The effects of sacrificial coatings on hydrogen embrittlement and re-embrittlement of ultra high strength steels

D. Figueroa, M.J. Robinson

Corrosion Science· Volume 50· Issue 4
Publisher page

Abstract

Abstract This paper describes an investigation of electrodeposited Zn–14% Ni and aluminium-based SermeTel 1140/962 coatings as possible replacements for cadmium. Slow strain rate tests were performed to measure the extent of direct hydrogen embrittlement of a high strength steel substrate as a result of the coating process and of hydrogen re-embrittlement caused by coating corrosion. The level of re-embrittlement was shown to depend on both the electrochemical potential of the coating and its barrier properties. Zn–14% Ni coatings caused the most re-embrittlement as they had the most active potential and contained through-thickness defects which left the steel exposed to hydrogen uptake. The microstructure of the high strength steel was also shown to be an important factor affecting the extent of embrittlement. AerMet 100 steel was more resistant than 300M steel and this was attributed to the presence of reverted austenite surrounding the martensite laths in AerMet 100, which trapped absorbed hydrogen and prevented a critical hydrogen concentration being reached in the more susceptible martensite phase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Defence Standard 03-4/2, The pre-treatment and protection of steel parts of specified maximum tensile strength exceeding 1450Nmm−2, 1977.
2. Statistical treatment of slow strain rate data for assessment of hydrogen embrittlement in high strength 4340 steel10.1016/0010-938X(92)90165-Y ↗
3. Hydrogen re-embrittlement of high strength steel by corrosion of cadmium and aluminium based sacrificial coatings10.1179/174327805X29822 ↗
4. Correlation of microstructure with mechanical properties of 300M steel10.1007/BF02642857 ↗
5. Microstructural analysis of a multistage heat-treated ultra-high strength low alloy steel10.1016/0025-5416(84)90175-7 ↗
6. Hydrogen trapping in high strength steels10.1016/S1359-6454(98)00247-X ↗
7. British Standard BS EN ISO 10308:1997, Metallic coatings-review of porosity tests, 1997.
8. Kutzelnigg · 1963
9. The effect of post-exposure heat treatment on the hydrogen embrittlement of high strength steel10.5006/1.3582987 ↗
10. T. Yokobori, Strength fracture and fatigue of materials, P. Noordhoff (Ed.), Groningen, 1965, pp. 22–28.
11. Hydrogen embrittlement of high strength steel electroplated with zinc–cobalt alloys10.1016/S0010-938X(03)00180-X ↗
12. Chatfield · 1983
13. Corrosion rate measurements of electrodeposited zinc–nickel alloy coatings10.1016/0010-938X(94)90137-6 ↗
14. 1976 · vol. 2 · 21
15. Analysis of hydrogen evolution and entry into metals for the discharge–recombination process10.1149/1.2097429 ↗
16. Factors controlling crack velocity in 7000 series aluminium alloys during fatigue in an aggressive environment10.1016/0010-938X(83)90117-8 ↗
17. The diffusivity of hydrogen in aluminium10.1016/0001-6160(86)90219-1 ↗
18. W.J. Dini, Electrodeposition, the material science of coatings and substrates, WestWood, US, 1993, pp. 249–278.
19. Porosity determination of nickel coatings on copper by anodic voltammetry10.1023/A:1020142515298 ↗
20. The effects of zinc alloy electroplating on the hydrogen embrittlement of high strength steels10.1080/00202967.1995.11871060 ↗
21. Permeation measurements to study hydrogen uptake by steel electroplated with zinc–cobalt alloys10.1016/j.corsci.2005.05.009 ↗
22. Crank · 1975
23. An example of the effect of hydrogen trapping on hydrogen embrittlement10.1007/BF02648348 ↗
24. M.J. Robinson, P.J. Kilgallon, A review of the effects of microstructure on the hydrogen embrittlement of high strength offshore steels, Health and Safety Executive – Offshore Technology Report OTH 555, HSE Books, 1998.
25. E.U. Lee, H. Sanders et al., Stress corrosion cracking of high strength steels, Naval Air Warfare Centre, Aircraft Division, Patuxent River, Maryland, Technical Report, US, 1999.
26. The role of hydrogen and other interstitials in the mechanical behaviour of metals
27. D.J. Figueroa, Hydrogen embrittlement susceptibility of ultra high strength steels, PhD thesis, Cranfield University, 2005.
28. Hydrogen diffusivity of AerMet 100 at room temperature under galvanostatic charging conditions10.1016/S0925-8388(03)00332-3 ↗
29. Trap-governed hydrogen diffusivity and uptake capacity in ultra high-strength AerMet®100 steel10.1007/s11661-002-0032-6 ↗
30. Internal hydrogen embrittlement of ultrahigh-strength AerMet®100 steel10.1007/s11661-003-0334-3 ↗
31. M.J. Robinson, P.J. Kilgallon, M. Newman, Hydrogen embrittlement of cathodically protected duplex stainless steels in seawater containing sulphides, in: Proceedings 15th International Conference on Offshore Mechanics & Arctic Engineering, Florence, Italy, June 16–20, 1996.
32. Determination of hydrogen diffusivity in austenitic stainless steels by subscale microhardness profiling10.1016/S0925-8388(96)02846-0 ↗
33. Transmission electron microscopy examination of hardening and toughening phenomena in AerMet 100