Galfan coatings on steel in laboratory exposures with predeposited NaCl and cyclic wet/dry conditions exhibit nearly the same corrosion products as after 5 years of marine exposure. A general scenario for corrosion product evolution on Galfan in chloride-rich atmospheres is proposed. It includes the initial formation of ZnO, ZnAl2O4 and Al2O3 and subsequent formation of Zn6Al2(OH)16CO3⋅4H2O, and Zn2Al(OH)6Cl⋅2H2O and/or Zn5Cl2(OH)8⋅H2O. An important phase is Zn6Al2(OH)16CO3⋅4H2O, which largely governs the reduced long-term zinc runoff from Galfan. A clear influence of microstructure could be observed on corrosion initiation in the slightly zinc-richer η-Zn phase adjacent to the β-Al phase.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Magnesium Oxide Properties and Applications · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Zhang · 1996
2. ArcelorMittal, Steels coated with Galfan zinc–aluminum alloy, 2008.
3. Surface characterization of hot-dip Galfan coatings10.1016/1044-5803(94)90071-X ↗
4. The Al−Zn (aluminum–zinc) system
5. The metallurgy of zinc-coated steel10.1016/S0079-6425(98)00006-1 ↗
6. Relationship between microstructure and corrosion resistance in Zn–Al alloy coated Galvanised steels10.1179/147842203770226924 ↗
7. The microstructure of annealed Galfan coating on steel substrate10.2478/v10172-012-0054-z ↗
8. Grain boundary wetting by a solid phase; microstructural development in a Zn–5wt.% Al alloy10.1016/j.actamat.2004.06.011 ↗
9. Microstructural changes in zinc aluminum alloy Galvanising as a function of processing parameters and their influence on corrosion10.1016/j.corsci.2004.11.011 ↗
10. Corrosion susceptibility of Zn–Al alloys with different grains and dendritic microstructures in Nacl solutions10.1016/j.corsci.2012.03.015 ↗
11. The effect of the dendritic microstructure on the corrosion resistance of Zn–Al alloys10.1016/j.jallcom.2005.01.035 ↗
12. Atmospheric corrosion of zinc Part 1: rural and urban atmospheres10.1179/000705900101501353 ↗
13. Atmospheric corrosion of zinc Part 2: marine atmospheres10.1179/000705900101501362 ↗
14. Long-term atmospheric corrosion of zinc10.1016/j.corsci.2006.08.003 ↗
15. Corrosion mechanisms for zinc exposed to the atmosphere10.1149/1.2096868 ↗
16. The atmospheric corrosion of zinc: the effects of salt concentration, droplet size and droplet shape10.1016/j.electacta.2010.09.099 ↗
17. Odnevall · 1995
18. In situ infrared reflection absorption spectroscopy studies of confined zinc surfaces exposed under periodic wet–dry conditions10.1149/1.1359397 ↗
19. Simultaneous infrared reflection absorption spectroscopy and quartz crystal microbalance measurements for in situ studies of the metal/atmosphere interface10.1149/1.1837948 ↗
20. Corrosion of Zn under acidified marine droplets10.1016/j.corsci.2011.01.044 ↗
21. Initial NaCl-particle induced atmospheric corrosion of zinc-Effect of CO2 and SO210.1016/j.corsci.2007.06.005 ↗
22. Atmospheric corrosion products on AlZn and AlZn metallic coatings10.5006/1.3584923 ↗
23. S.A. Matthes, S.D. Cramer, S.J. Bullard, B.S. Covino, B.S. Covino Jr, G.R. Holcomb, Atmospheric corrosion and precipitation runoff from zinc and zinc alloy surfaces, in: NACE Corrosion Conference, San Diego, CA (US), 2003.10.5006/C2003-03598 ↗
24. Atmospheric corrosion of zinc-based materials: runoff rates, chemical speciation and ecotoxicity effects10.1016/S0010-938X(00)00136-0 ↗
25. Atmospheric corrosion resistance of aluminum–zinc alloy-coated steel
26. Corrosion product formation on Zn55Al coated steel upon exposure in a marine atmosphere10.1016/j.corsci.2010.11.004 ↗
27. Formation of nano-crystalline corrosion products on Zn–Al alloy coating exposed to seawater10.1016/S0010-938X(00)00169-4 ↗
28. Characterization of black rust staining of unpassivated 55% Al–Zn alloy coatings. Effect of temperature, pH and wet storage10.1016/S0010-938X(99)00043-8 ↗
29. Understanding corrosion via corrosion product characterization: II. role of alloying elements in improving the corrosion resistance of Zn–Al–Mg coatings on steel10.1016/j.corsci.2011.03.016 ↗
30. Evolution of corrosion products and metal release from Galvalume coatings on steel during short and long-term atmospheric exposures10.1016/j.matchemphys.2012.01.054 ↗
31. The initial release of zinc and aluminum from non-treated Galvalume and the formation of corrosion products in chloride containing media10.1016/j.apsusc.2011.12.112 ↗
32. Zn/55Al coating microstructure and corrosion mechanism10.1016/j.corsci.2005.02.012 ↗
33. Corrosion performance of aluminum-containing zinc coatings10.2355/isijinternational.50.455 ↗
34. Corrosion behavior of superplastic Zn–Al alloys in simulated acid rain10.1016/j.corsci.2012.03.013 ↗
35. Neuer Laborkorrosionstest – relevante Ergebnisse10.1007/BF03241828 ↗
36. Chen · 2004
37. Quantitative in situ analysis of initial atmospheric corrosion of copper induced by acetic acid10.1149/1.2715315 ↗
38. ISO, ISO 17752:2012, Corrosion of metals and alloys – procedures to determine and estimate runoff rates of metals from materials as a result of atmospheric corrosion, 2012.
