journal article·2020-05

High-performance Cr2AlC MAX phase coatings: Oxidation mechanisms in the 900–1100°C temperature range

Zhenyu Wang, Guanshui Ma, Linlin Liu, Li Wang, Peiling Ke, Qunji Xue, Aiying Wang

Corrosion Science· Volume 167
Publisher page

Abstract

Abstract Dense and predominantly single-phase Cr2AlC MAX phase coatings without columnar structure were fabricated using an easy combined arc/sputtering deposition method followed by annealing. Isothermal oxidation of coatings was conducted under flowing air for 40 h at 900−1100 °C. Although the results revealed that the oxide scale showed strong dependence upon oxidation temperature, the coated samples remained intact even after oxidation at 1100 °C. Such excellent resistance to oxidation resulted in the parabolic kinetics exhibiting two stages. This was attributed to the formation of a dense and continuous Al2O3 interface layer and a (Cr, Al)2O3 outermost layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced Photocatalysis Techniques · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. The Mn+1AXnphases: a new class of solids: thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Mechanical properties of Cr2AlC ceramics10.1111/j.1551-2916.2007.01634.x ↗
3. Cold spray deposition of Cr2AlC MAX phase for coatings and bond-coat layers10.1016/j.jeurceramsoc.2018.11.035 ↗
4. Bonding and oxidation protection of Ti2AlC and Cr2AlC for a Ni-based superalloy10.1016/j.jeurceramsoc.2018.10.019 ↗
5. Environmental resistance of Cr2AlC MAX phase under thermal gradient loading using a burner rig10.1111/jace.15425 ↗
6. Oxyacetylene torch testing and microstructural characterization of a Cr2AlC ceramic10.1016/j.jallcom.2017.12.373 ↗
7. The ternary system: Cr-Al-C, V-Al-C, and Ti-Al-C and the behavior of H-phases (M2AlC)10.1016/0022-4596(80)90569-1 ↗
8. Saturation of ion irradiation effects in MAX phase Cr2AlC10.1016/j.actamat.2016.03.021 ↗
9. Protective coatings on zirconium-based alloys as accident-tolerant fuel (ATF) claddings10.1515/corrrev-2017-0010 ↗
10. Hot corrosion and low cycle fatigue of a Cr2AlC-coated superalloy10.1016/j.msea.2017.10.098 ↗
11. Improving the high-temperature oxidation resistance of a β–γ TiAl alloy by a Cr2AlC coating10.1016/j.corsci.2010.07.031 ↗
12. Short-term oxidation resistance and degradation of Cr2AlC coating on M38G superalloy at 900-1100 °C10.1016/j.corsci.2011.07.032 ↗
13. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
14. Influence of grain size on high temperature oxidation behavior of Cr2AlC ceramics10.1016/j.ceramint.2012.09.039 ↗
15. Reply to comment on “Microstructural evolution during high-temperature oxidation of Ti2AlC ceramics”10.1016/j.scriptamat.2011.08.015 ↗
16. Preparation of transmission electron microscopy cross-section specimens using focused ion beam milling10.1116/1.1378072 ↗
17. Application of the Rietveld refinement method for quantification of mineral concentrations in bauxite residues (alumina refining tailings)10.1016/j.minpro.2015.04.004 ↗
18. Phase formation and microstructure evolution of arc ion deposited Cr2AlC coating after heat treatment10.1016/j.apsusc.2012.09.082 ↗
19. Dense and high-stability Ti2AlN MAX phase coatings prepared by the combined cathodic arc/sputter technique10.1016/j.apsusc.2016.11.183 ↗
20. Behaviors of helium in Cr2AlC from first principles10.1111/jace.15781 ↗
21. Parabolic laws during high temperature oxidation: relations with the grain size and thickness of the oxide10.1023/A:1006677631548 ↗
22. Studying the oxidation of Ti2AlC MAX phase in atmosphere: a review10.1016/j.ijrmhm.2016.07.006 ↗
23. Cyclic oxidation of Ti3AlC2 at 1000–1300 °C in air10.1016/j.corsci.2010.09.033 ↗
24. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
25. Effect of Ti on the microstructure change and oxidation behavior of Ni+CrAlYHfSiN composite coatings10.1016/j.corsci.2019.01.023 ↗
26. Oxidation behavior of Cr2AlC ceramics at 1100 and 1250 °C10.1007/s10853-008-2516-2 ↗
27. High-temperature oxidation of Fe3Al based iron aluminides in oxygen10.1016/S0010-938X(01)00035-X ↗
28. Structure characterization and tribological study of magnetron sputtered nanocomposite nc-TiAlV(N,C)/a-C coatings10.1039/c1jm10707k ↗
29. Formation of Al2O3 diffusion barrier in cold-sprayed NiCoCrAlY/Ni multi-layered coatings on 304SS substrate10.1016/j.surfcoat.2016.09.058 ↗
30. Investigating efficiency of α-Al2O3 diffusion barrier layer in oxidation of EB-PVD NiCrAlY coatings10.1179/1743294414Y.0000000365 ↗
31. Coating designs for oxidation control of Mo–Si–B alloys10.1016/S1359-6462(02)00070-2 ↗
32. Ab initio calculations and experimental determination of the structure of Cr2AlC10.1016/j.ssc.2004.02.047 ↗
33. Fabrication and oxidation behavior of Cr2AlC coating on Ti6242 alloy10.1016/j.surfcoat.2010.01.002 ↗
34. A new approach to manufacture oxidation-resistant NiCrAl overlay coatings by electrodeposition10.1016/j.corsci.2019.01.039 ↗
35. Analysis of the microstructural evolution and interface diffusion behavior of NiCoCrAlYTa coating in high temperature oxidation10.1016/j.corsci.2019.03.022 ↗
36. Synthesis, Characterization, and Consolidation of Cr2(C,N) Solid Solution Powders10.1111/jace.14215 ↗
37. Part I. Mechanism of oxidation of Cr2AlC films in temperature range 700-1200°C10.1179/1743294414Y.0000000417 ↗
38. Part II. Oxidation of yttrium doped Cr2AlC films in temperature range between 700 and 1200 °C10.1179/1743294414Y.0000000418 ↗
39. Oxidation of Cr2AlC Between 900 and 1200 °C in Air10.1007/s11085-007-9071-0 ↗