journal article·2014-01

Atmospheric corrosion monitoring of a weathering steel under an electrolyte film in cyclic wet–dry condition

Ch. Thee, Long Hao, Junhua Dong, Xin Mu, Xin Wei, Xiaofang Li, Wei Ke

Corrosion Science· Volume 78
Publisher page

Abstract

Abstract Electrochemical Impedance Spectroscopy (EIS) and film thickness measurements have been employed to study the corrosion monitoring of steel under an electrolyte film in wet–dry cycles simulating a coastal atmosphere. The results indicate that within each cycle, the corrosion rate increases during drying process due to an increase in Cl − concentration and an enhancement of oxygen diffusion by thinning out of the electrolyte. As corrosion process proceeds, the corrosion rate increases greatly and reaches a maximum. During subsequent corrosion stage, the corrosion rate decreases greatly and keeps at a low value due to the formation of a stable rust layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Introduction to atmospheric corrosion research in China10.1016/j.stam.2007.08.010 ↗
2. Leygraf · 2000
3. On the atmospheric corrosion of metal which are covered with thin electrolyte layers–II10.1016/0010-938X(90)90033-2 ↗
4. EIS monitoring study of atmospheric corrosion under variable relative humidity10.1016/j.corsci.2010.07.018 ↗
5. Electrochemical studies on corrosion under a water film10.1016/0921-5093(95)80071-2 ↗
6. Electrochemical impedance study on galvanized steel corrosion under cyclic wet–dry conditions – influence of time of wetness10.1016/S0010-938X(03)00130-6 ↗
7. Rusting evolution of MnCuP weathering steel submitted to simulated industrial atmospheric corrosion10.1007/s11661-011-0977-4 ↗
8. Rusting evolvement of mild steel under wet/dry cyclic condition with pH 4 NaHSO3 solution
9. Development of the electrochemical theory of metallic corrosion10.5006/0010-9312-20.1.7t ↗
10. On the atmospheric corrosion of metal which are covered with thin electrolyte layers–III. The measurement of polarisation curves on metal surfaces which are covered by thin electrolyte layers10.1016/0010-938X(90)90034-3 ↗
11. Corrosion monitoring of nickel-containing steels in marine atmospheric environment10.1016/j.corsci.2004.10.009 ↗
12. A new experimental method for in situ corrosion monitoring under alternate wet–dry conditions10.3390/s91210400 ↗
13. Electrochemical behavior of rust formed on carbon steel in a wet/dry environment containing chloride ions10.5006/1.3280597 ↗
14. Influence of electrolyte layer thickness and pH on the initial stage of the atmospheric corrosion of iron10.1149/1.1837578 ↗
15. Evolvement of electrochemical impedance spectra of a bi-electrode cell for carbon steel in the initial stage of wet/dry process
16. ASTM D 5032-97, Standard practice for maintaining constant relative humidity by means of aqueous glycerin solutions, ASTM International, West Conshohocken, PA, 2003.
17. Advances in understanding atmospheric corrosion of iron. II. mechanistic modelling of wet–dry cycles10.1016/j.corsci.2003.09.028 ↗
18. Determination of corrosion rates by electrochemical DC and AC methods10.1016/0010-938X(81)90015-9 ↗
19. Minimization of high-frequency phase-shifts in impedance measurements10.1149/1.2095825 ↗
20. Evolution of atmospheric corrosion of MnCuP weathering steel in a simulated coastal-industrial atmosphere10.1016/j.corsci.2012.03.010 ↗
21. Cao · 2004
22. Anodic processes on iron covered by thin, dilute electrolyte layers (I) – anodic polarisation10.1016/0010-938X(94)90182-1 ↗
23. Anodic processes on iron covered by thin, dilute electrolyte layers (II) – AC impedance measurements10.1016/0010-938X(94)90183-X ↗
24. Mccafferty · 2010
25. Corrosion evolution of MnCuP weathering steel submitted to wet/dry cyclic tests in a simulated coastal atmosphere10.1016/j.corsci.2012.01.017 ↗
26. I. Kage, K. Matsui, F. Kawabata, Minimum maintenance steel plates and their application technologies for bridge-life cycle cost reduction technologies with environmental safeguards for preserving social infrastructure assets, in: JFE Technical Report No. 5, March 2005, also JFE GIHO No. 5, August 2004, pp. 31–37.
27. Rusting evolution of Mn–Cu alloying steel in a simulated coastal environment
28. Eight-year atmospheric corrosion exposure of steels in China10.5006/1.3283967 ↗
29. Corrosion behavior of weathering steel in marine atmosphere10.1016/S0254-0584(02)00110-4 ↗
30. Effect of Al alloying on corrosion performance of steel10.1179/174327807X214617 ↗
31. Orazem · 2008
32. Control of humidity in small controlled environment chambers using Glycerol-water solutions10.21273/HORTTECH.2.1.52 ↗
33. The corrosion mechanisms of carbon steel and weathering steel in SO2 polluted atmospheres10.1016/S0254-0584(97)80019-3 ↗
34. Atmospheric corrosion resistance of MnCuP weathering steel in simulated environments10.1016/j.corsci.2011.08.028 ↗
35. The atmospheric corrosion kinetics of low carbon steel in a tropical marine environment10.1016/j.corsci.2010.01.022 ↗
36. Electrochemical techniques in corrosion science and engineering
37. Study on the rusting evolution and the performance of resisting to atmospheric corrosion for Mn–Cu steel10.3724/SP.J.1037.2010.01365 ↗
38. A study of the evolution of rust on Mo–Cu-bearing fire-resistant steel submitted to simulated atmospheric corrosion10.1016/j.corsci.2011.09.023 ↗
39. Long-term atmospheric corrosion of mild steel10.1016/j.corsci.2010.10.007 ↗
40. Mechanical properties and corrosion resistance of low-alloy steels in atmospheric conditions containing chloride10.1016/j.msea.2005.02.064 ↗
41. Corrosion behavior of rusted mild steel under means of wet/dry alternate conditions