Source abstract
Abstract
Abstract Erosion–corrosion (E–C) behaviour of a Fe-based amorphous metallic coating (AMC) compared with 304 stainless steel (304 s.s.) was studied under a slurry impingement condition in a sand-containing NaCl solution. AMC exhibited much higher resistance to E–C than 304 s.s. The weight loss reached the maximum at an impact angle of 90° and the critical flow velocity was about 15 m/s for AMC, while 45° and 9 m/s for 304 s.s. The increment in passive current density under impingement for AMC was about 10 times lower than 304 s.s. Passive films formed at different impact velocities were of different thicknesses.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metallic Glasses and Amorphous Alloys · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Wear behaviour of an amorphous alloy10.1016/0043-1648(84)90216-3 ↗
2. Abrasive wear behaviour of Fe, Co and Ni based metallic glasses10.1016/j.wear.2004.09.010 ↗
3. Synthesis of Fe–Cr–Mo–C–B–P bulk metallic glasses with high corrosion resistance10.1016/S1359-6454(01)00366-4 ↗
4. Difference in compressive and tensile fracture mechanisms of Zr59CU20Al10Ni8Ti3 bulk metallic glass10.1016/S1359-6454(02)00521-9 ↗
5. J. Farmer, F. Wong, J. Haslam, J. Estill, D. Branagan, N. Yang, C. Blue, Development, processing and testing of high-performance corrosion-resistant HVOF coatings, in: Global 2003 Topical Meeting at the American Nuclear Society Conference, 2003.
6. Structural study of iron-based microstructured and nanostructured powders sprayed by HVOF thermal spraying10.1016/j.surfcoat.2004.02.023 ↗
7. Formation and corrosion behaviour of Fe-based amorphous metallic coatings by HVOF thermal spraying10.1016/j.surfcoat.2009.08.025 ↗
8. Effects of crystallization on the corrosion resistance of Fe-based amorphous coatings10.1016/j.corsci.2012.02.003 ↗
9. A comparison between the corrosion resistances of some HVOF-sprayed metal alloy coatings10.1016/j.surfcoat.2008.04.056 ↗
10. Electrochemical behaviour of Fe-based metallic glasses in acidic and neutral solutions10.1016/j.corsci.2012.05.025 ↗
11. Influence of yttrium as a minority alloying element on the corrosion behaviour in Fe-based bulk metallic glasses10.1016/j.electacta.2008.08.017 ↗
12. Cavitation erosion characteristics of a Fe–Cr–Si–B–Mn coating fabricated by high velocity oxy-fuel (HVOF) thermal spray10.1016/j.matlet.2006.07.147 ↗
13. Microstructure and properties of Fe-based amorphous metallic coating produced by high velocity axial plasma spraying10.1016/j.jallcom.2009.04.086 ↗
14. Slurry erosion–corrosion behaviour of high-velocity oxy-fuel (HVOF) sprayed Fe-based amorphous metallic coatings for marine pump in sand-containing NaCl solutions10.1016/j.corsci.2011.05.062 ↗
15. Single particle impingement current transients for prediction of erosion–enhanced corrosion on 304 stainless steel10.1016/j.corsci.2010.03.007 ↗
16. Some comments on mapping the combined effects of slurry concentration, impact velocity and electrochemical potential on the erosion–corrosion of WC/Co–Cr coatings10.1016/j.wear.2007.02.025 ↗
17. Erosion–corrosion of stainless steel under impingement by a fluid jet10.1016/j.corsci.2006.05.012 ↗
18. An assessment of the corrosion behaviour of high-grade alloys in seawater at elevated temperature and under a high velocity impinging flow10.1016/0010-938X(96)00180-1 ↗
19. Erosion–corrosion of candidate HVOF aluminium-based marine coatings10.1016/S0043-1648(03)00564-7 ↗
20. Effect of impact angle on the slurry erosion–corrosion of 304L stainless steel10.1016/S0043-1648(00)00344-6 ↗
