journal article·2021-07

Corrosion behavior of AZ91 Mg alloy with a heterogeneous structure produced by ECAP

Zhenquan Yang, Aibin Ma, Bingqian Xu, Jinghua Jiang, Jiapeng Sun

Corrosion Science· Volume 187
Publisher page

Abstract

Abstract The microstructure of a commercial AZ91 Mg alloy was modified via equal channel angular pressing (ECAP) and subsequent aging. Immersion corrosion testing in 3.5 wt.% NaCl solution indicated that the ECAP alloy with heterogeneous grain structure had the best corrosion performance, which mainly stemmed from that the galvanic effect was weakened due to the reduced fraction and modified distribution of β phase particles. An aging treatment consisting of 60–90 h at 150 ℃ produced fine β phase precipitates which enhanced the micro-galvanic effect, such that the corrosion rates increased but were still lower than that of the as-cast alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (94)

Show source-provided references
1. Fundamentals and advances in magnesium alloy corrosion10.1016/j.pmatsci.2017.04.011 ↗
2. Weight loss with magnesium alloys10.1126/science.1182848 ↗
3. On the ductility of magnesium based materials: a mini review10.1016/j.jallcom.2019.04.031 ↗
4. What is going on in magnesium alloys?10.1016/j.jmst.2017.07.019 ↗
5. High strength Mg-9Al serial alloy processed by slow extrusion10.1016/j.msea.2017.05.017 ↗
6. Fabrication of ultra-high strength magnesium alloys over 540 MPa with low alloying concentration by double continuously extrusion10.1016/j.jma.2018.04.003 ↗
7. Development of high-strength magnesium alloys via combined processes of extrusion, rolling and ageing10.1016/j.scriptamat.2011.01.042 ↗
8. Structural evolutions of metallic materials processed by severe plastic deformation10.1016/j.mser.2018.06.001 ↗
9. Enhanced quasi-isotropic ductility in bi-textured AZ91 Mg alloy processed by up-scaled RD-ECAP processing10.1016/j.jallcom.2018.12.008 ↗
10. Developing an industrial-scale ECAP Mg-Al-Zn alloy with multiheterostructure for synchronously high strength and good ductility10.1016/j.matchar.2020.110341 ↗
11. Effect of route on tensile anisotropy in equal channel angular pressing10.1016/j.msea.2016.08.108 ↗
12. Equal-channel angular pressing of magnesium alloy AZ91 and its effects on microstructure and mechanical properties10.1016/j.msea.2006.10.199 ↗
13. The grain size and texture dependence of tensile properties in extruded Mg-9Al-1Zn10.2320/matertrans.42.1182 ↗
14. Microstructure and mechanical behavior of AZ91 Mg alloy processed by equal channel angular pressing10.1016/j.jallcom.2004.10.050 ↗
15. Microstructure and anisotropic mechanical behavior of the high-strength and ductility AZ91 Mg alloy processed by hot extrusion and multi-pass RD-ECAP10.1016/j.msea.2020.139191 ↗
16. Mechanical properties and precipitate behavior of Mg–9Al–1Zn alloy processed by equal-channel angular pressing and aging10.1016/j.jallcom.2014.01.140 ↗
17. Managing strength and ductility in AZ91 magnesium alloy through ECAP combined with prior and post aging treatment10.1016/j.matchar.2019.04.022 ↗
18. Effect of ECAP die angles on microstructure mechanical properties and corrosion behavior of AZ80 Mg alloy10.1007/s11665-019-04080-5 ↗
19. Corrosion of hot extrusion AZ91 magnesium alloy: I-relation between the microstructure and corrosion behavior10.1016/j.corsci.2011.02.015 ↗
20. Corrosion behaviour of bulk ultra-fine grained AZ91D magnesium alloy fabricated by equal-channel angular pressing10.1016/j.corsci.2010.09.044 ↗
21. Enhanced corrosion resistance of Mg alloy ZK60 after processing by integrated extrusion and equal channel angular pressing10.1016/j.actamat.2011.06.033 ↗
22. Effect of ECAP processing on corrosion resistance of AE21 and AE42 magnesium alloys10.1016/j.apsusc.2012.12.096 ↗
23. Influence of aging prior to extrusion on the microstructure and corrosion resistance of Mg–8Sn–2Zn–0.2Mn alloy10.1016/j.jallcom.2018.11.400 ↗
24. Effect of extrusion on corrosion properties of Mg-2Ca-χAl (χ = 0, 2, 3, 5) alloys10.1016/j.corsci.2017.08.014 ↗
25. Enhanced corrosion resistance of AZ91 magnesium alloy through refinement and homogenization of surface microstructure by friction stir processing10.1016/j.corsci.2018.04.028 ↗
26. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
