Hydrogen influence on some advanced high-strength steels

Qinglong Liu, Qingjun Zhou, Jeffrey Venezuela, Mingxing Zhang, Andrej Atrens

Corrosion Science· Volume 125
Publisher page

Abstract

This paper studied the influence of hydrogen on some dual-phase (DP), quenching and partitioning (Q&P), and twinning-induced plasticity (TWIP) advanced high-strength steels (AHSS). All steels exhibited hydrogen sensitivity, manifested by (i) decreased yield strength (by a maximum of 13%) attributed to solid-solution softening by hydrogen, and (ii) reduced ductility (maximum decrease of reduction of area was from 65% to 9%), caused by hydrogen assisted fracture processes after the onset of necking. There was no sub-critical crack growth below the ultimate tensile strength. The hydrogen influence increased with increasing strength, more negative charging potential, and decreasing stress rate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (91)

Show source-provided references
1. Developments in advanced high strength steels
2. WorldAutoSteel · 2017
3. Zhu · 2007 · 1
4. A review of the influence of hydrogen on the mechanical properties of DP, TRIP, and TWIP advanced high-strength steels for auto construction10.1016/j.corsci.2016.01.032 ↗
5. Hydrogen embrittlement of advanced high strength steels for automotive use
6. BC De Cooman · 2009 · 165
7. BaoSteel · 2013
8. Baosteel · 2013
9. Matlock · 2009 · 185
10. Quenching and partitioning martensite—a novel steel heat treatment10.1016/j.msea.2006.02.133 ↗
11. Overview of mechanisms involved during the quenching and partitioning process in steels10.1007/s11661-011-0706-z ↗
12. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
13. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
14. A new model for hydrogen-assisted cracking (hydrogen embrittlement)10.1007/BF02642048 ↗
15. Hydrogen-enhanced localization of plasticity in an austenitic stainless steel10.1007/BF02669644 ↗
16. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
17. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process10.1016/0001-6160(88)90113-7 ↗
18. Hydrogen embrittlement of automotive advanced high-strength steels10.1007/s11661-012-1280-8 ↗
19. Hydrogen damage in superaustenitic 904L stainless steels10.1007/s11665-014-1044-2 ↗
20. Effect of hydrogen charging on the mechanical properties of advanced high strength steels10.1016/j.ijhydene.2013.12.190 ↗
21. Effects of hydrogen on the properties of iron and steel10.1007/BF02654700 ↗
22. Characterization of hydrogen embrittlement in automotive advanced high strength steels10.1002/mawe.201100917 ↗
23. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
24. Hydrogen embrittlement of dual-phase steels10.1007/BF02643572 ↗
25. Hydrogen effects on cathodically charged twinning-induced plasticity steel10.1016/j.scriptamat.2011.12.012 ↗
26. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
27. Linearly increasing stress test (LIST) for SCC research10.1088/0957-0233/4/11/017 ↗
28. The influence of hydrogen on 3.5NiCrMoV steel studied using the linearly increasing stress test10.1016/j.corsci.2012.10.019 ↗
29. Influence of hydrogen on the mechanical properties of some medium-strength Ni?Cr?Mo steels10.1016/j.msea.2014.08.056 ↗
30. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test10.1016/j.corsci.2015.06.038 ↗
31. Influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels in simulated service conditions10.1016/j.corsci.2016.05.040 ↗
32. Comparison of the linearly increasing stress test and the constant extension rate test in the evaluation of transgranular stress corrosion cracking of magnesium10.1016/j.msea.2007.03.021 ↗
33. The influence of microstructure on hydrogen diffusion and embrittlement of multiphase fine-grained steels with increased plasticity and strength
34. Hydrogen embrittlement of a medium carbon Q&P steel
35. Effect of retained austenite stability and morphology on the hydrogen embrittlement susceptibility in quenching and partitioning treated steels10.1016/j.msea.2016.02.026 ↗
36. Effect of retained austenite on the hydrogen embrittlement of a medium carbon quenching and partitioning steel with refined microstructure10.1016/j.msea.2016.04.025 ↗
37. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
38. Electrochemical corrosion and hydrogen diffusivity in dual-phase steel
39. Effect of aluminium on hydrogen-induced fracture behaviour in austenitic Fe–Mn–C steel10.1098/rspa.2012.0458 ↗
40. Effect of hydrogen content on the embrittlement in a Fe?Mn?C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
41. Stress corrosion cracking of high-strength steels10.1515/corrrev-2012-0018 ↗
42. Metallurgical aspects of rock bolt stress corrosion cracking10.1016/j.msea.2007.11.086 ↗
43. Hydrogen embrittlement and rock bolt stress corrosion cracking10.1016/j.engfailanal.2008.01.004 ↗
