Oxidation behavior of silicon carbide at 1200°C in both air and water–vapor-rich environments
Source abstract
Abstract
Abstract Oxidation of SiC in both air and water–vapor–rich environments was carried out at 1200 °C to examine the effects of different oxidation conditions on the early-stage oxidation behavior of SiC. Two different types of SiC oxidation behavior were found, passive or active, depending on the oxidation environment. All the samples possessed amorphous oxide layers, regardless of the oxidation environment. Three Si oxidation states (SiO, Si 2 O 3 , and SiO 2 ) were observed in this layer. The amorphous Si 2 O 3 state was dominant, and the ratio of the three different states changed with the test conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures10.1016/j.corsci.2010.04.032 ↗
2. Oxidation behavior of Hi-Nicalon SiC monofilament fibers in air and O2–H2O–Ar atmospheres10.1016/j.corsci.2011.12.019 ↗
3. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction10.1016/j.corsci.2013.05.009 ↗
4. Chemical degradation of SiC/SiC composite for the cladding of gas-cooled fast reactor in case of severe accident scenarios10.1016/j.corsci.2012.02.019 ↗
5. A modified dual-layer SiC oxidation protective coating for carbon/carbon composites prepared by onestep pack cementation10.1016/j.corsci.2010.09.043 ↗
6. A simple model for the oxidation of carbon-containing composites10.1016/j.corsci.2009.12.002 ↗
7. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
8. Radiation effects in SiC For nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
9. The Fukushima disaster-systemic failure as the lack of resilience10.5516/NET.03.2011.078 ↗
10. Cladding for high performance fuel10.1016/j.pnucene.2011.10.008 ↗
11. Fabrication of SiC/SiC composites for fuel cladding in advanced reactor designs10.1016/j.pnucene.2011.10.002 ↗
12. Thermodynamic analysis of the high-temperature stability of silicon nitride and silicon carbide10.1016/0390-5519(76)90022-3 ↗
13. High-Temperature oxidation of silicon carbide and silicon nitride10.2320/matertrans1989.38.821 ↗
14. Effects of high water–vapor pressure on oxidation of silicon carbide at 1200°C10.1111/j.1151-2916.2003.tb03460.x ↗
15. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
16. Oxidation kinetics of chemically vapor deposited silicon carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
17. Variation of the oxidation rate of silicon carbide with water–vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
18. Oxidation behaviors of C/SiC in the oxidizing environments containing water vapor10.1016/S0921-5093(02)00644-5 ↗
19. Silicon Oxidation Studies: the role of H2O10.1149/1.2133151 ↗
20. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
21. SiC recession caused by SiO2 scale volatility under combustion conditions: II, thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
22. Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions10.4028/www.scientific.net/MSF.461-464.765 ↗
23. Mass Spectrometric Identification of Si–O–H(g) Species from the Reaction of Silica with Water Vapor at Atmospheric Pressure10.1111/j.1151-2916.1997.tb02935.x ↗
24. K.A. Terrani, B.A. Pint, C.M. Parish, C.M. Silva, L.L. Snead, Y. Katoh, Silicon Carbide Oxidation in Steam up to 2 MPa, J. Am. Ceram. Soc. In Press, available online, 2014.10.1111/jace.13094 ↗
25. Oxidation behavior of 3D Hi-Nicalon/SiC composite exposed in wet and simulated air environments10.1016/j.corsci.2012.09.008 ↗
26. NEA (2009), Nuclear Fuel Behaviour in Loss-of-Coolant Accident Conditions, Report NEA No. 6846, ISBN 978-92-64-99091-3, Nuclear Energy Agency, OECD, Paris, France.
27. DRAFT REGULATORY GUIDE DG-1262, “TESTING FOR POSTQUENCH DUCTILIY” by U.S. Nuclear regulatory commission http://pbadupws.nrc.gov/docs/ML 1111/ML111100368.pdf.
28. Exposure of ceramics and ceramic-matrix composites in simulated and actual combustor environments10.1115/1.483197 ↗
29. Observations of accelerated silicon carbide recession by oxidation at high water–vapor pressures10.1111/j.1151-2916.2000.tb01172.x ↗
30. Silicon carbide oxidation in high-pressure steam10.1111/jace.12328 ↗
31. Microscopic structure of the SiO2/Si interface10.1103/PhysRevB.38.6084 ↗
32. High temperature oxidation behavior of SiC coating in TRISO coated particles10.1016/j.jnucmat.2014.06.055 ↗
33. Preparation of a double layer SiC coating and its oxidation resistance at 1773K10.1016/j.corsci.2014.06.024 ↗
34. XPS studies on SiOx thin films10.1016/0169-4332(93)90431-A ↗
35. Electron spectroscopic analysis of the SiO2/Si system and correlation with metal-oxide-semiconductor device characteristics10.1063/1.362676 ↗
36. Direct observation of the layer-by-layer growth of initial oxide layers on Si (100) surface during thermal oxidation10.1103/PhysRevLett.67.2387 ↗
37. Multiple-bonding configuration for oxygen on silicon surfaces10.1103/PhysRevB.28.3651 ↗
38. The localization and crystallographic dependence of Si suboxide species at the SiO2/Si interface10.1063/1.338215 ↗