This study investigated the dependent relationships between the microstructure and corrosion resistance of the 316L part using wire and arc additive manufacturing (WAAM), through electrochemical methods and multiscale characterization techniques. The results showed that the corrosion resistance strongly depended on anisotropy in the microstructure. On the top surface, fewer track-track fusion lines with weaker element segregation led to the best pitting corrosion resistance. But on the side surface perpendicular to the scanning direction, the narrower ferrite primary dendrite arm spacing, lower ferrite content and more uniform element distribution provided the best general corrosion resistance.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. EIS comparative study and critical Equivalent Electrical Circuit (EEC) analysis of the native oxide layer of additive manufactured and wrought 316L stainless steel10.1016/j.corsci.2020.108480 ↗
2. Stability, reactivity and breakdown of passive films
3. A. Karpagaraj, S. Baskaran, T. Arunnellaiappan, N.R. Kumar, A review on the suitability of wire arc additive manufacturing (WAAM) for stainless steel 316, in: ADVANCES IN MECHANICAL DESIGN, MATERIALS AND MANUFACTURE: Proceeding of the Second International Conference on Design, Materials and Manufacture (ICDEM 2019), 2020.10.1063/5.0004148 ↗
4. Wire and arc additive manufacturing: a comparison between CMT and TopTIG processes applied to stainless steel10.1007/s40194-018-0606-6 ↗
5. Wire + Arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
6. Adaptive process control implementation of wire arc additive manufacturing for thin-walled components with overhang features10.1007/s00170-019-04737-4 ↗
7. Thermo-mechanical analysis of Wire and Arc Additive Layer Manufacturing process on large multi-layer parts10.1016/j.commatsci.2011.06.023 ↗
8. Microstructural evolution and mechanical properties of maraging steel produced by wire + arc additive manufacture process10.1016/j.matchar.2017.12.002 ↗
9. Correlation between arc mode, microstructure, and mechanical properties during wire arc additive manufacturing of 316L stainless steel10.1016/j.msea.2019.02.078 ↗
10. Invited review article: Strategies and processes for high quality wire arc additive manufacturing
11. Evaluation of wire arc additive manufacturing for large-sized components in naval applications10.1007/s40194-017-0536-8 ↗
12. Fabrication of 316L nuclear nozzles on the main pipeline with large curvature by CMT wire arc additive manufacturing and self-developed slicing algorithm10.1016/j.msea.2021.141539 ↗
13. Microstructural characterization and mechanical integrity of stainless steel 316L clad layers deposited via wire arc additive manufacturing for nuclear applications10.1002/mawe.202000242 ↗
14. Microstructure and mechanical properties of the austenitic stainless steel 316L fabricated by gas metal arc additive manufacturing10.1016/j.msea.2017.05.024 ↗
15. Additive manufacturing – a general corrosion perspective10.1080/1478422X.2018.1511327 ↗
16. Influence of scanning strategy and building direction on microstructure and corrosion behaviour of selective laser melted 316L stainless steel10.1016/j.matdes.2021.109999 ↗
17. Statistical analysis of the pitting corrosion induced by potentiostatic pulse tests of wrought and SLM 316L stainless steels10.1016/j.corsci.2021.110036 ↗
18. Microstructure and corrosion characteristics of selective laser-melted 316L stainless steel: the impact of process-induced porosities10.1007/s11837-019-03647-w ↗
19. The corrosion of stainless steel made by additive manufacturing: a review10.3390/met11030516 ↗
20. Study on microstructure and tensile properties of 316L stainless steel fabricated by CMT wire and arc additive manufacturing10.1016/j.msea.2020.140006 ↗
21. Effect of post-heat treatment on the mechanical and corrosion behaviour of SS316L fabricated by wire arc additive manufacturing10.1016/j.matlet.2021.131015 ↗
22. Effect of heat treatment on microstructure, mechanical and corrosion properties of austenitic stainless steel 316L using arc additive manufacturing10.1016/j.msea.2017.10.002 ↗
23. Microstructural characterisation of thick-walled wire arc additively manufactured stainless steel10.1016/j.jmatprotec.2021.117373 ↗
24. Dynamic mechanical properties of 316L stainless steel fabricated by an additive manufacturing process10.1016/j.jmrt.2020.12.097 ↗
25. Effect of heat treatment temperature on microstructure and tensile properties of austenitic stainless 316L using wire and arc additive manufacturing10.1016/j.msea.2021.142446 ↗
26. Relationship between the microstructure and local corrosion properties of weld metal in austenitic stainless steels10.1016/j.corsci.2020.108867 ↗
27. Effects of linear heat input on microstructure and corrosion behavior of an austenitic stainless steel processed by wire arc additive manufacturing10.1016/j.vacuum.2019.109131 ↗
