journal article·2019-02

Transmission electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic

E. Charalampopoulou, R. Delville, M. Verwerft, K. Lambrinou, D. Schryvers

Corrosion Science· Volume 147
Publisher page

Abstract

Abstract The deployment of Gen-IV lead-cooled fast reactors requires a good compatibility between the selected structural/cladding steels and the inherently corrosive heavy liquid metal coolant. An effective liquid metal corrosion mitigation strategy involves the in-situ steel passivation in contact with the oxygen-containing Pb-alloy coolant. Transmission electron microscopy was used in this work to study the multi-layered oxide scales forming on an austenitic stainless steel fuel cladding exposed to oxygen-containing (CO ≈ 10−6 mass%) static liquid lead-bismuth eutectic (LBE) for 1000 h between 400 and 500 °C. The oxide scale constituents were analyzed, including the intertwined phases comprising the innermost biphasic layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear reactor physics and engineering · Nuclear Materials and Properties · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Lead-cooled fast reactor A2
2. MYRRHA – a multi-purpose fast spectrum research reactor10.1016/j.enconman.2012.02.025 ↗
3. 2007
4. Corrosion and deposition of steels and nickel-base alloys in liquid sodium
5. Lead-alloy coolant technology and materials – technology readiness level evaluation10.1016/j.pnucene.2007.10.016 ↗
6. Models of liquid metal corrosion10.1016/j.jnucmat.2010.05.024 ↗
7. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
8. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
9. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
10. Aspects of minimizing steel corrosion in liquid lead-alloys by addition of oxygen10.1016/j.nucengdes.2011.09.002 ↗
11. Analysis of corrosion scale structure of pre-oxidized stainless steel 316 in molten lead bismuth eutectic and the relation to impedance spectroscopy response10.1016/j.jnucmat.2009.10.029 ↗
12. Corrosion behavior of austenitic steels in liquid lead bismuth containing 10−6wt% and 10−8wt% oxygen at 400–500°C10.1016/j.jnucmat.2014.01.046 ↗
13. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
14. Characterization of oxide layers grown on D9 austenitic stainless steel in lead bismuth eutectic10.1016/j.jnucmat.2007.12.005 ↗
15. Analysis of bi-layer oxide on austenitic stainless steel, 316L, exposed to Lead–Bismuth Eutectic (LBE) by X-ray Photoelectron Spectroscopy (XPS)10.1016/j.jnucmat.2013.03.093 ↗
16. Modeling of oxidation of structural materials in LBE systems10.1016/j.jnucmat.2007.07.022 ↗
17. Oxidation mechanism of steels in liquid-lead alloys10.1007/s11085-005-4392-3 ↗
18. Oxidation mechanism of T91 steel in liquid lead-bismuth eutectic: with consideration of internal oxidation10.1038/srep35268 ↗
19. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
20. EFTEM and EELS analysis of the oxide layer formed on HCM12A exposed to SCW10.1016/j.jnucmat.2012.06.017 ↗
21. Long-term service of austenitic steel 1.4571 as a container material for flowing lead–bismuth eutectic10.1016/j.jnucmat.2011.07.026 ↗
22. Comparative oxidation behaviour of Fe-9Cr steel in CO2 and H2O at 550°C: Detailed analysis of the inner oxide layer10.1016/j.corsci.2015.07.032 ↗
23. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb–Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
24. Oxidation behaviour of P122 and a 9Cr–2W ODS steel at 550°C in oxygen-containing flowing lead–bismuth eutectic10.1016/j.jnucmat.2009.10.019 ↗
25. Corrosion investigations of steels in flowing lead at 400°C and 550°C10.1016/S0022-3115(01)00522-0 ↗
26. Effect of pre-deformation on the oxidation resistance of a high Si ferritic/martensitic steel in oxygen-saturated stagnant lead-bismuth eutectic at 550°C10.1016/j.corsci.2017.02.005 ↗
27. Effect of silicon on the oxidation resistance of 9wt.% Cr heat resistance steels in 550°C lead-bismuth eutectic10.1016/j.corsci.2016.04.020 ↗
28. AFM and MFM characterization of oxide layers grown on stainless steels in lead bismuth eutectic10.1016/j.jnucmat.2008.02.013 ↗
29. Results of a new production of nuclear-grade 1.4970 15-15Ti stainless steel fuel cladding tubes for GEN IV reactors
30. Performance of potentiometric oxygen sensors with LSM-GDC composite electrode in liquid LBE at low temperatures10.1016/j.snb.2013.08.017 ↗
31. Control of dissolved oxygen in liquid LBE by electrochemical oxygen pumping10.1016/j.snb.2014.07.117 ↗
32. Oxidation mechanism of an Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy at 470 °C (Part II)10.1016/j.corsci.2008.06.051 ↗
33. Physical chemistry of corrosion and oxygen control in liquid lead and lead-bismuth eutectic
34. Corrosion behaviors of US steels in flowing lead–bismuth eutectic (LBE)10.1016/j.jnucmat.2004.08.002 ↗
35. Self-diffusion in austenitic Fe-Cr-Ni alloys10.1088/0305-4608/10/3/009 ↗
36. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