journal article·2009-12

Corrosion of stainless steel 316L in simulated formation water environment with CO2–H2S–Cl−

W. He, O.Ø. Knudsen, S. Diplas

Corrosion Science· Volume 51· Issue 12
Publisher page

Abstract

Abstract A synergistic effect of high concentration of chloride and H 2 S on oxide formation and metal dissolution has been studied on 316L stainless steel by electrochemical measurements, inductive coupled plasma (ICP) and X-ray photoelectron spectroscopy (XPS). Chloride concentration had a significant effect on semiconductor properties of the oxide film, while the gases had little effect. A relatively high concentration of sulphur was found inside the oxide formed in a high chloride concentration electrolyte with high H 2 S compared to the oxide formed in low concentrations, which indicates that sulphur entered the oxide film through local weakening of the oxide by the chloride.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Recent progress in tubular products for oil and gas production
2. Studies on the stress corrosion cracking behavior of some alloys used in desalination plants10.1016/S0011-9164(99)00079-X ↗
3. H. Hoffmeister, Modeling of H2S corrosion by coupling of phase and polarization behaviour, Corrosion, NACE International Corrosion Conference & Expo, 2005, Paper 05476.
4. A theory for breakdown of anodic oxide films on metals10.1016/0013-4686(71)85079-X ↗
5. Pitting potentials and inhibition potentials of iron and nickel for different aggressive and inhibiting anions10.1016/0010-938X(77)90002-6 ↗
6. A point defect model for anodic passive films10.1149/1.2127592 ↗
7. The relationships between anodic passivity, brightening and pitting10.1016/S0010-938X(65)90614-1 ↗
8. Pit Initiation at single sulfide inclusions in stainless steel III. Mathematical model10.1149/1.1474432 ↗
9. Pitting corrosion of metals – a review of the critical factors10.1149/1.1838615 ↗
10. Sulfur-assisted corrosion mechanisms and the role of alloyed elements
11. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗
12. Pitting mechanism on an austenite stainless steel nanocrystalline coating investigated by electrochemical noise and in-situ AFM analysis10.1016/j.electacta.2008.06.076 ↗
13. Surface science approach of corrosion phenomena10.1016/S0013-4686(97)00239-9 ↗
14. Effect of CO2 and H2S on the composition and stability of passive film on iron alloys in geothermal water10.1016/j.electacta.2007.01.086 ↗
15. The Effect of CO2 and H2S on the passivation of chromium and stainless steels in aqueous solutions at elevated temperature and under high pressure
16. G.Ø. Lauvstad, R. Johnsen, Ø. Borck, E. Falck da Silva and J. Walmsley, Breakdown in passivity of austenitic stainless steels in Cl− and H2S – Modelling and characterization of the pit initiation process, NACE International Corrosion Conference & Expo, 2007, Paper 07660.
17. Influence of an elastic stress on the conductivity of passive films10.1016/S0921-5093(00)01843-8 ↗
18. Analogy between the effects of a mechanical and chemical perturbation on the conductivity of passive films10.1016/S0010-938X(01)00162-7 ↗
19. Influence of the Chemical Composition and Electronic Structure of Passive Films Grown on 316L SS on Their Transient Electrochemical Behavior10.1149/1.1803562 ↗
20. Influence of the temperature of film formation on the electronic structure of oxide films formed on 304 stainless steel10.1016/S0013-4686(01)00658-2 ↗
21. Electrochemical behavior of metallic materials used in seawater-interactions between glucose oxidase and passive layers10.1016/S0013-4686(03)00023-9 ↗
22. Effect of the final annealing of cold rolled stainless steels sheets on the electronic properties and pit nucleation resistance of passive films10.1016/j.corsci.2007.08.013 ↗
23. Semiconducting properties of passive films on AISI 304 and 316 stainless steels10.1016/0022-0728(93)80435-K ↗
24. In situ study on the effects of Ni and Mo on the passive film formed on Fe-20Cr alloys by photoelectrochemical and Mott–Schottky techniques10.1016/j.jelechem.2006.02.031 ↗
25. Role of Chloride Ion in Passivity Breakdown on Iron and Nickel10.1149/1.2048247 ↗
26. The electronic structure of passive films formed on stainless steels10.1016/0010-938X(95)00084-W ↗
27. Passivation model of 316 stainless steel in simulated cooling water and the effect of sulfide on the passive film10.1016/S0169-4332(03)00355-6 ↗
28. A co-ordinated study of the passivation of alloy steels by plasma source mass spectrometry and X-ray photoelectron spectroscopy-1. Characterization of the passive film, Corrosion
29. The role of molybdenum in the dissolution and the passivation of stainless steels with adsorbed sulphur10.1016/0010-938X(92)90150-2 ↗
30. AES sputter depth profiling of thin aluminium oxide
31. Ultrathin SiO2 on Si. VI. Evaluation of uncertainties in thickness measurement using XPS10.1002/sia.2020 ↗
32. Powell · 2000
33. Electrochemical passivation of iron alloys and the film characterisation by XPS10.1016/S0010-938X(00)00028-7 ↗
34. Esca-studies of the composition profile of low temperature oxide formed on chromium steels-I. Oxydation in dry oxygen10.1016/0010-938X(75)90033-5 ↗
35. Semiconducting properties of thermally grown oxide films on AISI 304 stainless steel10.1016/S0010-938X(99)00082-7 ↗
36. Angle-resolved XPS and AES: depth-resolution limits and a general comparison of properties of depth-profile reconstruction methods10.1016/0368-2048(94)02270-4 ↗