The aim of this study is to evaluate the effects of Ag3Sn intermetallic compounds (IMCs) on corrosion of Sn-3.0Ag-0.5Cu (SAC305) solder alloy under high-temperature and high-humidity condition. The Ag3Sn IMCs of SAC305 with various size and morphology were obtained by changing cooling rate. Commercial SAC305 solder with smallest Ag3Sn IMCs exhibits better corrosion resistance than air-cooled and furnace-cooled SAC305 solders because microgalvanic corrosion between large cathodic Ag3Sn IMCs plates and anodic Sn matrix decreased the corrosion resistance of air-cooled and furnace-cooled SAC305 solders. (c) 2012 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · 3D IC and TSV technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Electrochemical composite deposition of Sn–Ag–Cu alloys10.1016/j.mseb.2009.09.012 ↗
2. A new unified constitutive model with short- and longrange back stress for lead-free solders of Sn–3Ag–0.5Cu and Sn–0.7Cu10.1016/j.ijplas.2009.02.007 ↗
3. Mechanical and microstructural properties of SnAgCu solder joints10.1016/j.msea.2006.01.065 ↗
4. Influence of thermal aging on microhardness and microstructure of Sn-0.3Ag-0.7Cu-xIn lead-free solders10.1016/j.jallcom.2010.05.057 ↗
5. Effect of 9wt.% in addition to Sn3.5Ag0.5Cu solder on the interfacial reaction with the Au/NiP metallization on Cu pads10.1016/j.jallcom.2005.01.001 ↗
6. A reliability model for SAC solder covering isothermal mechanical cycling and thermal cycling conditions10.1016/j.microrel.2009.08.008 ↗
7. Corrosion characterization of tin–lead and lead free solders in 3.5wt.% NaCl solution10.1016/j.corsci.2007.11.025 ↗
8. Corrosion of tin alloys in sulfuric and nitric acids10.1016/S0010-938X(01)00094-4 ↗
9. Electrochemical corrosion study of Sn-3Ag-3Cu solder alloy in NaCl solution10.1016/j.electacta.2009.07.030 ↗
10. Electrochemical corrosion behaviour of lead-free Sn-8.5 Zn-XAg-0.1 Al-0.5 Ga solder in 3.5% NaCl solution10.1016/j.msea.2005.05.101 ↗
11. Electrochemical corrosion behaviour of Pb-free Sn-8.5Zn-0.05Al-XGa and Sn-3Ag-0.5Cu alloys in chloride containing aqueous solution10.1016/j.corsci.2008.06.042 ↗
12. Electrochemical behavior of a lead-free SnAg solder alloy affected by the microstructure array10.1016/j.matdes.2011.06.032 ↗
13. Formation of Ag3Sn plates in SnAgCu solder bumps10.1016/j.msea.2009.12.020 ↗
14. Effects of microstructure and temperature on corrosion behavior of Sn-3.0Ag-0.5Cu lead-free solder10.1007/s10854-011-0552-1 ↗
15. Anodic dissolution characteristics and electrochemical migration lifetimes of Sn solder in NaCl and Na2SO4 solutions10.1016/j.mee.2008.03.015 ↗
16. A study of the thin film on the surface of Sn-3.5Ag/Sn-3.5Ag-2.0Cu lead-free alloy10.1016/j.jallcom.2005.07.050 ↗
17. Effect of oxide thickness of solder powders on the coalescence of SnAgCu lead-free solder pastes10.1016/j.jallcom.2009.08.035 ↗
18. Corrosion products of tin in humid air containing sulfur dioxide and nitrogen dioxide at room temperature10.1016/S0010-938X(02)00151-8 ↗
19. Experimental and thermodynamic assessment of Sn–Ag–Cu solder alloys10.1007/s11664-000-0003-x ↗
20. Growth mechanism of bulk Ag3Sn intermetallic compounds in Sn–Ag solder during solidification10.1016/j.intermet.2008.06.016 ↗
21. The effects of suppressed beta tin nucleation on the microstructural evolution of lead-free solder joints10.1007/s10854-006-9012-8 ↗
22. Crystallization, morphology and distribution of Ag3Sn in Sn–Ag–Cu alloys and their influence on the vibration fracture properties10.1016/j.msea.2007.04.121 ↗
23. Effects of cooling speed on microstructure and tensile properties of Sn–Ag–Cu alloys10.1016/S0921-5093(01)01828-7 ↗
24. Evolution of Ag3Sn intermetallic compounds during solidification of eutectic Sn-3.5Ag solder10.1016/j.jallcom.2010.11.068 ↗
25. Observation of micro-droplets on metal surface in early atmospheric corrosion10.1016/j.elecom.2005.06.016 ↗
26. Generation of Tin(II) oxide crystals on lead-free solder joints in deionized water10.1007/s11664-009-0868-2 ↗
27. Effect of Ag addition on the corrosion properties of Sn-based solder alloys10.1002/maco.200905237 ↗
28. Oxidation behavior of rare-earth-containing Pb-free solders10.1007/s11664-008-0544-y ↗
29. Comparative cyclic voltammetry and SEM analysis of tin electrodes in citrate buffer solutions10.1016/j.jelechem.2006.11.019 ↗