The oxide scales of 316 stainless steel (316 SS) have been examined after exposure to supercritical water (SCW) with 2.0% H(2)O(2) for up to 250 h. The exposed samples were analyzed using weight measurement, scanning electron microscopy (SEM), and X-ray diffraction analysis (XRD). It was found that mass gain of all samples increased with increasing temperature and exposure time. Higher temperature SCW resulted in rougher surfaces and thicker oxide scales. Duplex layer oxide structures with Ni-enrichment at the oxide/metal interface developed on all samples exposed to SCW, which were identified as Fe(2)O(3)/Fe(3)O(4)+spinel/Cr(2)O(3)/Ni-enrichment/316 SS from the outer to inner layer. The possible oxidation mechanisms are also discussed. (C) 2009 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. M. Modell, Processing methods for the oxidation of organics in supercritical water, US Patent 4,388,199 (Jul. 6), 1982.
2. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
3. Stainless steel flow reactor for supercritical water oxidation: corrosion tests10.1016/S0896-8446(02)00264-4 ↗
4. Corrosion performance of metals for supercritical water, oxidation-utilized organic waste processing reactors10.5006/1.3278276 ↗
5. Analyses of oxide films grown on Alloy 625 in oxidizing supercritical water10.1016/j.supflu.2008.07.010 ↗
6. Corrosion of stainless steel in supercritical water
7. Corrosion of alumina ceramics in acidic aqueous solutions at high temperatures and pressures10.1023/A:1026714218522 ↗
8. Ceramic reactor for use with corrosive supercritical fluids10.1002/aic.690420632 ↗
9. Corrosion of ferritic–martensitic steel HT9 in supercritical water10.1016/j.jnucmat.2006.07.010 ↗
10. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650°C10.1016/j.corsci.2004.01.010 ↗
11. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
12. I.G. Wright, B.A. Pint, An assessment of the high-temperature oxidation behavior of Fe–Cr steels in water vapor and steam, Corrosion 2002 (Paper No. 02377).
13. Inverse growth transport in thermal chromia scales on Fe–15Cr steels in oxygen and in water vapour and its effect on scale adhesion10.1016/j.scriptamat.2007.06.050 ↗
14. Corrosion and stress corrosion cracking of ferritic/martensitic steel in super critical pressurized water10.1016/j.jnucmat.2007.03.212 ↗
15. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
16. Influence of oxide films on primary water stress corrosion cracking initiation of alloy 60010.1016/j.jnucmat.2005.10.002 ↗
17. Effect of pressure on the rate of corrosion of metals in high subcritical and supercritical aqueous systems10.1016/j.supflu.2003.09.004 ↗
18. Corrosion and corrosion fatigue behaviors of 9cr steel in a supercritical water condition10.1016/j.msea.2006.05.035 ↗
19. Stratified oxide scale growth on two Cr–Ni steels oxidized in high-pressure steam at 800°C10.1007/BF00603656 ↗
20. Enhanced oxidation of the 9% Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
21. The effect of water vapor on selective oxidation of Fe–Cr alloys10.1007/s11085-007-9090-x ↗