39. Corrosion-induced zinc runoff from construction materials in a marine environment10.1149/1.2403078 ↗
40. Long-term use of Galvanized steel in external applications. Aspects of patina formation, zinc runoff, barrier properties of surface treatments, and coatings and environmental fate10.1007/s10661-010-1377-8 ↗
41. The anodic dissolution of zinc and zinc alloys in alkaline solution. II. Al and Zn partial dissolution from 5% Al–Zn coatings10.1016/j.electacta.2012.04.037 ↗
42. T.E. Madey, J.T.J. Yates., Vibrational Spectroscopy of Molecules on Surfaces, first edition, Methods of Surface Characterization, Springer, 1987.
43. Synthesis and vibrational spectroscopic characterisation of synthetic hydrozincite and smithsonite10.1016/j.poly.2007.07.002 ↗
44. Thermo-Raman spectroscopy of selected layered double hydroxides of formula Cu6Al2(OH)16CO3 and Zn6Al2(OH)16CO310.1002/jrs.2148 ↗
45. Spatial distribution and formation of corrosion products in relation to zinc release for zinc sheet and coated pre-weathered zinc at an urban and a marine atmospheric condition
46. Characterization of nanosized ZnAl2O4 spinel synthesized by the sol–gel method10.1007/s10971-008-1833-x ↗
47. S. Sunder, S. Rohilla, S. Kumar, P. Aghamkar, Structural characterization of spinel zinc aluminate nanoparticles prepared by coprecipitation method, in: S.K. Tripathi, K. Dharamvir, R. Kumar, G.S.S. Saini, (Eds.), International Conference on Advances in Condensed and Nanomaterials, 2011.10.1063/1.3653640 ↗
48. Development of Al-containing zinc-rich paints for corrosion resistance10.1016/S0169-4332(01)00985-0 ↗
49. Template route to chemically engineering cavities at nanoscale: a case study of Zn(OH)2 template10.1007/s11671-010-9711-1 ↗
50. Relationship between properties of pseudo-boehmite and its synthetic conditions
51. Effects of sodium chloride particles, ozone, UV, and relative humidity on atmospheric corrosion of silver10.1149/1.3310812 ↗
52. Effect of carbon dioxide on sodium chloride-induced atmospheric corrosion of copper10.1149/1.2098327 ↗
53. Intracrystalline oxidation of thiosulfate-intercalated layered double hydroxides10.1021/la803402j ↗
54. Formation of NaZn4Cl(OH)6SO4⋅6H2O in a marine atmosphere10.1016/0010-938X(93)90082-R ↗
55. Synthesis and characterization of Ni–Al2O3 composite coatings containing different forms of alumina10.1007/s10800-010-0198-3 ↗
56. Structural characterization of phase transition of Al2O3 nanopowders obtained by polymeric precursor method10.1016/j.matchemphys.2007.02.046 ↗
57. Self-organized ZnAl2O4 nanostructures grown on c-sapphire10.1016/j.spmi.2007.04.015 ↗
58. Leygraf · 2000
59. Chemistry of corrosion products on Zn–Al–Mg alloy coated steel10.1016/j.corsci.2010.05.044 ↗
60. Corrosion products of hot-dip Zn–6%Al–3%Mg coated steel sheet subjected to atmospheric exposure Tetsu to Hagane10.2355/tetsutohagane1955.89.1_166 ↗
61. Analysis of the corrosion products on galvanized steels by FTIR spectroscopy10.1016/S0254-0584(98)00167-9 ↗
62. Thermal characterization of poly(styrene sulfonate) layered double hydroxide nanocomposites10.1346/CCMN.1997.0450207 ↗
63. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗
64. Pitting corrosion of Zn and Zn–Al coated steels in pH 2 to 12 NaCl solutions10.1149/1.2372691 ↗
65. Zinc aluminum layered double hydroxides for the removal of iodine and iodide from aqueous solutions10.1080/19443994.2012.669171 ↗
66. Corrosion mechanisms for aluminum exposed to the atmosphere10.1149/1.2096869 ↗
67. Occurrence and fate of corrosion-induced zinc in runoff water from external structures10.1016/j.scitotenv.2006.01.008 ↗