journal article·2006-05

Hydrogen effects on the passive film formation and pitting susceptibility of nitrogen containing type 316L stainless steels

S. Ningshen, U. Kamachi Mudali, G. Amarendra, P. Gopalan, R.K. Dayal, H.S. Khatak

Corrosion Science· Volume 48· Issue 5
Publisher page

Abstract

Abstract The effects of hydrogen on the passivity and pitting susceptibility of type 316L stainless steels have been investigated with alloys containing different nitrogen contents (0.015, 0.198 and 0.556 wt.% N). The study revealed that electrochemically pre-charged hydrogen significantly reduced the pitting resistance of alloys conatining 0.015 and 0.198 wt.% nitrogen contents. In alloy with highest nitrogen content (0.556 wt.% N), an increase in the passive film current density with hydrogen was observed without affecting breakdown potential. Auger electron spectroscopy (AES) analysis of the passive film indicated the presence of nitrogen in the passive film. On other hand, for hydrogen charged samples, nitrogen was found to be significantly less in the passive film. In Electrochemical impedance spectroscopy (EIS) measurement, the decrease in semi-circle radius of Nyquist plot, and the polarization resistance, R P associated with the resistance of the passive film was observed with hydrogen, indicating that hydrogen decreased the stability of the passive film. The present investigation indicated that precharged hydrogen deteriorated the passive film stability and pitting corrosion resistance in these alloys, and the increase in nitrogen content of the alloy offsets the deleterious effect of precharged hydrogen.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Kruger · Int. Mater. Rev. · 1988 · 33 · 11310.1179/imr.1988.33.1.113 ↗
2. Olsson · Electrochim. Acta · 2003 · 48 · 109310.1016/S0013-4686(02)00841-1 ↗
3. Armacanqui · Corrosion · 1988 · 44 · 69610.5006/1.3584931 ↗
4. Zakroczymsky · Corrosion · 1983 · 39 · 20710.5006/1.3580838 ↗
5. Hasegawa · Corrosion · 1983 · 39 · 11510.5006/1.3580826 ↗
6. Yang · Corrosion · 1988 · 54 · 62810.5006/1.3287639 ↗
7. Yashiro · Corros. Sci. · 1998 · 40 · 78110.1016/S0010-938X(97)00178-9 ↗
8. McKibben · Acta Metall. · 1987 · 35 · 25310.1016/0001-6160(87)90233-1 ↗
9. Clayton · Mater. Sci. Eng. A · 1995 · 198 · 13510.1016/0921-5093(95)80068-6 ↗
10. U. Kamachi Mudali, Studies on Pitting, Intergranular Corrosion and Passive Film in Nitrogen-Bearing Austenitic Stainless Steels, Ph.D. Thesis, University of Madras, Chennai, India, 1993.
11. Osozawa · 1976 · 135
12. Newman · Corros. Sci. · 1987 · 27 · 82710.1016/0010-938X(87)90040-0 ↗
13. Kamachi Mudali · Werkst. Korros. · 1986 · 37 · 456
14. Turnbull · 1990 · 121
15. Uhlemann · Mater. Sci. Forum. · 1999 · 318–320 · 52310.4028/www.scientific.net/MSF.318-320.523 ↗
16. 1987
17. Yang · J. Electrochem. Soc. · 1994 · 141 · 266910.1149/1.2059166 ↗
18. Olefjord · Corros. Sci. · 1990 · 31 · 8910.1016/0010-938X(90)90095-M ↗
19. Clayton · J. Electrochem. Soc. · 1986 · 133 · 246510.1149/1.2108451 ↗
20. Kirchheim · Corros. Sci. · 1989 · 29 · 89910.1016/0010-938X(89)90060-7 ↗
21. Sato · Corros. Sci. · 1970 · 10 · 78510.1016/S0010-938X(70)80002-6 ↗
22. Murphy · J. Electrochem. Soc. · 1984 · 131 · 278510.1149/1.2115408 ↗
23. Lu · J. Electrochem. Soc. · 1983 · 130 · 177410.1149/1.2120091 ↗
24. Gavriljuk · Acta Mater. · 2003 · 51 · 129310.1016/S1359-6454(02)00524-4 ↗
25. Okamoto · Nature · 1965 · 206 · 135010.1038/2061350a0 ↗
26. Ruetschi · J. Electrochem. Soc. · 1988 · 135 · 2662
27. Wallinder · Corros. Sci. · 2001 · 43 · 126710.1016/S0010-938X(00)00154-2 ↗
28. Qin · Brit. Corros. J. · 2001 · 36 · 3310.1179/000705901101501451 ↗
29. Yang · J. Electrochem. Soc. · 2001 · 148 · B2910.1149/1.1344529 ↗
30. Pyun · Corros. Sci. · 1989 · 29 · 48510.1016/0010-938X(89)90001-2 ↗
31. Ningshen · Brit. Corros. J. · 2001 · 36 · 3610.1179/000705901101501460 ↗
32. Caskay · Scr. Met. · 1981 · 14 · 118710.1016/0036-9748(81)90295-7 ↗
33. Ningshen · Corros. Sci. · 2001 · 43 · 225510.1016/S0010-938X(01)00017-8 ↗
34. Uhlemann · Mater. Sci. Technol. · 2002 · 18 · 117910.1179/026708302225006124 ↗
35. Kamachi Mudali · Bull. Electrochem. · 1999 · 15 · 74
36. Casanova · Corros. Sci. · 1996 · 38 · 153510.1016/0010-938X(96)00045-5 ↗