Kinetics inversion in isothermal oxidation of uncoated WC-based carbides between 450 and 800°C
Source abstract
Abstract
Abstract Oxidation of uncoated WC-based carbides (hard metals) has been investigated between 450 and 800 °C. An anomalous change in the oxidation behaviour has been found in the temperature range between 528 and 630 °C. Instead of the normal increase of the oxidation rates when the temperature increases, a kinetics inversion is produced: an anomalous decrease of the oxidation rates has been observed in this temperature range. Furthermore, this anomalous behaviour produces an important change in the activation energy. At temperatures below the anomaly (below 528 °C), an activation energy of 119 ± 8 kJ/mol has been found, whereas above the anomaly (above 630 °C), an activation energy of 208 ± 8 kJ/mol has been found. This anomalous temperature dependence of the oxidation behaviour can be related to a higher amount of complex oxide CoWO4 formed on the oxide scale, and to the effect that this oxide produces in the oxidation kinetics of the other oxides.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · High-Temperature Coating Behaviors · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Brookes · 1987
2. Advances in powder technology
3. Radiation thermometry applied to temperature measurement in the cutting process10.1088/0957-0233/18/11/022 ↗
4. Oxidation behaviour of hard and binder phase modified WC–10Co cemented carbides10.1007/BF00729663 ↗
5. Strength degradation of a tungsten carbide–cobalt composite at elevated temperatures10.1016/S1044-5803(98)00056-4 ↗
6. Oxidation of WC–Co, WC–Ni and WC–Co–Ni hard metals in the temperature range 500–800°C10.1016/0263-4368(96)00009-1 ↗
7. High-temperature oxidation of tungsten carbide–cobalt composites in the presence of MDF
8. Oxidation-induced strength degradation of WC–Co hardmetals10.1016/S0263-4368(01)00033-6 ↗
9. High-temperature fatigue of cemented carbides under cyclic loads10.1016/S0263-4368(99)00014-1 ↗
10. Oxidation behavior of WC–Co10.1016/0921-5093(95)10145-4 ↗
11. Kinetics of WC–Co oxidation accompanied by swelling10.1007/BF00351615 ↗
12. New experimental device for infrared spectral directional emissivity measurements in controlled environment10.1063/1.2393157 ↗
13. Iron oxidation kinetics study by using infrared spectral emissivity measurements below 570°C10.1016/j.corsci.2007.05.029 ↗
14. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650°C10.1016/j.corsci.2004.01.010 ↗
15. Anomalous high-temperature oxidation in the zirconium–copper system10.1016/j.corsci.2003.10.029 ↗
16. Effect of the ο-α-Al2O3 Transformation in scales on the oxidation behavior of a nickel-base Superalloy with an aluminide diffusion coating10.1023/A:1004654429687 ↗
17. Oxidation behavior of Al-alloyed ZrSi210.1023/A:1010317510122 ↗
18. Oxidation behavior of TiC-containing Ti3AlC2 based material at 500–900°C in air10.1007/s10019-003-0278-7 ↗