Hydrogen transport and embrittlement in 300M and AerMet100 ultra high strength steels
Source abstract
Abstract
Abstract This paper describes how hydrogen transport affects the severity of hydrogen embrittlement in 300 M and AerMet100 ultra high strength steels. Slow strain rate tests were carried out on specimens coated with electrodeposited cadmium and aluminium-based SermeTel 1140/962. Hydrogen diffusivities were measured using two-cell permeation and galvanostatic charging methods and values of 8.0 × 10−8 and 1.0 × 10−9 cm2 s−1 were obtained for 300 M and AerMet100, respectively. A two-dimensional diffusion model was used to predict the hydrogen distributions in the SSR specimens at the time of failure. The superior embrittlement resistance of AerMet100 was attributed to reverted austenite forming around martensite laths during tempering.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Defence Standard 03-4/2, ‘The pre-treatment and protection of steel parts of specified maximum tensile strength exceeding 1450Nmm−2, 1977.
2. The use of SIMS in quality control and failure analysis of electrodeposited items inspected for hydrogen effects10.1016/j.corsci.2008.01.016 ↗
3. Hydrogen re-embrittlement of high strength steel by corrosion of cadmium and aluminium based sacrificial coatings10.1179/174327805X29822 ↗
4. The effects of sacrificial coatings on hydrogen embrittlement and re-embrittlement of ultra high strength steels10.1016/j.corsci.2007.11.023 ↗
5. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
6. The effect of grain size and aging on hydrogen embrittlement of a maraging steel10.1016/j.corsci.2008.06.044 ↗
7. Correlation of microstructure with mechanical properties of 300M steel10.1007/BF02642857 ↗
8. Microstructural analysis of a multistage heat-treated ultra-high strength low alloy steel10.1016/0025-5416(84)90175-7 ↗
9. Hydrogen trapping in high strength steels10.1016/S1359-6454(98)00247-X ↗
10. M2C precipitates in isothermal tempering of high Co–Ni secondary hardening steel10.1007/BF02595438 ↗
11. Transmission electron microscopy examination of hardening and toughening phenomena in AerMet10010.1007/BF02666329 ↗
12. Stress corrosion cracking behaviour of 300M steel under different heat treatment conditions10.5006/1.3583005 ↗
13. The absorption and diffusion of electrolytic hydrogen in palladium10.1098/rspa.1962.0205 ↗
14. Use of electrochemical methods to determine chemical-diffusion coefficients in alloys: application to LiAl
15. Hydrogen diffusivity in AerMet100 at room temperature under galvanostatic charging conditions10.1016/S0925-8388(03)00332-3 ↗
16. Determination of the diffusion coefficient of hydrogen in gamma titanium aluminides during electrolytic charging10.1016/S1359-6454(99)00431-0 ↗
17. Generalised chronopotentiometric potential-time equations and their application to quasi-reversible processes10.1021/ac60222a003 ↗
18. The effect of post-exposure heat treatment on the hydrogen embrittlement of high strength steel10.5006/1.3582987 ↗
19. T. Yokobori, in: P. Noordhoff (Ed.), Strength Fracture and Fatigue of Materials, Groningen, 1965, pp. 22–28.
20. Hydrogen embrittlement of high strength steel electroplated with zinc–cobalt alloys10.1016/S0010-938X(03)00180-X ↗
21. Chatfield · 1983
22. A new model for hydrogen assisted cracking (hydrogen embrittlement)10.1007/BF02642048 ↗
23. Hydrogen embrittlement of cathodically protected high strength, low alloy steels exposed to sulphate-reducing bacteria10.5006/1.3293536 ↗
24. R.P. Gangloff, A review and analysis of the threshold for hydrogen environment embrittlement of steel, in Corrosion Prevention and Control, in: M. Levy, S. Isserow (Eds.), US Army Sagamore Materials Research Conference, vol. 33, Watertown, MA, US Laboratory Command, 1986, p. 64.
25. A study of the entry and removal of hydrogen during coating and thermal treatment of steel10.5006/1.3593844 ↗
26. Measurement and prediction of hydrogen embrittlement in high strength carbon steel10.1179/174327808X303491 ↗
27. The role of metallurgical variables in hydrogen-assisted environmental fracture
28. A new model for hydrogen-assisted cracking (hydrogen embrittlement)
29. Crank · 1975
30. Carslaw · 1959
31. The effect of silicon additions and retained austenite on stress corrosion cracking in ultra high strength steels10.1007/BF02647168 ↗
32. Trap-governed hydrogen diffusivity and uptake capacity in ultra high-strength AerMet® 100 steel10.1007/s11661-002-0032-6 ↗
33. Internal hydrogen embrittlement of ultrahigh-strength AerMet® 100 steel10.1007/s11661-003-0334-3 ↗
34. M.J. Robinson, P.J. Kilgallon, M. Newman, Hydrogen embrittlement of cathodically protected duplex stainless steels in seawater containing sulphides, in: Proceedings 15th International Conference on Offshore Mechanics & Arctic Engineering, Florence, Italy, June 16–20, 1996.
35. Hydrogen transport in a duplex stainless steel10.1016/S1359-6454(00)00122-1 ↗
36. Transmission electron microscopy examination of hardening and toughening phenomena in AerMet100