21. Electrochemical corrosion behaviour of X-65 steel in the simulated oil–sand slurry. II: Synergism of erosion and corrosion10.1016/j.corsci.2008.01.019 ↗
22. Cavitation erosion and jet impingement erosion mechanism of cold sprayed Ni–Al2O3 coating10.1016/j.nucengdes.2011.09.038 ↗
23. The electrochemical response of stainless steels in liquid–solid impingement10.1016/j.wear.2004.09.043 ↗
24. On the critical flow velocity of Cu–Ni alloy BFe30-1-1 in flowing artificial seawater
25. Effect of flow velocity and entrained sand on inhibition performances of two inhibitors for CO2 corrosion of N80 steel in 3% NaCl solution10.1016/j.corsci.2004.11.012 ↗
26. Effect of porosity sealing treatments on the corrosion resistance of high-velocity oxy-fuel (HVOF)-sprayed Fe-based amorphous metallic coatings10.1016/j.surfcoat.2011.08.045 ↗
27. Study of structure and corrosion resistance of Fe-based amorphous coatings prepared by HVAF and HVOF10.1016/j.corsci.2010.12.022 ↗
28. High-strength bulk amorphous-alloys with low critical cooling rates10.2320/matertrans1989.36.866 ↗
29. Formation of amorphous and nanocrystalline phases in high velocity oxy-fuel thermally sprayed a Fe–Cr–Si–B–Mn alloy10.1016/j.msea.2006.05.095 ↗
30. Erosion–corrosion resistance of microcrystalline and near-nanocrystalline WC-17Co high velocity oxy-fuel thermal spray coatings10.1016/j.corsci.2011.02.028 ↗
31. Corrosion performance of HVOF and APS thermally sprayed NiTi intermetallic coatings in 3.5% NaCl solution10.1016/j.corsci.2009.11.034 ↗
32. Influence of the size of spraying powders on the microstructure and corrosion resistance of Fe-based amorphous coating10.1016/j.electacta.2011.05.020 ↗
33. The influence of corrosion on the erosion of aluminum by aqueous silica slurries10.1016/0043-1648(95)07181-4 ↗
34. Impact angle effects on the erosion–corrosion of superlattice CrN/NbN PVD coatings10.1016/j.surfcoat.2004.07.075 ↗
35. A study of the erosion–corrosion of PVD CrN/NbN superlattice coatings in aqueous slurries10.1016/j.wear.2005.01.047 ↗
36. The effects of angle of impact and material properties on the erosion fates of ceramics10.1016/0043-1648(95)07130-X ↗
37. The birth of corrosion pits as stimulated by slurry erosion10.1016/S0010-938X(99)00100-6 ↗
38. An examination of the electrochemical characteristics of two stainless steels (UNS S32654 and UNS S31603) under liquid–solid impingement10.1016/S0043-1648(03)00563-5 ↗
39. Erosion–corrosion behaviour of nano-particle-reinforced Ni matrix composite alloying layer by duplex surface treatment in aqueous slurry environment10.1016/j.corsci.2009.02.029 ↗
40. Mapping erosion–corrosion of carbon steel in oil exploration conditions: some new approaches to characterizing mechanisms and synergies10.1016/j.triboint.2010.01.005 ↗
41. Erosion–corrosion of carbon steel in simulated tailing slurries10.1016/j.corsci.2010.11.034 ↗
42. Corrosion and synergy in a WCCoCr HVOF thermal spray coating—understanding their role in erosion–corrosion degradation10.1016/j.wear.2004.12.003 ↗
43. Erosion–corrosion resistance of engineering materials in various test conditions10.1016/j.wear.2009.01.052 ↗
44. Erosion–corrosion of 2205 duplex stainless steel in flowing seawater containing sand particles10.1016/j.corsci.2006.08.023 ↗
45. The influence of the flow field in slurry erosion10.1016/0043-1648(92)90122-O ↗
46. Erosion–corrosion behaviour of Zr-based bulk metallic glass in saline-sand slurry10.1016/j.triboint.2012.10.010 ↗