Abstract

Abstract Different welding thermal cycles from single-pass to triple-pass were performed on two kinds of 2304 duplex stainless steel through Gleebe thermal–mechanical simulator. The corresponding microstructure was observed, while the pitting corrosion resistance was investigated in 1.0 M NaCl by potentiostatic critical pitting temperature (CPT). The results showed that single-pass welding deteriorated microstructure and pitting corrosion resistance significantly. As the welding pass increased, the ferrite content decreased and CPT increased. However, CPT was still lower than that of the base metal. Nitride precipitated at the boundary between ferrite and austenite phase for low-alloyed 2304 after the single-pass welding thermal cycle.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. J. Charles, S. Bernhardson, Proc. Conference “Duplex Stainless Steels’ 91”, vol. 2, Beaune, France, 1991, pp. 3–48.
2. Overview of super duplex stainless steel10.1179/mst.1992.8.8.685 ↗
3. Corrosion resistance evaluation of the UNS S31803 duplex stainless steels aged at low temperatures (350–550°C) using DLEPR tests10.1007/s10853-005-5700-7 ↗
4. Effect of annealing treatment on microstructure evolution and the associated corrosion behavior of a super-duplex stainless steel10.1016/j.jallcom.2009.12.127 ↗
5. Effect of composition profiles on metallurgy and corrosion behavior of duplex stainless steel weld metals
6. Growth kinetics of secondary austenite in the welding microstructure of a UNS S32304 duplex stainless steel10.1016/j.actamat.2006.03.018 ↗
7. Effect of nickel and nitrogen addition on the microstructure and mechanical properties of power beam processed duplex stainless steel (UNS 31803) weld metals10.1016/j.matlet.2005.03.010 ↗
8. The relationship between atomic partitioning and corrosion resistance in the weld-heat affected zone microstructures of UNS S32304 duplex stainless steel10.1007/s10853-007-1881-6 ↗
9. The effect of N-2 addition upon the MIG welding process of duplex steels10.1007/s10853-006-0557-y ↗
10. Laser welding and surface treatment of a 22Cr–5Ni–3Mo duplex stainless steel10.1016/S0921-5093(02)00841-9 ↗
11. Effect of weld metal chemistry and heat input on the structure and properties of duplex stainless steels10.1016/S0921-5093(03)00077-7 ↗
12. Microstructural transformations of heat affected zones in duplex steel welded joints10.1016/j.matchar.2006.02.007 ↗
13. Effect of shielding gases on mechanical and metallurgical properties of duplex stainless-steel welds10.1007/s10853-008-3098-8 ↗
14. The relationship between chromium nitride and secondary austenite precipitation in duplex stainless steels10.1007/s11661-003-0304-9 ↗
15. Effect of solution treatment temperature on the precipitation kinetic of σ-phase in 2205 duplex stainless steel welds10.1016/j.msea.2008.06.024 ↗
16. Microstructure and stress corrosion cracking in simulated heat-affected zones of duplex stainless steels10.1016/S0010-938X(02)00068-9 ↗
17. Microstructural characterization of simulated heat affected zone in a nitrogen-containing 2205 duplex stainless steel10.1016/S0921-5093(02)00065-5 ↗
18. Austenite reformation in the heat-affected zone of duplex stainless steel 220510.1016/j.msea.2005.11.025 ↗
19. Effect of Mo substitution by W on impact property of heat affected zone in duplex stainless steels10.1016/S1359-6462(96)00377-6 ↗
20. Observations of ferrite/austenite transformations in the heat affected zone of 2205 duplex stainless steel spot welds using time resolved X-ray diffraction10.1016/j.msea.2004.03.037 ↗
21. Microstructure and pitting corrosion in simulated heat-affected zones of duplex stainless steels10.1016/S0254-0584(01)00409-6 ↗
22. The theory of moving sources of heat and its application to metal treatments
23. Dependence of critical pitting temperature on the concentration of sulphate ion in chloride containing solutions10.1016/j.apsusc.2007.03.034 ↗
24. Effect of annealing temperature on the pitting corrosion resistance of super duplex stainless steel UNS S3275010.1016/j.matchar.2009.04.009 ↗
25. Effects of solution treatment, continuous cooling on σ-phase precipitation in a 2205 duplex stainless steel10.1016/S0921-5093(01)00911-X ↗
26. Influence of nickel on the susceptibility to corrosion fatigue of duplex stainless steel welds10.1016/S0142-1123(01)00018-4 ↗
27. Effect of nickel alloying on crevice corrosion resistance of stainless steels10.1016/j.corsci.2004.01.003 ↗
28. T.G. Gooch, Conf. Proc. Duplex Stainless Steels, St. Louis, ASM, 1983, pp. 573–602.
29. Annealing temperature effects on superduplex stainless steel UNS S32750 welded joints. II: pitting corrosion resistance evaluation10.1007/s10853-010-4311-0 ↗
30. Effects of Cr2N on the pitting corrosion of high nitrogen stainless steels10.1016/j.electacta.2006.08.034 ↗
31. Characterization of weld solidification cracking in a duplex stainless steel10.1016/0026-0800(89)90037-2 ↗
32. Correlation between critical pitting temperature and degree of sensitisation on alloy 2205 duplex stainless steel10.1016/j.corsci.2010.10.009 ↗
33. Failure analysis of duplex stainless steel weld used in flexible pipes in off shore oil production10.1016/j.engfailanal.2010.05.012 ↗
34. Partitioning of chromium and molybdenum in super duplex stainless steels with respect to nitrogen and nickel content10.1016/S0921-5093(97)00521-2 ↗
35. Garfias-Mesias · Corros. Sci. · 1996 · 38 · 131910.1016/0010-938X(96)00022-4 ↗
36. Corrosion resistance of super duplex stainless steels in chloride ion containing environments: investigations by means of a new microelectrochemical method: I. Precipitation-free states10.1016/S0010-938X(00)00087-1 ↗
37. Effect of thermal cycles on the corrosion and mechanical properties of UNS S31803 duplex stainless steel10.1016/j.corsci.2009.08.015 ↗