44. E562-08 · 2008
45. E-112 · 2010
46. Vander Voort · 1984
47. Determination of the hydrogen fugacity during electrolytic charging of steel10.1016/j.corsci.2014.06.033 ↗
48. Hydrogen trapping in some advanced high strength steels10.1016/j.corsci.2016.05.046 ↗
49. Hydrogen concentration in dual-Phase (DP) and quenched and partitioned (Q&P) advanced high-Strength steels (AHSS) under simulated service conditions compared with cathodic charging conditions10.1002/adem.201600217 ↗
50. Influence of martensite content on the hydrogen embrittlement of dual-phase steels10.1016/0036-9748(83)90255-7 ↗
51. Non-Metallic inclusions in TWIP steel10.1002/srin.201300354 ↗
52. The effect of Ti precipitates on hydrogen embrittlement of Fe–18Mn–0. 6 C–2Al–xTi twinning-induced plasticity steel10.1016/j.corsci.2014.08.005 ↗
53. Some aspects of high manganese twinning-induced plasticity (TWIP) steel, a review10.1007/s40195-012-0501-x ↗
54. Characterization of hydrogen induced cracking in TRIP-assisted steels10.1016/j.ijhydene.2015.06.017 ↗
55. Electrochemical studies of hydrogen diffusion and permeability in Ni10.1016/0010-938X(80)90102-X ↗
56. The influence of hydrogen on the sub-structure of the martensite and ferrite dual-phase steel10.1016/0036-9748(89)90352-9 ↗
57. Study of hydrogen embrittlement of the trip 800 steels by means of tensile tests at simultaneous hydrogen charging
58. Crank · 1979
59. Reversible hydrogen trapping in a 3.5NiCrMoV medium strength steel10.1016/j.corsci.2015.04.011 ↗
60. Hydrogen embrittlement susceptibility of tempered 9%Cr–1%Mo steel10.1016/j.ijhydene.2011.08.096 ↗
61. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
62. Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe–Mn–C TWIP steels10.1016/j.corsci.2014.01.022 ↗
63. Effect of sample thickness on the tensile behaviors of Fe–30Mn–3Si–3Al twinning-induced plasticity steel10.1016/j.msea.2015.07.004 ↗
64. Multiscale mechanics of TRIP-assisted multiphase steels: I. Characterization and mechanical testing10.1016/j.actamat.2007.02.029 ↗
65. Multiscale mechanics of TRIP-assisted multiphase steels: II. Micromechanical modelling10.1016/j.actamat.2007.02.015 ↗
66. Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel10.1016/j.actamat.2012.04.010 ↗
67. Delayed static failure of twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.038 ↗
68. Hydrogen transport by dislocations10.1007/BF02644079 ↗
69. Improved resistance to hydrogen embrittlement in a high-strength steel by quenching–partitioning–tempering treatment10.1016/j.scriptamat.2014.10.030 ↗
70. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
71. Effect of morphology of second-phase martensite on tensile properties of Fe-0.1C dual phase steels10.1007/BF00580148 ↗
72. Effects of cryogenic and tempered treatment on the hydrogen embrittlement susceptibility of TRIP-780 steels10.1016/j.ijhydene.2013.05.113 ↗
73. Hydrogen effects in prestrained transformation induced plasticity steel10.1007/s11661-011-1075-3 ↗
74. Hydrogen embrittlement studies of a trip steel10.1007/BF02648707 ↗
75. Effect of hydrogen on the properties and fracture characteristics of TRIP 800 steels10.1016/j.corsci.2011.04.015 ↗
76. The effect of Si on hydrogen embrittlement of Fe-18Mn-0.6C-xSi twinning-induced plasticity steels10.1016/j.actamat.2015.10.015 ↗
77. Effects of static and dynamic strain aging on hydrogen embrittlement in TWIP steels containing Al10.2355/isijinternational.53.1268 ↗
78. The mechanism of enhanced resistance to the hydrogen delayed fracture in Al-added Fe–18Mn–0. 6C twinning-induced plasticity steels10.1016/j.ijhydene.2012.03.100 ↗
79. Fractographic analysis of the role of hydrogen diffusion on the hydrogen embrittlement susceptibility of DP steel10.1016/j.msea.2015.09.124 ↗
80. The role of dislocations during transport of hydrogen in hydrogen embrittlement of iron10.1007/BF02645814 ↗
81. Trap theory of Hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
82. An example of the effect of hydrogen trapping on hydrogen embrittlement10.1007/BF02648348 ↗
83. Notch ductility of steels for automotive components10.1016/j.engfracmech.2014.06.007 ↗
84. Shear fracture of advanced high strength steels10.1016/S1006-706X(14)60165-5 ↗
85. Nagumo · 2009 · 95 · 222
86. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe-Mn-Al-C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
87. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe-18Mn-1.5 Al-0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
88. Moeser · 2016
89. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
90. Hydrogen traps, repellers, and obstacles in steel; Consequences on hydrogen diffusion solubility, and embrittlement10.1007/BF02662391 ↗
91. A quantitative analysis of hydrogen trapping10.1007/BF02661939 ↗