journal article·2004-05

Pit to crack transition in stress corrosion cracking of a steam turbine disc steel

A Turnbull, S Zhou

Corrosion Science· Volume 46· Issue 5
Publisher page

Abstract

Abstract Long term exposure tests have been carried out on a 3 NiCrMoV steam turbine disc steel in the form of cylindrical tensile test specimens self-loaded to 90% of σ 0.2 and exposed to three environmental conditions, viz. deaerated pure water, aerated pure water, and aerated water containing 1.5 ppm of chloride ion. Pitting occurred in all environments but the density and depth of pits in the chloride-containing medium was markedly greater. No cracking was observed in deaerated pure water but cracks initiated in aerated water between 13 and 19 months and in less than 7 months in aerated 1.5 ppm Cl − solution. The probability of a crack initiating from a pit of specific depth in aerated solution could be described well by a Weibull function. Profiling of pits and cracks in the disc steel tested in aerated 1.5 ppm Cl − solution showed that there while there were many cracks with a depth greater than that of the corresponding pit the depth of some cracks was smaller than that of the corresponding pit, suggesting that cracks do not necessarily initiate from the bottom of the pits. The growth rate of short cracks emerging from pits appeared greater than that of long cracks in fracture mechanics specimens.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Material Properties and Failure Mechanisms · High Temperature Alloys and Creep · Nuclear Engineering Thermal-Hydraulics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. S. Zhou, A. Turnbull, Steam Turbine Operating Conditions, Chemistry of Condensates and Environment Assisted Cracking––An Overview, NPL Report MATC (A) 45 (2002)
2. ASTM, E 8-94a, Standard Test Methods for Tension Testing of Metallic Materials, 1994
3. British Standard, BS ISO 4287, Geometric Product Specification (GPS)––Surface Texture––Terms, definitions and surface texture parameters, 1997
4. Development of a pre-pitting procedure for turbine disc steel10.1179/000705900101501137 ↗
5. Marshall · J. Chem. Eng. Data · 1987 · 32 · 22110.1021/je00048a027 ↗
6. P.E. Francis, A.D. Mercer, Corrosion of a mild steel in distilled water and chloride solutions: Development of a test method, in: G.S. Hayne, R. Baboian (Eds.), Laboratory Corrosion Tests and Standards, ASTM STP 866, American Society fro Testing and Materials, Philadelphia, 1985, pp. 184–19610.1520/STP33779S ↗
7. A.D. Mercer, G.M. Brook, La Tribune du, CEBEDEAU 31 (417–418) (1978) 299–306
8. Turnbull · Corros. Sci. · 2004 · 46 · 19310.1016/S0010-938X(03)00118-5 ↗
9. A. Turnbull, S. Zhou, Effect of Oxygen and Chloride on Pitting and Stress Corrosion Cracking of a Steam Turbine Disc Steel, NPL Report MATC (A) 133, 2003
10. Baes · 1976
11. G. Gabetta, E. Caretta, Investigation on pit susceptibility in low pressure rotor steels, in: Proceedings of Materials for Advanced Power Engineering, 1994, 3–6 October, Kluwer Academic Press, Dordrecht, 1994, pp. 209–21810.1007/978-94-011-1048-8_14 ↗
12. W. David, G. Rottger, K. Schleithoff, H. Hamel, H. Termuehlen, Disk-type LP turbine rotor experience, PWR-Vol 21, The Steam Turbine Generator Today: Material, Flow Path Design, Repair and Refurbishment, ASME 1993, pp. 83–91, 1993
13. M.O. Speidel, R. Magdowski, in: 2nd International Symposium Environmental Effects on Degradation in Nuclear Power Plants, Monterey, 9–12 September 1985, pp. 267–275
14. M.O. Speidel, J. Denk, B. Scarlin, Stress corrosion cracking and corrosion fatigue of steam-turbine rotor and blade materials, Cost Project, EUR 13186 EN, 1991
15. M.O. Speidel, B. Scarlin, Stress corrosion cracking and corrosion fatigue of steam-turbine rotor and blade materials, in: Proceedings of High Temperature Materials for Power Engineering, Liege, Belgium, 24–27 September 1990, p. 343
16. Kondo · Corrosion · 1989 · 45 · 710.5006/1.3577891 ↗
17. S. Zhou, A. Turnbull, Environment assisted cracking of steam turbine disc and blade steels––description of test procedure and preliminary results, NPL Report, MATC(A)41, 2001