Towards a better understanding of localised corrosion induced by typical non-metallic inclusions in low-alloy steels
Source abstract
Abstract
Abstract Detailed understanding of localised corrosion phenomena induced by inclusions in low-alloy steel is extremely critical as any corrosion-induced premature failure can potentially lead to a catastrophe. In particular, there is still ambiguity as to whether the localised corrosion initiation induced by non-metallic inclusions is an electrochemical process or a chemical process. Herein, the localised heterogeneous electrochemical mechanism of typical non-metallic inclusions–Al2O3, ZrO2-Ti2O3-Al2O3, and (RE)AlO3-(RE)2O2S-(RE)xSy – was investigated using scanning Kelvin probe force microscopy and current-sensing atomic force microscopy. The chemical stability of typical non-metallic inclusions was characterized by Pourbaix diagrams. The results indicate that the localised corrosion behaviour shows no correlation to the Volta potential difference between the non-metallic inclusions and the matrix. Moreover, the localised corrosion initiation process is mainly a chemical corrosion process rather than an electrochemical corrosion process. Thus, the applicability of Volta potential difference in predicating the preferential corrosion area in different system (conductive/nonconductive system) should be given full attention.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
2. Stress corrosion cracking behavior of X70 pipe steel in an acidic soil environment10.1016/j.corsci.2008.05.011 ↗
3. Influence of rare earth metals on mechanisms of localised corrosion induced by inclusions in Zr-Ti deoxidised low alloy steel10.1016/j.corsci.2020.108463 ↗
4. The effect of nonmetal inclusions and microstructure on local corrosion of carbon and low-alloyed steels10.1023/B:PROM.0000043062.19272.c5 ↗
5. Role of Al2O3 inclusions on the localized corrosion of Q460NH weathering steel in marine environment10.1016/j.corsci.2018.04.007 ↗
6. Mechanism of (Mg,Al,Ca)-oxide inclusion-induced pitting corrosion in 316L stainless steel exposed to sulphur environments containing chloride ion10.1016/j.corsci.2012.09.044 ↗
7. Materials science: share corrosion data10.1038/527441a ↗
8. Pitting corrosion of X70 pipeline steel in the simulated wet storage environment
9. Use of the electrochemical microcell technique and the SVET for monitoring pitting corrosion at MnS inclusions10.1016/j.elecom.2004.05.001 ↗
10. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in NaCl solution10.5006/1837 ↗
11. Effect of SO42− on the corrosion of 316L stainless steel in molten FLiNaK salt10.1016/j.corsci.2018.08.057 ↗
12. In situ characterization by localized electrochemical impedance spectroscopy of the electrochemical activity of microscopic inclusions in an X100 steel10.1016/j.corsci.2010.11.026 ↗
13. Pitting corrosion behavior in advanced high strength steels10.1016/j.jallcom.2014.08.243 ↗
14. Pitting initiation and propagation of x70 pipeline steel exposed to chloride-containing environments10.3390/ma10091076 ↗
15. Initial microzonal corrosion mechanism of inclusions associated with the precipitated (Ti, Nb)N phase of Sb-containing weathering steel10.1016/j.corsci.2019.108232 ↗
16. Identification of MnCr2O4 nano-octahedron in catalysing pitting corrosion of austenitic stainless steels10.1016/j.actamat.2010.05.043 ↗
17. Mechanism of Yttrium composite inclusions on the localized corrosion of pipeline steels in NaCl solution10.1016/j.micron.2019.102820 ↗
18. Modelling of pitting corrosion in marine and offshore steel structures – a technical review10.1016/j.jlp.2015.06.008 ↗
19. Effect of inclusions modified by rare earth elements (Ce, La) on localized marine corrosion in Q460NH weathering steel10.1016/j.corsci.2017.10.001 ↗
20. Why stainless steel corrodes10.1038/415770a ↗
21. Characterization of AA2024-T3 by scanning kelvin probe force microscopy10.1149/1.1838633 ↗
22. Corrosion behaviour of different tempers of AA7075 aluminium alloy10.1016/j.electacta.2004.01.046 ↗
23. The role of Intermetallics on the corrosion initiation of twin roll cast AZ31 Mg alloy10.1149/2.0291509jes ↗
24. SKPFM measured Volta potential correlated with strain localisation in microstructure to understand corrosion susceptibility of cold-rolled grade 2205 duplex stainless steel10.1016/j.corsci.2015.06.035 ↗
25. Effect of annealing temperature on the corrosion behavior of duplex stainless steel studied by in situ techniques10.1016/j.corsci.2011.07.019 ↗
26. Localized corrosion resistance of 21% Cr ferritic stainless steel10.5006/1.3635800 ↗
27. Effect of carbo-nitride-rich and oxide-rich inclusions on the pitting susceptibility of depleted uranium10.1016/j.corsci.2017.05.019 ↗
28. Microscale investigation of the correlation between microstructure and galvanic corrosion of low alloy steel A508 and its welded 309/308L stainless steel overlayer10.1016/j.corsci.2019.03.027 ↗
29. High-resolution Kelvin probe microscopy in corrosion science: scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
30. Unusual correlation between SKPFM and corrosion of nickel aluminum bronzes10.1149/2.0391709jes ↗
31. A. Kosari, H. Zandbergen, F. Tichelaar, P. Visser, P. Taheri, H. terryn, J.M.C. Mol, In-situ nanoscopic observations of dealloying-driven local corrosion from surface initiation to in-depth propagation, Corrosion Science, (Accepted).
