Oxidation behavior, thermal stability, and the coating/substrate interface evolution of CrN-coated Zircaloy under high-temperature steam
Source abstract
Abstract
Abstract CrN-coated Zircaloy samples were prepared by cathodic arc ion plating, and the microstructure, stability, and oxidation behaviors of the CrN coatings in high-temperature steams were comprehensively investigated. The CrN coating significantly increased the oxidation resistance of Zircaloy exposed to steam through the formation of a dense Cr2O3 oxide layer without cracking or spallation. Two different multi-layered coatings were produced after the steam exposures. The nitrogen diffusion properties of the CrN coatings during oxidation were examined. The internal oxidation of Zr particles inside the nitride coating was observed. A ZrN nano-twinned layer formed at the coating/substrate interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Nuclear Materials and Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Corrosion resistance and antifouling activities of silver-doped CrN coatings deposited by magnetron sputtering10.1016/j.surfcoat.2018.09.006 ↗
2. Effect of positive pulse voltage in bipolar reactive HiPIMS on crystal structure, microstructure and mechanical properties of CrN films10.1016/j.surfcoat.2020.125773 ↗
3. Study of the oxidation behavior of CrN coating on Zr alloy in air10.1016/j.jnucmat.2019.01.006 ↗
4. Investigation of oxidation behaviors of coated Zircaloy as accident-tolerant fuel with CrAlN and CrAlSiN coatings in high-temperature steam10.1016/j.corsci.2020.108896 ↗
5. Comparative study on protective properties of CrN coatings on the ABS substrate by DCMS and HiPIMS techniques10.1016/j.surfcoat.2020.125890 ↗
6. Friction and wear behavior of CrN coating on 316L stainless steel in liquid sodium at elevated temperature10.1016/j.triboint.2019.106079 ↗
7. Improvement in corrosion resistance of CrN coatings10.1016/j.surfcoat.2018.07.018 ↗
8. Fretting damage of TiN coated zircaloy-4 tube10.1016/S0043-1648(01)00674-3 ↗
9. Superior corrosion resistance properties of TiN-based coatings on Zircaloy tubes in supercritical water10.1016/j.jnucmat.2014.04.010 ↗
10. Ceramic coating for corrosion (c3) resistance of nuclear fuel cladding10.1016/j.surfcoat.2015.08.062 ↗
11. Multilayer (TiN, TiAlN) ceramic coatings for nuclear fuel cladding10.1016/j.jnucmat.2016.05.021 ↗
12. Investigation of the impact of coatings on corrosion and hydrogen uptake of Zircaloy-410.1016/j.jnucmat.2015.09.041 ↗
13. Characterization of PVD Cr, CrN, and TiN coatings on SiC10.1016/j.jnucmat.2019.151781 ↗
14. High temperature oxidation of a CrN coating deposited on a steel substrate by ion plating10.1016/S0257-8972(01)01238-5 ↗
15. High temperature oxidation of ion-plated CrN films10.1557/JMR.1994.0151 ↗
16. Oxidation resistance of PVD Cr, Cr-N and Cr-NO hard coatings10.1016/0257-8972(93)90091-2 ↗
17. Mechanical properties, thermal stability and oxidation resistance of TiN/CrN multilayer coatings10.1016/j.vacuum.2020.109468 ↗
18. Adhesion property and high-temperature oxidation behavior of Cr-coated Zircaloy-4 cladding tube prepared by 3D laser coating10.1016/j.jnucmat.2015.06.030 ↗
19. High-temperature oxidation of thick Cr coating prepared by arc deposition for accident tolerant fuel claddings10.1016/j.jnucmat.2019.01.039 ↗
20. Influence of pulse parameters on the mechanical properties and electrochemical corrosion behavior of electrodeposited Ni-W alloy coatings with high tungsten content10.1016/j.corsci.2019.108409 ↗
21. Effects of multi-layer structure on microstructure, wear and erosion performance of the Cr/CrN films on Ti alloy substrate10.1016/j.apsusc.2019.04.008 ↗
22. Oxidation of CrNx hard coatings reactively sputtered at low temperature10.1016/0040-6090(93)90718-5 ↗
23. Thermal decomposition routes of CrN hard coatings synthesized by reactive arc evaporation and magnetron sputtering10.1016/j.tsf.2008.06.086 ↗
24. Intermetallics and phase transformations of the Zr-1.0Sn-0.3Nb-0.3Fe-0.1Cr alloy10.1016/S1001-0521(08)60164-3 ↗
25. 2.07 – zirconium alloys: properties and characteristics10.1016/B978-0-08-056033-5.00015-X ↗
26. A systematic study of the oxidation behavior of Cr coatings on Zry4 substrates in high temperature steam environment10.1016/j.corsci.2020.108826 ↗
27. Thermal stability of CrN/AlN superlattice coatings10.1016/j.surfcoat.2013.12.035 ↗
28. Thermally induced transitions of CrN thin films10.1016/j.scriptamat.2007.03.058 ↗
29. Barin · 1989
30. Phase equilibria and multiphase reaction diffusion in the Cr-C and Cr-N systems10.1361/105497199770335929 ↗
31. Dislocation reactions in ZrN10.1016/S1359-6454(02)00250-1 ↗
32. First-principles calculations of the twin boundary energies and adhesion energies of interfaces for cubic face-centered transition-metal nitrides and carbides10.1016/j.apsusc.2015.07.189 ↗
33. High temperature steam oxidation of chromium-coated zirconium-based alloys: kinetics and process10.1016/j.corsci.2020.108537 ↗
34. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
35. Deformation twinning10.1016/0079-6425(94)00007-7 ↗
36. Effects of twin boundaries in vanadium nitride films subjected to tensile/compressive deformations10.1016/j.apsusc.2017.07.174 ↗
37. Strength and ductility of 316L austenitic stainless steel strengthened by nano-scale twin bundles10.1016/j.actamat.2011.11.009 ↗
38. Gestin · 2017
39. Okamoto · 1990
40. Growth twins and deformation twins in metals10.1146/annurev-matsci-070813-113304 ↗
41. Nucleation and thickening of shear bands in nano-scale twin/matrix lamellae of a Cu–Al alloy processed by dynamic plastic deformation10.1016/j.actamat.2010.01.049 ↗
42. G.T. Gray III. Orientation dependence of shock-induced twinning and substructures in a copper bicrystal10.1016/j.actamat.2009.09.033 ↗
43. AlN/CrN multilayer structures with increased thermal stability10.1016/j.scriptamat.2016.12.020 ↗
44. Temperature dependence of thermal expansion coefficient and Bi-axial Modulus of arc-ion plated tin, crn, Cr2N and AlTin coations10.4139/sfj.50.52 ↗
45. High rate deposition of thick CrN and Cr2N coatings using modulated pulse power (MPP) magnetron sputtering10.1016/j.surfcoat.2010.11.039 ↗
46. Material selection for hard coatings10.1116/1.573700 ↗
47. Helium irradiation induced ultra-high strength nanotwinned Cu with nanovoids10.1016/j.actamat.2019.07.003 ↗
48. High-strength sputter-deposited Cu foils with preferred orientation of nanoscale growth twins10.1063/1.2198482 ↗