journal article·2019-08

Effects of laser glazing on CMAS corrosion behavior of Y2O3 stabilized ZrO2 thermal barrier coatings

Zheng Yan, Lei Guo, Zhihua Li, Yang Yu, Quanjun He

Corrosion Science· Volume 157
Publisher page

Abstract

Abstract Calcium-magnesium-alumina-silicate (CMAS) is a serious threat to thermal barrier coatings (TBCs). The goal of this study is to tailor YSZ coating microstructures by laser for alleviating CMAS attack. A smooth laser glazed layer with a columnar microstructure and some open channels is produced on the coating surface. Under molten CMAS conditions, the glazed layer remains phase stability and has little evidence of dissolution. Exposed to thermal shock tests with CMAS deposits, the glazed layer keeps structural integrity. However, the open channels also act as the paths for CMAS penetration, which brings destructive damages to the coating beneath the glazed layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Thermal-barrier coatings for more efficient gas-turbine engines10.1557/mrs.2012.232 ↗
2. Overview on advanced thermal barrier coatings10.1016/j.surfcoat.2010.08.151 ↗
3. Thermal barrier coating materials10.1016/S1369-7021(05)70934-2 ↗
4. The influence of oxides on the performance of advanced gas turbines10.1016/j.jeurceramsoc.2007.12.023 ↗
5. Processing science of advanced thermal-barrier systems10.1557/mrs.2012.233 ↗
6. Investigation on hot-fatigue behaviors of gradient thermal barrier coatings by EB-PVD10.1016/S0257-8972(01)01347-0 ↗
7. Thermodynamic conditions for cluster formation in supersaturated boundary layer during plasma spray-physical vapor deposition10.1016/j.apsusc.2018.12.070 ↗
8. Gaseous material capacity of open plasma jet in plasma spray-physical vapor deposition process10.1016/j.apsusc.2017.09.218 ↗
9. Jet engine coatings for resisting volcanic ash damage10.1002/adma.201004783 ↗
10. Environmental degradation of thermal-barrier coatings by molten deposits10.1557/mrs.2012.230 ↗
11. Ti2AlC MAX phase for resistance against CMAS attack to thermal barrier coatings10.1016/j.ceramint.2019.01.059 ↗
12. Mechanism of crack nucleation and growth in YSZ thermal barrier coatings corroded by CMAS at high temperatures: first-principles calculation10.1016/j.corsci.2018.07.033 ↗
13. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
14. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
15. Calcia-magnesia-alumino-silicate (CMAS)-induced degradation and failure of air plasma sprayed yttria-stabilized zirconia thermal barrier coatings10.1016/j.actamat.2015.12.044 ↗
16. Zirconium silicate growth induced by the thermochemical interaction of yttria-stablized zirconia coatings with molten CMAS deposits10.1016/j.corsci.2019.01.011 ↗
17. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
18. A delamination mechanism for thermal barrier coatings subject to calcium-magnesium-alumino-silicate (CMAS) infiltration10.1016/j.actamat.2004.11.028 ↗
19. Microstructure and thermo-physical properties of yttria stabilized zirconia coatings with CMAS deposits10.1016/j.jeurceramsoc.2011.04.006 ↗
20. Calcium-magnesium-alumina-silicate (CMAS) resistance property of BaLn2Ti3O10 (Ln=La, Nd) for thermal barrier coating applications10.1016/j.ceramint.2017.05.107 ↗
21. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
22. Hot corrosion behavior of La2(Zr0.7Ce0.3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium aluminosilicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
23. La2(Zr0.7Ce0.3)2O7 thermal barrier coating prepared by electron beam-physical vapor deposition that are resistant to high temperature attack by molten silicate10.1016/j.corsci.2016.11.015 ↗