27. Formation and characteristic corrosion behavior of alternately lamellar arranged α and β in as-cast AZ91 Mg alloy10.1016/j.jallcom.2018.08.103 ↗
28. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
29. Corrosion behavior of ECAP-Processed AM90 magnesium alloy10.1007/s13369-018-3203-5 ↗
30. Effect of grain refinement on material properties of Mg-8%Al-0.5%Zn alloy after the combined processes of multi-direction forging and equal channel angular pressing10.1088/2053-1591/ab2ddf ↗
31. Effect of annealing and aging treatment on pitting corrosion resistance of fine-grained Mg-8%Al-0.5%Zn alloy
32. Volta potential of second phase particles in extruded AZ80 magnesium alloy10.1016/j.electacta.2005.10.010 ↗
33. Phase analysis of Al-Mn compounds in the AZ magnesium alloys10.4028/www.scientific.net/MSF.546-549.395 ↗
34. Study of β-precipitates and their effect on the directional yield asymmetry of friction stir processed and aged AZ91C alloy10.1016/j.msea.2012.09.095 ↗
35. Heterogeneous materials: a new class of materials with unprecedented mechanical properties10.1080/21663831.2017.1343208 ↗
36. Perspective on hetero-deformation induced (HDI) hardening and back stress10.1080/21663831.2019.1616331 ↗
37. Heterostructured materials: superior properties from hetero-zone interaction10.1080/21663831.2020.1796836 ↗
38. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
39. Microstructure evolution and mechanical behavior of a binary Al–7Mg alloy processed by equal-channel angular pressing10.1016/j.actamat.2014.10.025 ↗
40. An initial analysis of mechanisms leading to late stage abnormal grain growth in nanocrystalline Ni10.1016/S1359-6462(02)00098-2 ↗
41. High strength and ductility in multimodal-structured Zr10.1016/j.matdes.2011.08.002 ↗
42. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
43. Ultrastrong low-carbon nanosteel produced by heterostructure and interstitial mediated warm rolling10.1126/sciadv.aba8169 ↗
44. Achieving high strength and high ductility in magnesium alloy using hard-plate rolling (HPR) process10.1038/srep17100 ↗
45. Deformation behavior of ultra-strong and ductile Mg-Gd-Y-Zn-Zr alloy with bimodal microstructure10.1007/s11661-018-4507-5 ↗
46. The synergy effect of fine and coarse grains on enhanced ductility of bimodal-structured Mg alloys10.1016/j.jallcom.2018.11.229 ↗
47. Achieving ultra-high strength in Mg–Gd–Ag–Zr wrought alloy via bimodal-grained structure and enhanced precipitation10.1016/j.jmst.2020.04.031 ↗
48. Bimodal microstructure - A feasible strategy for high-strength and ductile metallic materials10.1016/j.jmst.2017.11.018 ↗
49. Multimodal microstructure and mechanical properties of AZ91 Mg alloy prepared by equal channel angular pressing plus aging10.3390/met8100763 ↗
50. Improving mechanical properties of heterogeneous Mg-Gd alloy laminate via accumulated extrusion bonding10.1016/j.msea.2020.139324 ↗
51. High strength and ductility AZ91 magnesium alloy with multi-heterogenous microstructures prepared by high-temperature ECAP and short-time aging10.1016/j.msea.2018.07.075 ↗
52. Inhomogeneous evolution of microstructure in AZ91 Mg-alloy during high temperature equal-channel angular pressing10.1016/j.jallcom.2009.11.150 ↗
53. Correlation of plastic deformation and dynamic recrystallization in magnesium alloy ZK6010.1016/S1359-6454(01)00020-9 ↗
54. Characteristics of plastic deformation by rotary-die equal-channel angular pressing10.1016/j.scriptamat.2004.11.014 ↗
55. A corrosion study of the main constituent phases of AZ91 magnesium alloys10.1016/S0010-938X(03)00109-4 ↗
56. Influence of microstructure and composition on the corrosion behaviour of Mg/Al alloys in chloride media10.1016/j.electacta.2008.06.001 ↗
57. Discontinuous and continuous precipitation in magnesium–aluminium type alloys10.1016/j.jallcom.2008.11.008 ↗
58. Effects of dynamic recrystallization and strain-induced dynamic precipitation on the corrosion behavior of partially recrystallized Mg–9Al–1Zn alloys10.1016/j.jma.2020.09.005 ↗
59. Enhanced mechanical properties and corrosion resistance of a fine-grained Mg-9Al-1Zn alloy: the role of bimodal grain structure and β-Mg17Al12 precipitates10.1016/j.mtla.2020.100840 ↗
60. Corrosion morphologies on magnesium alloy AZ 9110.1002/maco.19940450603 ↗
61. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
62. The corrosion of Al-supersaturated Mg matrix and the galvanic effect of secondary phase nanoparticles10.1016/j.corsci.2021.109410 ↗
63. Advances in Mg corrosion and research suggestions10.1016/j.jma.2013.09.003 ↗
64. The influence of yttrium (Y) on the corrosion of Mg–Y binary alloys10.1016/j.corsci.2010.07.019 ↗
65. Effect of heat treatment on corrosion behavior of AZ63 magnesium alloy in 3.5 wt.% sodium chloride solution10.1016/j.corsci.2016.05.019 ↗
66. Improvement of corrosion resistance and biocompatibility of rare-earth WE43 magnesium alloy by neodymium self-ion implantation10.1016/j.corsci.2015.01.049 ↗
67. Effect of chloride ion concentration on electrochemical behavior and corrosion product of AM60 magnesium alloy in aqueous solutions10.5006/0010-9312-68-4-2 ↗
68. AC impedance spectroscopy in characterizing time-dependent corrosion of AZ91 and AM50 magnesium alloys characterization with respect to their microstructures10.1149/1.1415722 ↗
69. Investigation of magnesium corrosion in aerated sodium sulfate solution by electrochemical impedance spectroscopy10.1016/0013-4686(90)87043-2 ↗
70. CPE analysis by local electrochemical impedance spectroscopy10.1016/j.electacta.2005.02.128 ↗
71. On the electrical capacitance of interfaces exhibiting constant phase element behaviour
72. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
73. Electrochemical impedance spectroscopy study of thermally grown oxides exhibiting constant phase element behaviour10.1016/j.electacta.2013.09.054 ↗
74. On the corrosion mechanism of Mg investigated by electrochemical impedance spectroscopy10.1016/j.electacta.2019.03.080 ↗
75. Correlation between electrochemical impedance measurements and corrosion rate of magnesium investigated by real-time hydrogen measurement and optical imaging10.1016/j.electacta.2015.03.050 ↗
76. The surface, microstructure and corrosion of magnesium alloy AZ31 sheet10.1016/j.electacta.2010.02.068 ↗
77. Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution10.1016/j.corsci.2009.10.004 ↗
78. Enhanced corrosion resistance of ultrafine-grained AZ61 alloy containing very fine particles of Mg17Al12 phase10.1016/j.corsci.2013.05.032 ↗
79. Corrosion behavior of fine-grained AZ31B magnesium alloy10.1016/j.corsci.2012.04.039 ↗
80. The relation between microstructure and corrosion behavior of AZ80 Mg alloy following different extrusion temperatures10.1016/j.corsci.2008.03.003 ↗
81. The influence of microstructure on the corrosion behaviour of AZ91D studied by scanning Kelvin probe force microscopy and scanning Kelvin probe10.1016/j.corsci.2005.05.008 ↗
82. Corrosion resistance of aged die cast magnesium alloy AZ91D10.1016/j.msea.2003.08.060 ↗
83. Effects of the second phases on corrosion resistance of AZ91-xGd alloys treated with ultrasonic vibration10.1016/j.jallcom.2019.01.002 ↗
84. Effectiveness of Ti-micro alloying in relation to cooling rate on corrosion of AZ91 Mg alloy10.1016/j.jallcom.2016.02.043 ↗
85. Influence of trace As content on the microstructure and corrosion behavior of the AZ91 alloy in different metallurgical conditions10.1016/j.jma.2019.12.004 ↗
86. Corrosion behavior of electron beam processed AZ91 magnesium alloy10.1016/j.jma.2020.08.012 ↗
87. Effect of SiC particulates on the corrosion behavior of extruded AZ91/SiCp composites during the early stage of exposure10.1149/2.0631514jes ↗
88. Effect of samarium on the microstructure and corrosion resistance of AZ91 magnesium alloy treated by ultrasonic vibration10.3390/ma11112331 ↗
89. Effects of combined addition of Ca and Y on the corrosion behaviours of die-cast AZ91D magnesium alloy10.1016/j.corsci.2020.108451 ↗
90. To study the corrosion behavior of friction stir processed magnesium alloy AZ91
91. Corrosion behaviour of magnesium/aluminium alloys in 3.5wt.% NaCl10.1016/j.corsci.2007.11.005 ↗
92. XPS study of the surface chemistry on AZ31 and AZ91 magnesium alloys in dilute NaCl solution10.1016/j.apsusc.2010.02.058 ↗
93. Electrochemical corrosion behavior of biodegradable Mg-Y-RE and Mg-Zn-Zr alloys in Ringer’s solution and simulated body fluid10.1016/j.corsci.2014.11.015 ↗
94. Characterization and corrosion behavior of plasma electrolytic oxidation coated AZ91-T6 magnesium alloy10.1016/j.surfcoat.2016.07.021 ↗