Abstract The evolution of atmospheric corrosion of MnCuP weathering steel in a simulated coastal-industrial atmosphere was investigated by weight gain, SEM, XRD, and electrochemical measurements. The results indicate that the corrosion kinetics divides into two stages with a higher corrosion rate in the first stage and a lower rate in the second stage. The increased amount of α-FeOOH indicates an improved resistance of the rust. The rust enhances initially and then stabilizes the cathodic process, but the anodic process tends to be inhibited. The EIS results indicate that the protective ability of the rust layer can be evaluated by the charge transfer resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Experimental determination of duration of wetness on metal surfaces10.1179/174327807X214554 ↗
2. Electrochemical impedance of thin rust film of low-alloy steels10.1016/j.corsci.2003.08.002 ↗
3. Atmospheric corrosion of carbon steel in Colombia10.1016/j.corsci.2009.09.006 ↗
4. A mechanistic study of initial atmospheric corrosion kinetics using electrical resistance sensors10.1016/j.corsci.2005.04.011 ↗
5. Possible effects of climate change on atmospheric corrosion in Australia10.1179/147842209X12579401586483 ↗
6. Evaluation of hydrogen entry into high strength steel under atmospheric corrosion10.1016/j.corsci.2009.11.046 ↗
7. The long term growth of the protective rust layer formed on weathering steel by atmospheric corrosion during a quarter of a century10.1016/0010-938X(94)90158-9 ↗
8. A study of the atmospheric corrosion behavior of low alloy steels containing copper
9. Atmospheric corrosion of carbon steels and weathering steels in Taiwan
10. The influence of Ni alloying on corrosion behaviour of low alloy steels under wet/dry cyclic conditions10.1179/cmq.2007.46.2.195 ↗
11. Eight-year atmospheric corrosion exposure of steels in China10.5006/1.3283967 ↗
12. Corrosion behavior of weathering steel in marine atmosphere10.1016/S0254-0584(02)00110-4 ↗
13. Effect of Al alloying on corrosion performance of steel10.1179/174327807X214617 ↗
14. Influence of Cu and Mn on corrosion behavior of low alloy steel in a simulated coastal environment
15. Effect of Ni on the ion-selectivity of rust layer on low alloy steel10.1016/j.matlet.2007.01.014 ↗
16. Corrosion behavior of MnCu cost-effective weathering steel under cyclic load in a wet/dry cyclic corrosion environment
17. Introduction to atmospheric corrosion research in China10.1016/j.stam.2007.08.010 ↗
18. Characterization of the rust formed on weathering steel exposed to Qinghai salt lake atmosphere10.1016/j.corsci.2007.06.020 ↗
19. Effect of Co and Ni on the corrosion behavior of low alloy steels in wet/dry environments10.1016/S0010-938X(00)00018-4 ↗
20. Structure and protective performance of atmospheric corrosion product of Fe-Cr alloy film analyzed by Mössbauer spectroscopy and with synchrotron radiation X-rays10.1016/S0010-938X(02)00093-8 ↗
21. Electrochemical behavior of rust formed on carbon steel in a wet/dry environment containing chloride ions10.5006/1.3280597 ↗
22. Atmospheric corrosion resistance of MnCuP weathering steel in simulated environments10.1016/j.corsci.2011.08.028 ↗
23. Long-term atmospheric corrosion of mild steel10.1016/j.corsci.2010.10.007 ↗
24. Industrial atmospheric corrosion resistance of P-RE weathering steel10.1016/S1006-706X(11)60080-0 ↗
25. Mechanical properties and corrosion resistance of low-alloy steels in atmospheric conditions containing chloride10.1016/j.msea.2005.02.064 ↗
26. The corrosion mechanisms of carbon steel and weathering steel in SO2 polluted atmospheres10.1016/S0254-0584(97)80019-3 ↗
27. A study of the evolution of rust on Mo–Cu-bearing fire-resistant steel submitted to simulated atmospheric corrosion10.1016/j.corsci.2011.09.023 ↗
28. Leygraf · 2000
29. Progress in research on rust layer of weathering steel
30. Corrosion behavior of rusted mild steel under means of wet/dry alternate conditions
31. Atmospheric corrosion of different steels in marine, rural and industrial environments10.1016/S0010-938X(99)00005-0 ↗
32. Composition and protective ability of rust layer formed on weathering steel exposed to various environments10.1016/j.corsci.2005.10.004 ↗
33. On the rust products formed on weathering and carbon steels exposed to chloride in dry–wet cyclical processes10.1007/s10751-005-9175-3 ↗
34. Atmospheric corrosion investigation in industrial, marine and rural environments in South-East brazil
35. Study on the rusting evolution and the performance of resisting to atmospheric corrosion for Mn–Cu steel10.3724/SP.J.1037.2010.01365 ↗
36. Corrosion evolution of MnCuP weathering steel submitted to wet/dry cyclic tests in a simulated coastal atmosphere10.1016/j.corsci.2012.01.017 ↗
37. In-depth distribution of rusts on a plain carbon steel and weathering steels exposed to coastal-industrial atmosphere for 17years10.1016/S0010-938X(03)00070-2 ↗
38. Whitney award lecture – don’t be afraid of electrochemical techniques but use them with care10.5006/1.3584957 ↗
39. Determination of corrosion rates by electrochemical DC and AC methods10.1016/0010-938X(81)90015-9 ↗
40. Minimization of high-frequency phase-shifts in impedance measurements10.1149/1.2095825 ↗
41. Rusting evolution of MnCuP weathering steel submitted to simulated industrial atmospheric corrosion10.1007/s11661-011-0977-4 ↗
42. Aqueous corrosion behaviour of weathering steel and carbon steel in acid-chloride environments10.5006/1.3280508 ↗
43. Changes in atmospheric corrosion rate caused by chloride ions depending on rain regime10.1016/j.corsci.2004.06.003 ↗
44. The mechanism of formation of iron oxide and oxyhydroxides in aqueous solutions at room temperature10.1016/S0010-938X(74)80051-X ↗
45. Initial stages of atmospheric corrosion of steel in the Arabian Gulf10.1016/0010-938X(91)90123-7 ↗
46. An electrochemical study of phase-transition in rust layers10.1016/0010-938X(83)90024-0 ↗