24. Calcium-magnesium-alumina-silicate (CMAS) resistance characteristics of LnPO4 (Ln=Nd, Sm, Gd) thermal barrier oxides10.1016/j.jeurceramsoc.2016.08.013 ↗
25. Plasma sprayed nanostructured GdPO4 thermal barrier coatings: preparation microstructure and CMAS corrosion resistance10.1111/jace.14924 ↗
26. Air-plasma-sprayed thermal barrier coatings that are resistant to high-temperature attack by glassy deposits10.1016/j.actamat.2010.09.013 ↗
27. Composition-microstructure- mechanical property relationships and toughening mechanisms of GdPO4-doped Gd2Zr2O7 composites10.1016/j.compositesb.2018.12.135 ↗
28. High temperature wettability between CMAS and YSZ coating with tailored surface microstructures10.1016/j.matlet.2018.06.066 ↗
29. Laser surface modification of plasma sprayed CYSZ thermal barrier coatings10.1016/j.ceramint.2012.09.005 ↗
30. Surface laser-glazing of plasma-sprayed thermal barrier coatings10.1016/j.apsusc.2005.01.047 ↗
31. Microstructural evaluation of laser remelted gadolinium zirconate thermal barrier coatings10.1016/j.surfcoat.2015.06.074 ↗
32. Improving the erosion resistance of plasma-sprayed zirconia thermal barrier coatings by laser glazing10.1016/j.surfcoat.2007.07.005 ↗
33. Microstructure and thermal cyclic performance of laser-glazed plasma-sprayed ceria–yttria–stabilized zirconia thermal barrier coatings10.1016/j.surfcoat.2008.06.118 ↗
34. Improving the thermal shock resistance of plasma sprayed CYSZ thermal barrier coatings by laser surface modification10.1016/j.optlaseng.2011.12.007 ↗
35. The influence of laser treatment on thermal shock resistance of plasma-sprayed nanostructured yttria stabilized zirconia thermal barrier coatings10.1016/j.ceramint.2013.06.008 ↗
36. Improving the hot corrosion resistance of plasma sprayed ceria–yttria stabilized zirconia thermal barrier coatings by laser surface treatment10.1016/j.matdes.2013.12.075 ↗
37. Evaluation of laser-glazed plasma-sprayed thermal barrier coatings under high temperature exposure to molten salts10.1016/j.surfcoat.2005.10.011 ↗
38. The role of the surface morphology and segmented cracks on the damage forms of laser re-melted thermal barrier coatings in presence of a molten salt (Na2SO4 + V2O5)10.1016/j.corsci.2016.11.011 ↗
39. The influence of laser treatment on hot corrosion behavior of plasma-sprayed nanostructured yttria stabilized zirconia thermal barrier coatings10.1016/j.jeurceramsoc.2014.01.031 ↗
40. Effects of laser surface remelting on the molten salt corrosion resistance of yttria-stabilized zirconia coatings10.1016/j.ceramint.2018.09.041 ↗
41. Phase stability and thermal conductivity of RE2O3 (RE=La, Nd, Gd, Yb) and Yb2O3 co-doped Y2O3 stabilized ZrO2 ceramics10.1016/j.ceramint.2016.01.138 ↗
42. Preparation and hot corrosion behavior of plasma sprayed nanostructured Gd2Zr2O7-LaPO4 thermal barrier coatings10.1016/j.jallcom.2016.12.241 ↗
43. Wetting, infiltration and interaction behavior of CMAS towards columnar YSZ coatings deposited by plasma spray physical vapor10.1016/j.jeurceramsoc.2018.04.013 ↗
44. Surface tension, wettability and reactivity of molten titanium in Ti/yttria-stabilized zirconia system10.1016/S0921-5093(01)01732-4 ↗
45. Defects/CMAS corrosion resistance relationship in plasma sprayed YPSZ coating10.1016/j.jallcom.2016.10.074 ↗
46. Influence of preheating processes on the microstructure of laser glazed YSZ coatings10.1016/j.ceramint.2016.12.125 ↗
47. Influence of laser glazing on the characterization of plasma-sprayed YSZ coatings10.1007/s11666-016-0481-x ↗