Corrosion behavior of Alloy 690 in aerated supercritical water
Source abstract
Abstract
Abstract The oxidation behavior of Alloy 690 exposed to aerated supercritical water at different temperatures was investigated using gravimetry, scanning electron microscopy/energy dispersive X-ray spectroscopy, X-ray diffraction, X-ray photoelectron spectroscopy, Raman spectroscopy and electron probe micro-analyzer. The oxide films showed a duplex layer structure with Ni and Fe rich in the outer layer, and Cr rich in the inner layer. Some pits and nodules observed in the oxide films could be related to TiN inclusions in the alloy matrix. The oxidation mechanism and effects of TiN inclusions are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. A Technology Roadmap for Generation IV Nuclear Energy Systems, in: US DOE Nuclear Energy Research Advisory Committee and the Generation IV International Forum (GIF-002-00), 2002.
2. Generation IV roadmap R&D scope report for water cooled reactor systems, in: US DOE Nuclear Energy Research Advisory Committee and the Generation IV International Forum (GIF-003-00), 2002.
3. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
4. Progress in corrosion resistant materials for supercritical water reactors10.1016/j.corsci.2009.07.007 ↗
5. G.S. Was, S. Teysseyre, Challenges and recent progress in corrosion and stress corrosion cracking of alloys for supercritical water reactor core components, in: 12th International Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors, Minerals, Metals and Materials Society, Salt Lake City, UT, United states, 2005, pp. 1343–1357.
6. Time, temperature, and dissolved oxygen dependence of oxidation of austenitic and ferritic–martensitic alloys in supercritical water
7. Corrosion behavior of alloys 625 and 718 in supercritical water10.5006/1.3278410 ↗
8. Analyses of oxide films grown on Alloy 625 in oxidizing supercritical water10.1016/j.supflu.2008.07.010 ↗
9. Corrosion behavior of Hastelloy C-276 in supercritical water10.1016/j.corsci.2009.05.041 ↗
10. Corrosion behavior of Ni-base alloys for advanced high temperature water-cooled nuclear plants10.1016/j.corsci.2008.08.024 ↗
11. Behavior of grain boundary chemistry and precipitates upon thermal treatment of controlled purity alloy 69010.1007/BF02647868 ↗
12. Influence of laser surface melting on the susceptibility to intergranular corrosion of sensitized Alloy 60010.1016/S0010-938X(00)00149-9 ↗
13. Stress corrosion cracking of alloy 600 and alloy 690 in hydrogen/steam at 380°C10.1016/S0010-938X(97)86103-3 ↗
14. Microscopic investigation of sensitized Ni-base alloy 600 after laser surface melting10.1007/s11661-997-0288-y ↗
15. Pitting corrosion of the laser surface melted Alloy 60010.1016/j.jnucmat.2004.08.015 ↗
16. Crack initiation mechanisms for low cycle fatigue of type 316 stainless steel in high temperature10.1016/j.msea.2007.12.043 ↗
17. The role of TiN inclusions in stress corrosion crack initiation for Alloy 690TT in high-temperature and high-pressure water10.1016/j.corsci.2009.11.015 ↗
18. Selective carbide oxidation and internal nitridation of the Ni-base superalloys IN 738 LC and IN 939 in air10.1007/BF00656646 ↗
19. G.S. Was, S. Teysseyre, J. McKingley, Z. Jiao, Corrosion of austenitic alloys in supercritical water, in: NACE CORROSION 2005, Huston, TX, 2005, Paper No. 05397.
20. In situ Raman spectroscopic investigation of aqueous iron corrosion at elevated temperatures and pressures10.1149/1.1393565 ↗
21. Effects of hydrogen peroxide on corrosion of stainless steel, (V) Characterization of oxide film with multilateral surface analyses10.1080/18811248.2006.9711173 ↗
22. Effects of heat-treatment on the extent of chromium depletion and caustic corrosion resistance of Alloy 69010.1016/j.corsci.2006.05.043 ↗
23. XPS and STM study of the growth and structure of passive films in high temperature water on a nickel-base alloy10.1016/j.electacta.2004.04.032 ↗
24. Effects of temperature on the protective property, structure and composition of the oxide film on Alloy 62510.1016/j.corsci.2009.06.043 ↗
25. The effect of chromium, carbon, and yttrium on the oxidation of nickel-base alloys in high temperature water10.1149/1.2220732 ↗
26. XPS study of oxides formed on nickel-base alloys in high-temperature and high-pressure water10.1002/sia.1282 ↗
27. Characterization of oxide films formed on alloy 182 in simulated PWR primary water10.1016/j.jnucmat.2009.06.012 ↗
28. Effects of temperature on the oxide film properties of 304 stainless steel in high temperature lithium borate buffer solution10.1016/j.corsci.2009.08.006 ↗
29. W. Cook, J. Miles, C. Bradley, J. Li, W. Zheng, A experimental study of comercially availabe alloys for potential use in the CANDU-SCWR, in: Nuclear Plant Chemistry Conference, Quebec City, Canada, 2010.
30. Corrosion behavior of Alloy 625 in supercritical water environments10.1016/j.pnucene.2011.12.015 ↗
31. The mechanism of oxide film formation on Alloy 690 in oxygenated high temperature water10.1016/j.corsci.2011.07.038 ↗
32. Corrosion behavior of Ni-base alloys in supercritical water10.5516/NET.2009.41.1.107 ↗
33. A detailed TEM and SEM study of Ni-base alloys oxide scales formed in primary conditions of pressurized water reactor10.1016/j.jnucmat.2010.05.010 ↗
34. Potential-pH diagrams for iron in supercritical water10.5006/1.3290292 ↗
35. Chemical thermodynamics consideration on corrosion products in supercritical-water-cooled reactor coolant10.13182/NT06-A3749 ↗
36. Pourbaix diagrams for the iron–water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2011.10.034 ↗
37. Pourbaix diagrams for the nickel–water system extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.007 ↗
38. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
39. Electrochemical properties and growth mechanism of passive films on Alloy 690 in high-temperature alkaline environments10.1016/j.corsci.2010.06.016 ↗
40. Birks · 2006
41. X-ray photoelectron studies of the aqueous oxidation of Inconel-600 Alloy10.1149/1.2129132 ↗
42. An investigation of thin oxide-films thermally grown insitu on Fe–24Cr and Fe–24Cr–11Mo by auger-electron spectroscopy and X-ray photoelectron-spectroscopy10.1016/0010-938X(86)90022-3 ↗
43. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
44. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
45. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
46. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
47. Kofstad · 1988