28. J. Bruckner, S. Schweißtechnik, Cold Metal Transfer (CMT)–Ein neuer Prozess in der Fügetechnik, Magna Steyr, (2005).
29. Unanticipated drastic decline in pitting corrosion resistance of additively manufactured 316L stainless steel after high-temperature post-processing10.1016/j.corsci.2019.108412 ↗
30. On the pitting corrosion of 2205 duplex stainless steel produced by laser powder bed fusion additive manufacturing in the as-built and post-processed conditions10.1016/j.matdes.2021.110260 ↗
31. Corrosion properties of 304L stainless steel made by directed energy deposition additive manufacturing10.1016/j.corsci.2019.02.029 ↗
32. Microstructure and corrosion behavior of a novel additively manufactured maraging stainless steel10.1016/j.electacta.2020.135925 ↗
33. Microstructure and corrosion performance of 316L stainless steel fabricated by Selective Laser Melting and processed through high-pressure torsion10.1016/j.jallcom.2018.05.284 ↗
34. Effect of build orientation and annealing on corrosion resistance of additively manufactured duplex stainless steel in 3.5% NaCl10.1149/1945-7111/abc5dd ↗
35. Modification of surface characteristics and electrochemical corrosion behavior of laser powder bed fused stainless-steel 316L after laser polishing
36. Effects of crystallographic orientation on the corrosion behavior of stainless steel 316L manufactured by laser powder bed fusion10.1016/j.corsci.2021.110009 ↗
37. The passivity of selective laser melted 316L stainless steel10.1016/j.apsusc.2019.144495 ↗
38. Enhancement of corrosion resistance of a biomedical grade 316LVM stainless steel by potentiodynamic cyclic polarization10.1016/j.tsf.2006.11.054 ↗
39. EIS study of potentiostatically formed passive film on 304 stainless steel10.1016/j.electacta.2011.07.072 ↗
40. The enhancement of microstructure on the passive and pitting behaviors of selective laser melting 316L SS in simulated body fluid10.1016/j.apsusc.2018.10.150 ↗
41. Electrochemical studies on the effect of residual stress on the corrosion of 316L manufactured by selective laser melting10.1016/j.corsci.2019.108314 ↗
42. The analysis of electrode impedances complicated by the presence of a constant phase element10.1016/S0022-0728(84)80324-1 ↗
43. Technical note: concerning the conversion of the constant phase element parameter Y0 into a capacitance10.5006/1.3280607 ↗
44. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
45. Production of corrosion-resistant 316L stainless steel clads on carbon steel using powder bed fusion-selective laser melting10.1016/j.jmatprotec.2019.05.024 ↗
46. Revealing relationships between porosity, microstructure and mechanical properties of laser powder bed fusion 316L stainless steel through heat treatment10.1016/j.matdes.2020.108481 ↗
47. Quantitative multiscale correlative microstructure analysis of additive manufacturing of stainless steel 316L processed by selective laser melting10.1016/j.matchar.2019.110074 ↗
48. Effect of molten pool boundaries on the mechanical properties of selective laser melting parts10.1016/j.jmatprotec.2014.06.002 ↗
49. Multi-scale characterisation of microstructure and texture of 316L stainless steel manufactured by laser powder bed fusion10.1016/j.matchar.2021.111663 ↗
50. Micro- and macro-structural heterogeneities in 316L stainless steel prepared by electron-beam melting10.1016/j.matchar.2018.04.026 ↗
51. Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing10.1016/j.actamat.2016.03.063 ↗
52. Effect of cooling rate on solidification microstructures in AISI 304 stainless steel10.1179/174328408X295962 ↗
53. Measurement of ferrite content of stainless steel sheet welds using a new Ferrite Density Number scale10.1016/j.jmatprotec.2019.116278 ↗
54. Wire and arc additive manufactured steel: Tensile and wear properties
55. Study on microstructure and tensile properties of high nitrogen Cr-Mn steel processed by CMT wire and arc additive manufacturing10.1016/j.matdes.2019.107611 ↗
56. Characterization of stainless steel parts by Laser Metal Deposition Shaping10.1016/j.matdes.2013.09.006 ↗
57. Microstructure of stainless steel single-crystal electron beam welds10.1007/BF02672592 ↗
