On the oxidation mechanism of pure tungsten in the temperature range 600–800°C
Source abstract
Abstract
The oxidation behavior of International Thermonuclear Experimental Reactor (ITER)-reference tungsten grade has been evaluated in dry air in the temperature range 600-800 °C. At 600 °C , the scale remained protective while the integrity of W₁₈O₄₉ layer was kept. Rapid increase in mass gain resulted from massive cracking at local areas in the W₁₈O₄₉ layer. Then, a coarse non-protective columnar WO₂.₉₂ scale was developed which favoured rapid inward oxygen transport into the alloy. At 700 and 800 °C, growth stresses in the scale were released through local cracking. At this stage, WO₂.₉₂ became progressively transformed into WO₃ when the oxygen partial pressure increased across the scale thickness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Critical questions in materials science and engineering for successful development of fusion power10.1016/j.jnucmat.2007.02.007 ↗
2. Armour materials for the ITER plasma facing components10.1238/Physica.Topical.081a00074 ↗
3. M. Rieth, J.L. Boutard, S.L. Dudarev, T. Ahlgren, S. Antusch, et al., Review on the EFDA programme on tungsten materials technology and science, J. Nucl. Mater., in press. doi:10.1016/j.jnucmat.2011.01.075.10.1016/j.jnucmat.2011.01.075 ↗
4. Materials for the plasma-facing components of fusion reactors10.1016/j.jnucmat.2004.04.005 ↗
5. D.A. Petti, K.A. McCarthy, W. Gulden, S.J. Piet, Y. Seki, B. Kolbasov, An overview of safety and environmental considerations in the selection of materials for fusion facilities, J. Nucl. Mater. 233–237 (part I) (1996) 37–43.10.1016/S0022-3115(96)00302-9 ↗
6. An investigation for ground state features of some structural fusion materials10.1007/s10894-010-9326-7 ↗
7. Tritium inventory and recovery in next-step fusion devices10.1016/S0920-3796(02)00248-X ↗
8. Materials Assessment Report (MAR), ITER Doc. G 74 MA 10 01-07-11 W 0.2, 2001.
9. Material erosion at the vessel walls of future fusion10.1016/S0022-3115(02)01580-5 ↗
10. Comparison of tokamak behavior with tungsten and low-Z plasma facing materials10.1088/0741-3335/42/12B/322 ↗
11. Plasma-wall interaction: important ion induced surface processes and strategy of the EU task force10.1016/j.nimb.2006.12.168 ↗
12. Temperature transients of a fusion–fission ITER pebble bed reactor in loss of coolant accident10.1016/S0920-3796(02)00162-X ↗
13. Simulation of the sublimation process in the preparation of photochromic WO3 film by laser microprobe mass spectrometry10.1016/S0022-3093(00)00226-X ↗
14. Kinetics of the oxidation of pure tungsten from 500 to 1300°C10.1149/1.2427787 ↗
15. The structure of oxide layers on tungsten10.1149/1.2425800 ↗
16. Oxidation mechanism of niobium (673–823K) and tungsten (773–973K)
17. Kinetics of oxidation of pure tungsten, 1150–1615°C10.1149/1.2426043 ↗
18. Thin oxide films on tungsten
19. Eigenschaften von molybdän und wolfram bei niedrigen und mittleren temperaturen
20. Oxidation of tungsten10.1149/1.2430238 ↗
21. High pressure oxidation of metals—Tungsten in oxygen10.1149/1.2430309 ↗
22. The formation of porous oxides on metals. II. Tungsten and the paralinear rate law10.1149/1.2427925 ↗
23. V.Y. Ivanov, Y.P. Nechiporenko, L.N. Yefimenko, M.I. Yurchenko, High temperature oxidation protection of tungsten, NASA Tecnichal Traslations, NASA TT F-583, 1969, Translation from “Atom” Press, 1968.
24. Cracking failure study of ITER-reference tungsten grade under single pulse thermal shock loads at elevated temperatures10.1016/j.jnucmat.2009.01.313 ↗
25. The oxidation kinetics of tungsten and the determination of oxygen diffusion coefficient in tungsten trioxide10.1016/0010-938X(80)90092-X ↗
26. An electron diffraction study of oxide films formed on molybdenum tungsten, and alloys of molybdenum, tungsten and nickel
27. Formation and incorporation of dopant phases during technical reduction of NS-doped tungsten blue oxide10.1016/0263-4368(95)00006-2 ↗
28. The effect of niobium on the oxidation behavior of titanium in N2/20% O2 atmospheres10.1016/S0921-5093(00)00754-1 ↗
29. On the influence of water vapour on the oxidation behavior of pure Ti10.1016/j.corsci.2006.06.030 ↗
30. Surface electrical properties of tungsten oxides in equilibrium with the gas phase10.1007/BF00603671 ↗