Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions
Source abstract
Abstract
Abstract The supercritical water-cooled reactor (SCWR) is a Generation IV concept that will operate with water above its thermodynamic critical point as the coolant. To aid in material selection and reactor design, Pourbaix diagrams for the alloying elements chromium, aluminum, and titanium have been developed under high-subcritical and low-supercritical conditions. The necessary thermodynamic extrapolations were performed using a revised Helgeson–Kirkham–Flowers model. The diagrams reveal the necessity to examine the transient reactor operating conditions such as start-up and shut-down to avoid active corrosion or dissolution of these elements from the alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · Chemical Looping and Thermochemical Processes · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. CANDU technology for Generation III+ and IV reactors10.1016/j.nucengdes.2006.04.020 ↗
2. Deposition, characterization and performance evaluation of ceramic coatings on metallic substrates for supercritical water-cooled reactors10.1016/j.surfcoat.2010.12.017 ↗
3. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
4. M. Pourbaix, N. de Zubov, Atlus d’Equifibres Electrochimiques, in: M. Pourbaix (Ed.), Gauthier-Villars and Cie, Paris, 1963.
5. Revised Pourbaix diagrams for nickel at 25–300°C10.1016/S0010-938X(97)00002-4 ↗
6. Revised Pourbaix diagrams for chromium at 25–300°C10.1016/S0010-938X(97)89244-X ↗
7. Revised Pourbaix diagrams for iron at 25–300°C10.1016/S0010-938X(96)00067-4 ↗
8. Chemical thermodynamics consideration on corrosion products in supercritical-water-cooled reactor coolant10.13182/NT06-A3749 ↗
9. The ionization constant of water over wide ranges of temperature and density10.1063/1.1928231 ↗
10. IAPWS, Release on the Ionization Constant of H2O (2007).
11. Calculation of the thermodynamic and transport properties of aqueous species at high pressures and temperatures: correlation algorithms for ionic species and equation of state predictions to 5kb and 1000°C10.1016/0016-7037(88)90181-0 ↗
12. Calculation of the thermodynamic properties of aqueous species at high pressures and temperatures. Effective electrostatic radii, dissociation constants and standard partial molal properties to 1000°C and 5kbar10.1039/FT9928800803 ↗
13. Summary of the apparent partial molal Gibbs free energies of formation of aqueous species, minerals. and gases at pressures 1–5000bars and temperatures 25–1000°C10.1063/1.555976 ↗
14. Inorganic species in geologic fluids: correlations among standard molal thermodynamic properties of aqueous ions and hydroxide complexes10.1016/S0016-7037(96)00339-0 ↗
15. Predictive model for equilibrium constants of aqueous inorganic species at subcritical and supercritical conditions10.1021/ie010956y ↗
16. Solubility and phase behavior of Cr(III) oxides in alkaline media at elevated temperatures10.1023/A:1022688528380 ↗
17. P.R. Roberge, Handbook of Corrosion Engineering, McGraw-Hill, 2000.10.5006/C2000-00478 ↗
18. Aqueous high-temperature solubility studies. II. The solubility of boehmite at 0.03m ionic strength as a function of temperature and pH as determined by in situ measurements10.1016/S0016-7037(01)00585-3 ↗
19. Thermodynamics of the Al2O3-Al4C3 system. I. Thermochemical functions of Al oxide, carbide and oxycarbides between 298 and 2100 K10.1016/j.jeurceramsoc.2006.06.009 ↗
20. Titanium(IV) oxide phase stability in alkaline sodium phosphate solutions at elevated temperatures10.1021/cm00029a019 ↗
21. Ti(IV) hydrolysis constants derived from rutile solubility measurements made from 100 to 300°C10.1016/S0883-2927(00)00081-0 ↗
22. Pourbaix diagrams for titanium in concentrated aqueous lithium bromide solutions at 25°C10.1016/j.corsci.2011.01.013 ↗
23. 2005
24. Kubaschewksi · 1979
25. Standard free energies of formation of titanium hydroxo-complexes and of the Ti4+ ion in aqueous solution
26. Understanding chemical conditions in supercritical water oxidation systems