58. Excellent mechanical and corrosion properties of austenitic stainless steel with a unique crystallographic lamellar microstructure via selective laser melting10.1016/j.scriptamat.2018.09.017 ↗
59. Non-metallic inclusions in steels – origin and control10.1016/j.jmrt.2018.04.003 ↗
60. Additive manufacturing of steels: a review of achievements and challenges10.1007/s10853-020-05109-0 ↗
61. Hardened austenite steel with columnar sub-grain structure formed by laser melting10.1016/j.msea.2014.12.018 ↗
62. Characterization of nano-scale oxides in austenitic stainless steel processed by powder bed fusion10.1016/j.scriptamat.2018.06.011 ↗
63. Austenitic stainless steel strengthened by the in situ formation of oxide nanoinclusions10.1039/C4RA16721J ↗
64. On the enhanced corrosion resistance of a selective laser melted austenitic stainless steel10.1016/j.scriptamat.2017.07.037 ↗
65. Enhanced corrosion resistance of additively manufactured 316L stainless steel after heat treatment10.1149/1945-7111/abc10e ↗
66. Inclusion evolution in additive manufactured 316L stainless steel by laser metal deposition process10.1016/j.matdes.2018.06.001 ↗
67. Why stainless steel corrodes10.1038/415770a ↗
68. Corrosion of metallic materials fabricated by selective laser melting10.1038/s41529-019-0086-1 ↗
69. Microstructural and selective dissolution analysis of 316L austenitic stainless steel10.1016/j.jmrt.2021.10.009 ↗
70. Evaluation of microstructure and electrochemical corrosion behavior of austenitic 316 stainless steel weld metals with varying chemical compositions10.1361/10599490523977 ↗
71. Microstructural evolution and chemical corrosion of electron beam wire-feed additively manufactured AISI 304 stainless steel10.1016/j.jallcom.2019.06.246 ↗
72. The effect of ferrite content on mechanical properties and corrosion behaviour of austenitic stainless steel 308L weld metal10.4028/www.scientific.net/SSP.263.108 ↗
73. Effect of solution concentration on semiconducting properties of passive films formed on austenitic stainless steels10.1016/j.corsci.2009.09.003 ↗
74. Quasi-in-situ ex-polarized TEM observation on dissolution of MnS inclusions and metastable pitting of austenitic stainless steel10.1016/j.corsci.2015.08.009 ↗
75. Composition changes around sulphide inclusions in stainless steels, and implications for the initiation of pitting corrosion10.1016/j.corsci.2010.07.021 ↗
76. On the corrosion and metastable pitting characteristics of 316l stainless steel produced by selective laser melting10.1149/2.0551706jes ↗
77. The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions10.1016/0010-938X(92)90074-D ↗
78. On the in-situ characterisation of metastable pitting using 316L stainless steel as a case study10.1016/j.corsci.2020.109004 ↗
79. Improvement of corrosion resistance of SS316L manufactured by selective laser melting through subcritical annealing10.1016/j.corsci.2019.108353 ↗
80. On the pitting behaviour of laser powder bed fusion prepared 316L stainless steel upon post-processing heat treatments10.1016/j.corsci.2021.110060 ↗
81. Towards a better understanding of localised corrosion induced by typical non-metallic inclusions in low-alloy steels10.1016/j.corsci.2020.109150 ↗
82. Localized corrosion: passive film breakdown vs. Pit growth stability, Part VI: Pit dissolution kinetics of different alloys and a model for pitting and repassivation potentials10.1016/j.corsci.2021.109277 ↗
83. Plenary Lecture—1986: effects of alloy composition and microstructure on the passivity of stainless steels10.5006/1.3584918 ↗
84. Pit growth studies in stainless steel foils. I. Introduction and pit growth kinetics10.1016/S0010-938X(01)00133-0 ↗
85. Study of the correlation between pitting corrosion and the component ratio of the dual phase in duplex stainless steel welds10.1016/j.corsci.2013.04.033 ↗
86. Comparative studies on microstructure evolution and corrosion resistance of 304 and a newly developed high Mn and N austenitic stainless steel welded joints10.1016/j.corsci.2021.109338 ↗
87. The influence of crystallographic orientation distribution on 316LVM stainless steel pitting behavior10.1016/j.corsci.2008.12.019 ↗
88. Wire arc deposition additive manufacturing and experimental study of 316L stainless Steel by CMT + P Process10.3390/met10111419 ↗