32. A. Kosari, F. Tichelaar, P. Visser, H. Zandbergen, H. Terryn, J.M.C. Mol, Dealloying-driven local corrosion by intermetallic constituent particles and dispersoids in aerospace aluminium alloys, Corrosion Science, (Accepted).
33. Analysis of historic copper patinas. Influence of inclusions on patina uniformity10.3390/ma10030298 ↗
34. Electrochemical behavior of 304 stainless steel in marine atmosphere and its simulated solution10.1080/00032719.2012.706847 ↗
35. Long-term monitoring of atmospheric corrosion at weathering steel bridges by an electrochemical impedance method10.1016/j.corsci.2014.06.007 ↗
36. The influence and the mechanism of the precipitate/austenite interfacial C-enrichment on the intergranular corrosion sensitivity in 310S stainless steel10.1016/j.corsci.2016.05.021 ↗
37. Study of nobility of chromium nitrides in isothermally aged duplex stainless steels by using SKPFM and SEM/EDS10.1016/j.corsci.2009.08.057 ↗
38. Characterization of corrosion interfaces by the scanning kelvin probe force microscopy technique10.1149/1.1359199 ↗
39. Nanoscale surface potential imaging of the photocatalytic TiO 2 films on aluminum10.1039/c3ra43082k ↗
40. Stability, reactivity and breakdown of passive films. Problems of recent and future research10.1016/S0013-4686(00)00347-9 ↗
41. Metal-insulator transitions in VO2, Ti2O3 and Ti2-x V x O310.1080/14786439808206565 ↗
42. Kelvin probe force microscopy and its application10.1016/j.surfrep.2010.10.001 ↗
43. Surface potential images of polycrystalline organic semiconductors obtained by Kelvin probe force microscopy10.1007/s00339-008-5035-8 ↗
44. In-situ nanoscale mapping of surface potential in all-solid-state thin film Li-ion battery using Kelvin probe force microscopy10.1063/1.3699214 ↗
45. Determination of contact potential difference by the kelvin probe (Part I) I. Basic principles of measurements
46. Gold nanoclusters on alkali halide surfaces: charging and tunneling10.1063/1.2410223 ↗
47. Kelvin probe force microscopy of semiconductor surface defects10.1103/PhysRevB.70.085320 ↗
48. Influence of space charge on the performance of the Kelvin probe10.1063/1.1367363 ↗
49. Deformation behavior of inclusions in stainless steel strips during multi-pass cold rolling10.1016/j.jmatprotec.2008.02.016 ↗
50. Effects of cerium on the compositional variations in and around inclusions and the initiation and propagation of pitting corrosion in hyperduplex stainless steels10.1016/j.corsci.2013.06.020 ↗
51. Xiaohong · 2010 · 5 · 612
52. Modification Mechanism of Cerium on the Inclusions in Drill Steel
53. E.M. Gutman, Mechanochemistry of Solid Surfaces.
54. Effect of tempering heat treatment on the CO2 corrosion resistance of quench-hardened Cr-Mo low-alloy steels for oil and gas applications10.1016/j.corsci.2019.03.036 ↗
55. Carbon steel corrosion: a review of key surface properties and characterization methods10.1039/C6RA25094G ↗
56. An investigation on dislocation density in cold-rolled copper using electrochemical impedance spectroscopy10.1155/2013/921825 ↗
57. Self-accelerated corrosion of nuclear waste forms at material interfaces10.1038/s41563-019-0579-x ↗
58. Synergistic effect of Al2O3 inclusion and pearlite on the localized corrosion evolution process of carbon steel in marine environment10.3390/ma11112277 ↗
59. Dissolution kinetics of the sulfide-oxide complex inclusion and resulting localized corrosion mechanism of X70 steel in deaerated acidic environment10.1016/j.corsci.2020.108815 ↗
60. Thermodynamics of chemical and electrochemical stability of corrosion active nonmetal inclusions10.1134/S0033173207010043 ↗
61. Strain-induced preferential dissolution at the dislocation emergences in MnS: an atomic scale study10.1080/14786435.2015.1052030 ↗
62. Mechanism of MnS-mediated pit initiation and propagation in carbon steel in an anaerobic sulfidogenic media10.1016/j.corsci.2013.06.049 ↗
63. Influence of alloy sulfur content and bulk electrolyte composition on crevice corrosion initiation of austenitic stainless steel10.5006/1.3284838 ↗