Abstract Pitting corrosion resistance and mechanical properties of 2304 duplex stainless steel with different Creq/Nieq values after plasma-arc welding and welding thermal simulation were systematically studied. The results showed that the lower the Creq/Nieq value in the experimental range, the better the microstructure after welding or welding thermal cycle. High pitting resistance equivalent number in the chemical composition brought in low weight loss rate and high critical pitting temperature for base metal. Furthermore, as the Creq/Nieq value decreased, the degradation of pitting corrosion resistance after welding thermal cycle reduced.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. J. Charles, Super duplex stainless steels: structure and properties, in: Proc. Conference “Duplex Stainless Steels’91”, vol. 2, Beaune, France, 1991, pp. 3–48.
2. Super duplex stainless steel10.1179/mst.1992.8.8.685 ↗
3. Mechanical properties, microstructure stability and kinetics of σ-phase formation in 29Cr–6Ni–2Mo–0.38N superduplex stainless steel10.1007/s11661-000-0050-1 ↗
4. Effect of thermal cycles on the corrosion and mechanical properties of UNS S31803 duplex stainless steel10.1016/j.corsci.2009.08.015 ↗
5. Evaluation of localized corrosion in duplex stainless steel aged at 850°C with critical pitting temperature measurement10.1016/j.electacta.2008.11.038 ↗
6. Formation of an aluminum-alloyed coating on AZ91D magnesium alloy in molten salts at lower temperature10.1016/j.surfcoat.2010.09.034 ↗
7. Effects of solution heat-treatment and nitrogen in shielding gas on the resistance to pitting corrosion of hyper duplex stainless steel welds10.1016/j.corsci.2011.02.013 ↗
8. Gas tungsten arc and laser beam welding processes effects on duplex stainless steel 2205 properties10.1016/j.msea.2012.04.012 ↗
9. Characterization of microstructure, chemical composition, corrosion resistance and toughness of a multipass weld joint of superduplex stainless steel UNS S3275010.1016/j.matchar.2006.07.006 ↗
10. Weld oxide formation on lean duplex stainless steel10.1016/j.corsci.2008.06.024 ↗
11. Laser welding and surface treatment of a 22Cr–5Ni–3Mo duplex stainless steel10.1016/S0921-5093(02)00841-9 ↗
12. Protective diffusion coatings on magnesium alloys: a review of recent developments10.1016/j.jallcom.2011.12.124 ↗
13. Lower temperature fabrication of continuous intermetallic coatings on AZ91D magnesium alloy in molten salts10.1016/j.jallcom.2010.05.120 ↗
14. Austenite reformation in the heat-affected zone of duplex stainless steel 220510.1016/j.msea.2005.11.025 ↗
15. Influence of cooling rate on microstructure evolution and pitting corrosion resistance in the simulated heat-affected zone of 2304 duplex stainless steels10.1016/j.corsci.2012.01.018 ↗
16. Microstructural characterization of simulated heat affected zone in a nitrogen-containing 2205 duplex stainless steel10.1016/S0921-5093(02)00065-5 ↗
17. Influence of welding thermal cycles on microstructure and pitting corrosion resistance of 2304 duplex stainless steels10.1016/j.corsci.2011.10.039 ↗
18. Optimization of the pulsed current gas tungsten arc welding (PCGTAW) parameters for corrosion resistance of super duplex stainless steel (UNS S32760) welds using the Taguchi method10.1016/j.jallcom.2010.09.087 ↗
19. Secondary austenite and chromium nitride precipitation in simulated heat affected zones of duplex stainless steels10.1179/136217104225021715 ↗
20. Effect of shielding gases on mechanical and metallurgical properties of duplex stainless-steel welds10.1007/s10853-008-3098-8 ↗
21. The relationship between atomic partitioning and corrosion resistance in the weld-heat affected zone microstructures of UNS S32304 duplex stainless steel10.1007/s10853-007-1881-6 ↗
22. An experimental and theoretical study of heat-affected zone austenite reformation in three duplex stainless steels10.1007/s11661-997-0130-6 ↗
23. Growth kinetics of secondary austenite in the welding microstructure of a UNS S32304 duplex stainless steel10.1016/j.actamat.2006.03.018 ↗
24. Effect of composition profiles on metallurgy and corrosion behavior of duplex stainless steel weld metals
25. Effect of weld metal chemistry and heat input on the structure and properties of duplex stainless steel welds10.1016/S0921-5093(03)00077-7 ↗
26. Effect of nickel and nitrogen addition on the microstructure and mechanical properties of power beam processed duplex stainless steel (UNS 31803) weld metals10.1016/j.matlet.2005.03.010 ↗
27. Microstructure and stress corrosion cracking in simulated heat-affected zones of duplex stainless steels10.1016/S0010-938X(02)00068-9 ↗
28. Microstructure and pitting corrosion in simulated heat-affected zones of duplex stainless steels10.1016/S0254-0584(01)00409-6 ↗
29. The ferrite content of austenitic stainless steel weld metal
30. The effect of nitrogen and heat treatment on the microstructure and tensile properties of 25Cr–7Ni–1.5Mo–3W–xN duplex stainless steel castings10.1016/S0921-5093(00)01263-6 ↗
31. The effect of cooling rate on the mechanical and corrosion properties of SAF 2205 (UNS 31803) duplex stainless steel welds10.1016/S1359-6462(00)00613-8 ↗
32. Pitting corrosion of duplex stainless steels10.5006/1.3584986 ↗
33. Secondary austenite formation and its relation to pitting corrosion in duplex stainless steel weld metal10.1179/mst.1995.11.3.276 ↗
34. Annealing temperature effect on the pitting corrosion resistance of plasma arc welded joints of duplex stainless steel UNS S32304 in 1.0 M NaCl10.1016/j.corsci.2011.02.041 ↗
35. Effect of post-weld heat treatment on microstructure evolution and pitting corrosion behavior of UNS S31803 duplex stainless steel welds10.1016/j.corsci.2012.04.047 ↗
36. Effect of a brief post-weld heat treatment on the microstructure evolution and pitting corrosion of laser beam welded UNS S31803 duplex stainless steel10.1016/j.corsci.2012.08.054 ↗