↗
4. Young · High Temp. Tech · 1982 · 10110.1080/02619180.1982.11753189 ↗
5. Baxter · Oxid. Met · 1989 · 31 · 30510.1007/BF00846691 ↗
6. Gordon · Oxid. Met · 1979 · 13 · 19710.1007/BF00611979 ↗
7. Gesmundo · High Temp. Matls. Process · 1989 · 8 · 14910.1515/HTMP.1989.8.3.149 ↗
8. Jacob · Oxid. Met · 1979 · 13 · 2510.1007/BF00715869 ↗
9. Stroosnijder · High Temperature Tech · 1986 · 4 · 8310.1080/02619180.1986.11753321 ↗
10. Goebel · Met. Trans · 1973 · 4 · 26110.1007/BF02649626 ↗
11. Mechanisms of low temperature hot corrosion
12. New perspectives on hot corrosion mechanisms
13. Low temperature hot corrosion
14. The hot corrosion of metals by molten salts
15. Rapp · J. Met · 1994 · 46 · 47
16. Lee · J. Electrochem. Soc · 1990 · 137 · 85910.1149/1.2086569 ↗
17. Kim · Corros. NACE · 1990 · 46 · 74610.5006/1.3585177 ↗
18. Reese · Werkstoffe und Korrosion · 1992 · 43 · 54710.1002/maco.19920431202 ↗
19. Reese · Werkstoffe und Korrosion · 1993 · 44 · 4110.1002/maco.19930440204 ↗
20. Shinata · Mater. Trans. (JIM) · 1991 · 32 · 96910.2320/matertrans1989.32.969 ↗
21. Stott · Werkstoffe und Korrosion · 1988 · 39 · 40110.1002/maco.19890390902 ↗
22. Fundamental mechanisms of the attack of chlorine hcl and chlorides on steels and high temperature alloys in the temperature range 400 to 900 °C
23. Phase diagrams for ceramists
24. Zhang · Oxid. Met · 1994 · 40 · 52910.1007/BF00666390 ↗
25. Zhang · J. Electrochem. Soc · 1994 · 141 · 125510.1149/1.2054906 ↗
26. Halogen corrosion of metals
27. Corrosion by chlorine in waste-fueled boilers