Oxidation of alloys for energy applications in supercritical CO2 and H2O
Source abstract
Abstract
Abstract To facilitate development of supercritical CO 2 (sCO 2 ) power plants, a comparison of the oxidation behavior of austenitic stainless steels and Ni-base alloys in sH 2 O and sCO 2 were made. Experiments were conducted at 730 °C/207 bar (sCO 2 ) and 726 °C/208 bar (sH 2 O). Ni-base alloys in sCO 2 did not exhibit much change with pressure. Ni-base alloys in sH 2 O had an increase in corrosion rate and the log of the parabolic rate constant was proportional to pressure. Fine-grain austenitic stainless steels in sCO 2 and sH 2 O were both less protective with pressure as the dense protective chromia scale was replaced with faster growing Fe-oxide rich scales.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. U.S. DOE R&D program on supercritical CO2 power cycles
2. Allam · 2013
3. Supercritical CO2 cycle development at pratt & whitney rocketdyne
4. A critical look at supercritical power plants
5. U.S. Department of Energy and Ohio Coal Development Office Advanced Ultra-Supercritical Materials Project for Boilers and Steam Turbines—Summary of Results, EPRI 1022770, Palo Alto, CA, 2011, pp. 24.
6. Steam oxidation and fireside corrosion testing of several advanced alloys in a steam loop at A-USC design temperatures
7. High pressure steam oxidation of alloys for advanced ultra-Supercritical conditions10.1007/s11085-014-9491-6 ↗
8. I.G. Wright, P.F., Tortorelli, M. Schütze, Program on Technology Innovation: Oxide Growth and Exfoliation on Alloys Exposed to Steam, EPRI 1013666, Palo Alto, CA, 2007.
9. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
10. H.E. McCoy, B. McNabb, Corrosion of Several Metals in Supercritical Steam at 538 (C, Oak Ridge National Laboratory ORNL/TM-5781, Oak Ridge, TN, 1977, pp. 51.
11. Oxidation of 316 stainless steel in supercritical water10.1016/j.corsci.2009.03.008 ↗
12. J.C. Griess, W.A. Maxwell, The long-Term Oxidation of Selected Alloys in Superheated Steam at 482 and 538 (C, Oak Ridge National Laboratory ORNL-5771, Oak Ridge, TN, 1981, pp. 46.10.2172/6464269 ↗
13. Corrosion behavior of steels and nickel alloys in superheated steam10.5006/0010-9312-22.5.147 ↗
14. High temperature corrosion behaviour of some boiler steels in pure water vapour10.4028/www.scientific.net/MSF.369-372.239 ↗
15. Steam oxidation of fine-Grain steels
16. Sarver · 2009
17. Steam oxidation of martensitic steels and of Ni-Base alloys: comparison of lab tests with operating power plants10.1007/s11085-014-9480-9 ↗
18. Compatibility of FBR structural materials with supercritical carbon dioxide10.1016/j.pnucene.2011.04.030 ↗
19. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
20. The effect of temperature on the sCO2 compatibility of conventional structural alloys
21. Corrosion of materials in supercritical carbon dioxide environments
22. Alloys SS316 and hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
23. An exploration of the effect of temperature on different alloys in a supercritical carbon dioxide environment
24. Comparison of the corrosion behaviors of Fe-base and Ni-base austenitic alloys in high temperature S-CO2 environment
25. Compatibility of candidate structural materials in high-temperature S-SO2 environment
26. Corrosion of a stainless steel and nickel-based alloys in high temperature supercritical carbon dioxide environment10.1016/j.corsci.2012.11.041 ↗
27. Corrosion of supercritical CO2 turbomachinary components
28. Corrosion of nickel-Base alloys
29. Corrosion and carburization behavior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment10.1016/j.corsci.2015.07.007 ↗
30. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
31. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
32. Kinetics of Breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
33. Water vapour effects on corrosion of Fe–Cr and Fe–Cr–Ni alloys containing cerium and manganese in CO2 gas at 818°C10.1016/j.corsci.2014.08.029 ↗
34. Calculations of parabolic reaction rate constants10.1007/BF00667057 ↗
35. Cast alloys for advanced ultra supercritical steam turbines
36. Some factors in the oxidation of austenitic stainless steel
37. Oxidation of 18%Cr, 8%Ni steels in CO2
38. Factors in the oxidation assessment of AISI type 310 steels in high pressure carbon dioxide10.1016/0010-938X(82)90129-9 ↗
39. Oxidation of boiler tubing
40. The effect of water vapor on selective oxidation of Fe–Cr alloys10.1007/s11085-007-9090-x ↗
41. Oxygen permeability measurements in ni using H2/H2O, CO/CO2 and Ni/NiO rhines pack atmospheres10.1007/s11085-014-9511-6 ↗
42. Quantitative approach for determining the critical volume fraction for the transition from internal to external oxidation10.1007/s11085-014-9516-1 ↗
43. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873K in the presence of 10% water vapor10.1023/A:1018875024306 ↗
44. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation10.1023/A:1004642310974 ↗
45. Dual environment effects on the oxidation of metallic interconnects10.1361/105994906X117198 ↗
46. Diffusion of hydrogen in metals